• A40

Certificates

 

WKZ077-2005         A40

Adopt the Ⅱstage rolling, air steel thickness≥2 h, finishing temperature stage ≤880 ℃.

Normalized technology: heat preservation temperature: 910 ±10 ℃, total heating time: 1.5 min/mm