• P355GH

Certificates

 

WKZ071-2005        P355GH

1, must use Ⅱstage rolling, air steel thickness > 2 h, Ⅱstage finishing rolling temperature ≤900 ℃.

2, normalized

normalized technology : normalizing furnace: 910±10℃.

Total heat time  ≥1.5min/mm

outside machine furnace and car bottom furnace:920±10℃

the heat preservation time  ≥1.5min/mm