GB/T 24186 brasion resistant
Welding NM400 Wear Plate: Preheat, Consumables and Cracking R
Welding NM400 wear plate is routine in chutes, liners and dump bodies when hydrogen, preheat and joint restraint are controlled. This article summarizes practical buyer questions on preheat, consumables and cracking risks. Chemistry and hardness live on GB/T 24186 NM400 - this page is not a WPS.

Canonical product page: GB/T 24186 NM400 holds chemistry, full hardness tables, sizes and RFQ fields. This article explains the topic in the title; it is not a second datasheet.
Why NM400 is weldable - with controls
NM400 is chosen partly because ~400 HBW wear service can still be welded with low-hydrogen processes. Risk rises with thickness, high CEV, high restraint and poor hydrogen control. Always follow a qualified welding procedure for the ordered thickness.
Preheat, consumables and process checklist
| Topic | Practical note |
|---|---|
| Preheat | Depends on thickness, CEV and restraint; heavier plate usually needs more preheat. Use the WPS, not a website rule of thumb. |
| Consumables | Low-hydrogen SMAW / GMAW / FCAW matched to required strength/toughness. |
| Interpass | Keep within WPS limits; avoid overheating the hard plate. |
| HAZ / cutting | Thermal cut edges may need grind-back before critical bends. |
| Backing | Liner-on-mild-steel backing is common; design welds for the soft backing. |
Cracking risks - common causes
Insufficient preheat, high hydrogen, high restraint, hard HAZ, or treating wear plate like mild steel. Control hydrogen and heat input; do not skip qualified procedures.
Hardness context for welding discussions
| Grade | Nominal HBW | Primary surface band (from canon pages) | Product page |
|---|---|---|---|
| NM300 | ~300 | 270 to 330 (<=80 mm) | GB/T 24186 NM300 |
| NM360 | ~360 | 330 to 400 (<=80 mm) | GB/T 24186 NM360 |
| NM400 | ~400 | 370 to 430 (<=80 mm) | GB/T 24186 NM400 |
| NM450 | ~450 | 420 to 480 (<=80 mm) | GB/T 24186 NM450 |
| NM500 | ~500 | 470 to 540 (<=70 mm) | GB/T 24186 NM500 |
| NM550 | ~550 | 520 to 580 (<=70 mm) | GB/T 24186 NM550 |
| NM600 | ~600 | 570 to 640 (<=60 mm) | GB/T 24186 NM600 |
Bands above are copied from the canonical GB/T 24186 product pages on this site. Confirm the ordered edition and thickness on the MTC.
NM400 primary band: 370 to 430 (<=80 mm) on GB/T 24186 NM400.
FAQ
Can you weld NM400 steel plate?
Yes. GB/T 24186 NM400 is commonly welded in chutes, liners and dump bodies when thickness, joint restraint and hydrogen are controlled. Low-hydrogen SMAW/GMAW/FCAW processes are typical. Higher thickness and higher restraint need more preheat and stricter hydrogen control. This article is buyer guidance only - the qualified WPS is the authority.
What preheat temperature for NM400?
Preheat depends on thickness, carbon equivalent, joint restraint and the filler/process in the WPS. Many fabricators increase preheat as plate gets thicker or joints get more restrained. There is no single website temperature that replaces a qualified procedure. Ask your fabricator for the WPS tied to the ordered GB/T 24186 NM400 heat and thickness.
Which electrodes for NM400 welding?
Use low-hydrogen consumables matched to the required strength and toughness (SMAW stick, GMAW solid/metal-cored, or FCAW as specified). Follow the filler manufacturer data and the project WPS for parameters, baking/holding of electrodes, and interpass limits. Do not pick consumables from a blog list without procedure qualification.
Why does NM400 crack after welding?
Common causes include insufficient preheat, high diffusible hydrogen, high restraint, a hard heat-affected zone, or treating wear plate like mild steel. Control hydrogen, respect interpass temperature, and grind/cut HAZ carefully before bending. If cracking persists, review thickness, joint design and whether a lower hardness grade or liner-on-backing design is more appropriate. Grade data: GB/T 24186 NM400.
Should wear plate be welded to mild-steel backing?
Yes - liner-on-backing is a common design: the hard NM400 takes wear while welds and structure lean on milder steel. Design throat size and sequence for the soft backing, avoid over-welding the hard plate, and keep hydrogen low. Confirm the ordered NM400 hardness band on GB/T 24186 NM400 so the liner matches the wear duty.
Ordering pointer
On the inquiry, write grade GB/T 24186 NM400, thickness, width, length, hardness band, delivery condition and certificate (3.1 or 3.2). Send RFQs via Gangsteel - HENAN GANG IRON AND STEEL CO.,LTD.
-
GB/T 24186 NM300-NM600 Abrasion
Overview of GB/T 24186 NM300 to NM600 abrasion resistant steel grades with links to each canonical Gangsteel pr
-
WNM vs NM Wear Plate: What WNM3
What WNM360L means vs GB/T 24186 NM360 for buyers: brand naming, MTC checks and when to order the canonical NM
-
Cutting and Bending NM500 Wear
Buyer guide to cutting and bending NM500 wear plate: plasma, flame, waterjet, bend radius and edge softening no
-
Welding NM400 Wear Plate: Prehe
Practical welding notes for NM400 wear plate: preheat, consumables, cracking risks and backing to mild steel. S