GB/T 3077 Alloy Steel Plate
GB/T 3077 20CrNiMo Alloy Steel Plate: Chemistry & Properties
Gangsteel (HENAN GANG IRON AND STEEL CO.,LTD.) supplies GB/T 3077 20CrNiMo (unified numerical code A50202) as alloy steel plate cut to customer drawings. GB/T 3077-2015 lists 20CrNiMo as a nickel-chromium-molybdenum carburizing steel with C 0.17–0.23%, Mn 0.60–0.95%, chromium 0.40–0.70%, molybdenum 0.20–0.30%, nickel 0.35–0.75%. It is a low-carbon Ni-Cr-Mo carburizing grade with a balanced, lean alloy content, widely used for case-hardened gears and shafts. The sections below give the 2015-edition chemistry, the quality-class limits for phosphorus and sulphur, the recommended heat treatment and minimum properties of Table 3, and the points a plate order has to settle because the standard is written for bars.
What is GB/T 3077 20CrNiMo?
GB/T 3077-2015 Alloy structure steels is the Chinese national standard for alloy structural steel. It replaced GB/T 3077-1999. The 2015 edition no longer lists separate “A” grades in Table 1; instead the quality level is ordered as a class — quality steel, high-grade quality steel (grade name followed by A) or special high-grade quality steel (followed by E) — and the class sets the phosphorus and sulphur limits of Table 2. In the designation 20CrNiMo, the leading digits give the mean carbon content in hundredths of a percent, and the element symbols that follow name the principal alloying elements; a number after a symbol signals a higher content of that element.
Scope note for plate: the standard applies to hot-rolled and forged bars up to 250 mm nominal diameter or thickness (larger sizes by agreement), but it states that its grades and chemical compositions also apply to ingots, billets and their products. Plate in 20CrNiMo is therefore supplied to the GB/T 3077 chemistry, while dimensions, tolerances, delivery condition and any mechanical testing of the plate itself are agreed in the contract. The Table 3 properties below are defined on heat-treated sample blanks of a stated size.
20CrNiMo Chemical Composition (GB/T 3077-2015 Table 1)
Table 1 gives the heat (ladle) analysis of 20CrNiMo. Phosphorus, sulphur and residual elements are not in Table 1; they depend on the ordered quality class and are given in Table 2.
| Grade (code) | C % | Si % | Mn % | Cr % | Mo % | Ni % |
|---|---|---|---|---|---|---|
| 20CrNiMo (A50202) | 0.17–0.23 | 0.17–0.37 | 0.60–0.95 | 0.40–0.70 | 0.20–0.30 | 0.35–0.75 |
Table 2 limits (maximum, %) by quality class:
| Quality class | P | S | Cu | Cr | Ni | Mo |
|---|---|---|---|---|---|---|
| Quality steel | 0.030 | 0.030 | 0.30 | 0.30 | 0.30 | 0.10 |
| High-grade quality steel (A) | 0.020 | 0.020 | 0.25 | 0.30 | 0.30 | 0.10 |
| Special high-grade quality steel (E) | 0.020 | 0.010 | 0.25 | 0.30 | 0.30 | 0.10 |
Notes: the Cr, Ni and Mo columns of Table 2 are residual limits; for 20CrNiMo they apply to no element, since Cr, Ni and Mo are all specified, because the other elements are specified in Table 1. For steel intended for hot pressure working, copper is limited to 0.20%. Residual tungsten, vanadium and titanium are analysed and reported on the certificate and can be limited on request. Product (check) analysis tolerances follow GB/T 222.
20CrNiMo Mechanical Properties (GB/T 3077-2015 Table 3)
Table 3 gives minimum longitudinal properties measured on a sample blank of 15 mm after the recommended heat treatment, together with the maximum Brinell hardness for bars delivered annealed or high-temperature tempered.
| Sample blank, mm | Rm min, MPa | ReL min, MPa | A min, % | Z min, % | KU2 min, J | HBW max (annealed / high-temp tempered) |
|---|---|---|---|---|---|---|
| 15 | 980 | 785 | 9 | 40 | 47 | 197 |
Notes: where the yield point is not distinct, the specified non-proportional extension strength Rp0.2 may be used instead of ReL. If a bar is smaller than the sample blank size, it is heat treated at its own size. Impact tests are not made on rounds under 16 mm diameter or on squares and flats under 12 mm thick. The values apply to sizes up to 80 mm; for larger sections clause 6.4.2 allows the reductions below, or the sample may be forged or rolled down to a 70–80 mm section and tested to Table 3.
| Nominal size, mm | Elongation A | Reduction of area Z | Impact energy KU2 |
|---|---|---|---|
| > 80 to 100 | −1 (absolute) | −5 (absolute) | −5% |
| > 100 to 150 | −2 (absolute) | −10 (absolute) | −10% |
| > 150 to 250 | −3 (absolute) | −15 (absolute) | −15% |
20CrNiMo Delivery Condition
Under clause 6.3 of GB/T 3077-2015, bars are normally delivered hot rolled or hot forged. When the contract states it, they may be delivered heat treated — annealed, normalized or high-temperature tempered — and by agreement the surface may be ground, peeled or otherwise finished. For 20CrNiMo plate the same logic applies: the delivery condition is stated on the order, and the fabricator then carries out the final heat treatment of the machined part.
| Condition | Basis in GB/T 3077-2015 | Requirement for 20CrNiMo |
|---|---|---|
| Hot rolled / hot forged | 6.3.1 (normal delivery) | Chemistry to Tables 1 and 2 |
| Annealed or high-temperature tempered | 6.3.2 (by agreement) | Hardness ≤ 197 HBW (Table 3) |
| Normalized | 6.3.2 (by agreement) | As agreed |
| Quenched and tempered properties | 6.4 / Table 3 | Proven on a heat-treated sample blank of 15 mm |
Notes: the order should name the standard, the grade or unified code, the quality class, the delivery condition, the dimensions and tolerances, and any special requirements agreed under the standard, such as restricted residual elements. Because Table 3 is defined on sample blanks, any requirement for properties measured on the plate itself, and the thickness at which they apply, must be agreed separately.
20CrNiMo Heat Treatment
Table 3 gives the recommended heat treatment for the sample blank. It is the reference treatment for verifying the minimum properties and a sound starting point for parts, although section size and shape may call for adjustment in production.
| Step | Recommended for 20CrNiMo |
|---|---|
| Quenching temperature | 850 °C |
| Quenching coolant | oil |
| Tempering temperature | 200 °C |
| Tempering coolant | air |
Notes: the permitted adjustment of the listed temperatures is ±15 °C for quenching, ±20 °C for low-temperature tempering and ±50 °C for high-temperature tempering. The recommended treatment applies to the sample blank; for real parts the quenchant and time at temperature should be chosen with the section, shape and distortion risk in mind.
Related Grades and Alternatives to 20CrNiMo
GB/T 3077-2015 Annex A lists the following as similar grades to 20CrNiMo: 8620 (ASTM A29/A29M-2012), SNCM220 (JIS G 4053-2008). These are similarity listings, not certified equivalents. Within the site, related pages are: GB/T 3077 20CrMnMo steel is a nickel-free carburizing grade with higher hardenability; GB/T 3077 20Cr2Ni4 steel is a high-nickel carburizing grade for heavier sections. Any substitution should be checked against the chemistry, heat treatment and property requirements of the governing standard.
Typical Applications of 20CrNiMo Plate
Typical uses are carburized gears, pinions, shafts, bearing races and wear parts that need a hard case on a tough core. In plate form, the steel is usually profile-cut and machined before the final heat treatment, so the order should state who heat treats the part and how the properties are to be proven.
20CrNiMo Plate Supply and Ordering Information
The supply range below is taken from the original product page and is subject to confirmation for each enquiry.
| Item | Range / option |
|---|---|
| Thickness | 8 to 250 mm |
| Width | 1500 to 4050 mm |
| Length | 3000 to 15000 mm |
| Quality class | Quality steel, A or E (Table 2) |
| Delivery condition | Hot rolled; annealed, normalized or high-temperature tempered by agreement |
Notes: 250 mm corresponds to the upper size limit of the standard’s bar scope; plate properties at any thickness are agreed in the contract. State GB/T 3077-2015, 20CrNiMo or A50202, the quality class and the inspection document on the order.
20CrNiMo Steel FAQ
What is the chemical composition of GB/T 3077 20CrNiMo?
Table 1 gives C 0.17–0.23%, Si 0.17–0.37%, Mn 0.60–0.95%, chromium 0.40–0.70%, molybdenum 0.20–0.30%, nickel 0.35–0.75%. Phosphorus and sulphur depend on the quality class: 0.030% maximum each for quality steel, 0.020% each for grade A and 0.020% P with 0.010% S for grade E.
What are the mechanical properties of 20CrNiMo?
After the recommended heat treatment of a 15 mm sample blank, Table 3 requires Rm ≥ 980 MPa, ReL ≥ 785 MPa, A ≥ 9%, Z ≥ 40% and KU2 ≥ 47 J. Annealed or high-temperature tempered bars are limited to 197 HBW.
What heat treatment does GB/T 3077 recommend for 20CrNiMo?
Quench from 850 °C in oil, then temper at 200 °C and cool in air. The listed temperatures may be adjusted by ±15 °C for quenching and ±20 °C or ±50 °C for low- or high-temperature tempering.
Does GB/T 3077 cover 20CrNiMo plate?
The standard is written for hot-rolled and forged bars up to 250 mm, but it states that its grades and chemical compositions also apply to ingots, billets and their products. Plate is therefore ordered to the GB/T 3077 chemistry, with plate dimensions, condition and any property testing agreed in the contract.
Is there a 20CrNiMoA grade in GB/T 3077-2015?
Not as a separate grade. The 2015 edition replaced the old A grades with quality classes; ordering 20CrNiMoA now means 20CrNiMo with the high-grade quality limits of Table 2 (P and S 0.020% maximum each).
Is 20CrNiMo the same as AISI 8620?
GB/T 3077-2015 Annex A lists ASTM 8620 and JIS SNCM220 as similar grades. The windows are close but the standards differ, so specify one standard on the order.
What core properties does GB/T 3077 require for 20CrNiMo?
On a 15 mm blank quenched from 850 °C in oil and tempered at 200 °C, Table 3 requires Rm ≥ 980 MPa, ReL ≥ 785 MPa, A ≥ 9%, Z ≥ 40% and KU2 ≥ 47 J.
-
20Mn2|20Mn2 Alloy Steel Plate
Gangsteel is specialized in supplying Alloy steel plate in 20Mn2,20Mn2 alloy,20Mn2 alloy steel plates
-
50Cr|GB/T 3077 50Cr Alloy Steel
Gangsteel supply 50Cr,50Cr alloy,50Cr steel plates
-
15Cr|15Cr Alloy Steel Plate
Gangsteel is specialized in supplying Alloy steel plate in 15Cr,15Cr alloy,15Cr steel steel plates
-
40Cr|40Cr steel plate
Gangsteel supply alloy steel plate 40Cr.High quality,Competitive price