Cutting and bending NM500 wear plate needs more care than mild steel or softer NM grades. Thermal cutting leaves a heat-affected edge; bends need larger radii. This buyer guide outlines process choices and points to GB/T 24186 NM500 for hardness and supply data. It is not a shop procedure.

Cutting and Bending NM500 Wear Plate: Practical Buyer Guide

Canonical product page: GB/T 24186 NM500 holds chemistry, full hardness tables, sizes and RFQ fields. This article explains the topic in the title; it is not a second datasheet.

NM500 hardness reminder

Primary surface band: 470 to 540 (<=70 mm); thicker band 450 to 540 (>70 to 100 mm). Full tables: GB/T 24186 NM500.

Cutting methods - practical comparison

MethodBuyer note
PlasmaCommon for medium thickness; expect HAZ that may need grind-back
Flame / oxy-fuelHeavier sections; preheat often helps reduce edge cracking
WaterjetMinimal HAZ; slower/costlier for many shapes
LaserGood on thinner plate when available

Bending notes

Use mill/fabricator bend charts for ordered thickness and rolling direction. NM500 needs larger radii than NM400. Grind thermal HAZ before critical bends. Softened cut edges can wear faster if left as the working edge.

Grade hardness context

GradeNominal HBWPrimary surface band (from canon pages)Product page
NM300~300270 to 330 (<=80 mm)GB/T 24186 NM300
NM360~360330 to 400 (<=80 mm)GB/T 24186 NM360
NM400~400370 to 430 (<=80 mm)GB/T 24186 NM400
NM450~450420 to 480 (<=80 mm)GB/T 24186 NM450
NM500~500470 to 540 (<=70 mm)GB/T 24186 NM500
NM550~550520 to 580 (<=70 mm)GB/T 24186 NM550
NM600~600570 to 640 (<=60 mm)GB/T 24186 NM600

Bands above are copied from the canonical GB/T 24186 product pages on this site. Confirm the ordered edition and thickness on the MTC.

FAQ

Can NM500 be plasma cut?

Yes. Plasma is common for medium thickness NM500. Expect a heat-affected edge that may need grind-back before critical bends or when the cut edge is the wear face. Parameter choice depends on thickness and shop practice. Hardness context for the ordered plate is on GB/T 24186 NM500 (about 470 to 540 HBW for <=70 mm).

Does flame cutting NM500 need preheat?

Heavy sections often benefit from preheat to reduce edge cracking during oxy-fuel cutting. The exact temperature and hold time come from fabricator practice and thickness - not from a one-line web rule. After cutting, inspect the edge and grind HAZ when bends or fatigue-sensitive details follow.

What bend radius for NM500?

Use mill or fabricator bend charts for the ordered thickness and rolling direction. NM500 needs larger radii than softer grades such as GB/T 24186 NM400. Always remove or grind thermal cut HAZ before tight bends. If the part needs aggressive forming, reconsider whether GB/T 24186 NM450 or NM400 fits the duty better.

Waterjet vs plasma for NM500?

Waterjet minimizes heat-affected softening and is preferred when edge integrity is critical. Plasma is usually faster and cheaper for many shapes. Choose based on edge quality needs, thickness and cost. Either way, specify the NM500 hardness band on the PO and verify on the MTC via GB/T 24186 NM500.

Will cutting soften the wear edge?

Thermal cutting can alter hardness in the heat-affected zone along the cut edge. If that edge becomes the wearing face, grind back the HAZ or allow for faster local wear. Waterjet reduces this effect. Design and inspection should assume HAZ exists unless proven otherwise. Grade/hardness tables: GB/T 24186 NM500.

Ordering pointer

On the inquiry, write grade GB/T 24186 NM500, thickness, width, length, hardness band, delivery condition and certificate (3.1 or 3.2). Send RFQs via Gangsteel - HENAN GANG IRON AND STEEL CO.,LTD.

Other Products