P275NL1 Steel Plate Specifications
EN 10028-3 P275NL1 (1.0488) is a weldable fine-grain pressure-vessel steel for low-temperature service grade under EN 10028-3. This specification page covers grade identity, chemistry, mechanical requirements, related grades, and RFQ practice. Accept material against the ordered edition and the mill test certificate.
Grade Identity and Delivery Condition
EN 10028-3 P275NL1 (1.0488) is supplied for projects that name this designation on the purchase order or calculation sheet. Standard delivery condition is Normalized (+N). Gangsteel supplies export plate and related products with EN 10204 documentation. Do not accept an alternate heat-treatment route unless a written concession changes the specification requirement.
Chemical Composition - Heat Analysis (EN 10028-3 P275NL1 (1.0488))
Ladle analysis for P275NL1. Confirm EN 10028-3 edition and thickness option.
| Element / rule | Requirement |
|---|
| C, max | 0.16 |
| Si, max | 0.40 |
| Mn | 0.80-1.50 |
| P, max | 0.025 |
| S, max | 0.015 |
| Al total, min | 0.020 |
| N, max | 0.012 |
| Nb+Ti+V, max | 0.12 |
Mechanical Properties (EN 10028-3 P275NL1 (1.0488))
Confirm thickness, specimen orientation, and any supplementary impact, UT, or hardness requirements on the PO.
| Property | Requirement |
|---|
| Yield ReH min (t<=16 mm) | 275 MPa |
| Tensile Rm (t<=60 mm typical) | 390-510 MPa |
| Elongation A, min | 24% |
| Impact (transverse) | -40 deg C, >=27 J typical |
| Delivery | +N normalized |
Related / Near-Equivalent Grades
Near-equivalents are for cross-reference only. They are not automatic code substitutes. Substitution requires engineer approval and matching certificate scope.
| System | Grade | Note |
|---|
| EN 10028-3 | P275NL2 | Colder impact option |
| EN 10028-3 | P355NH / P355NL1 | Higher strength pressure grades |
| ASTM | A516 Grade 60 (approx.) | Not identical - confirm PED/ASME route |
Frequently Asked Questions
What is EN 10028-3 P275NL1 (1.0488)?
EN 10028-3 P275NL1 (1.0488) is a weldable fine-grain pressure-vessel steel for low-temperature service under EN 10028-3. It is ordered when drawings or the calculation sheet name this designation specifically.
What chemical composition applies to EN 10028-3 P275NL1 (1.0488)?
Controlled elements and limits are tabulated above from the governing standard. Always verify the heat analysis on the MTC against the ordered edition.
What mechanical properties should buyers expect for EN 10028-3 P275NL1 (1.0488)?
Tensile, yield, elongation, and related limits are tabulated above. Design allowables must come from the applicable pressure-vessel or structural code, not from a web summary.
What delivery condition is required for EN 10028-3 P275NL1 (1.0488)?
Standard delivery is Normalized (+N). State it explicitly on the PO. Do not accept an alternate route without a written concession.
How does EN 10028-3 P275NL1 (1.0488) differ from near-equivalent grades?
Near-equivalents may differ in carbon or alloy bands, tensile class, impact temperature, or heat treatment. Substitution needs engineering approval and matching certificate scope.
How do I RFQ EN 10028-3 P275NL1 (1.0488) from Gangsteel?
Send EN 10028-3 P275NL1 (1.0488), thickness x width x length, quantity or tonnage, delivery condition, optional impact/UT/Z tests, EN 10204 3.1 or 3.2, destination, and any dual-mark needs. Gangsteel replies with mill options, lead time, and packing notes.
Ordering and Mill Certificates
State grade EN 10028-3 P275NL1 (1.0488), dimensions, quantity, delivery condition, optional NDT/PMI, and certificate (EN 10204 3.1 standard; 3.2 when third-party inspection is ordered). Gangsteel supplies export plate and related products with mill test certificates. Contact Gangsteel for stock and mill production RFQs.