ASME SA240 / ASTM A240 UNS S31060 Stainless Steel Sheet for sales

 

For applications requiring excellent high-temperature corrosion resistance, good strength, and moderate weldability, ASME SA240/ASTM A240 UNS S31060 Stainless Steel Sheet (commonly known as 310S) is a reliable choice.

 

As a leading uns stainless supplier, Gangsteel specializes in providing high-quality sa 240/a 240 uns s31060 sheets, plates, coils, bars, and custom components, all compliant with sa 240/a 240 uns stainless grades standards, including ASTM A240 and ASME SA240. With an inventory exceeding 600 tons and advanced manufacturing capabilities, Gangsteel ensures rapid delivery and tailored solutions for clients worldwide.

This comprehensive guide explores the ASME SA240/ASTM A240 UNS S31060 chemical composition, density, mechanical properties, corrosion resistance, weldability, stainless steel surface finishes, equivalent materials, specifications, applications, and competitive ASME SA240/ASTM A240 UNS S31060 price per kg.

 

Whether you're an engineer designing furnace components or a procurement specialist sourcing for petrochemical applications, this article will clarify why 310S stainless steel (UNS S31060) is a trusted option. Explore our sa 240/a 240 uns stainless grades portfolio for related grades like sa 240/a 240 uns s30615, sa 240/a 240 uns s30815, sa 240/a 240 uns s30909, sa 240/a 240 uns s30940, sa 240/a 240 uns s31040, sa 240/a 240 uns s31041, sa 240/a 240 uns s31050, sa 240/a 240 uns s31254, and sa 240/a 240 uns s31266.


Why Choose ASME SA240/ASTM A240 UNS S31060 Stainless Steel Sheet?

 

ASME SA240/ASTM A240 UNS S31060, known as 310S, is an austenitic stainless steel with 24.0-26.0% chromium, 19.0-22.0% nickel, and a low carbon content (≤ 0.08%). It is designed for high-temperature applications requiring excellent corrosion resistance, good strength, and moderate weldability, making it ideal for industries such as petrochemical, power generation, and furnace manufacturing. The low carbon content improves weldability compared to sa 240/a 240 uns s31041, while the high chromium and nickel content ensure robust oxidation resistance up to 1100°C (2012°F).

The ASME SA240/ASTM A240 UNS S31060 stainless steel sheet offers excellent high-temperature corrosion resistance compared to sa 240/a 240 uns s30909 and better weldability than sa 240/a 240 uns s30815 due to its lower carbon content. While it is less corrosion-resistant in highly aggressive environments than grades like sa 240/a 240 uns s31050 or sa 240/a 240 uns s31254, its balance of corrosion resistance and high-temperature performance makes it a preferred choice for furnace and heat exchanger applications.

 

Key benefits of ASME SA240/ASTM A240 UNS S31060 stainless steel sheet include:

  • Excellent High-Temperature Corrosion Resistance: High chromium (24.0-26.0%) and nickel (19.0-22.0%) content provide robust oxidation resistance, surpassing sa 240/a 240 uns s30615.
  • Good Weldability: Low carbon content (≤ 0.08%) minimizes carbide precipitation, outperforming sa 240/a 240 uns s31041 in welded applications.
  • Moderate Strength: Suitable for high-temperature applications requiring durability, such as furnace linings.
  • Cost-Effective: Offers a balance of performance and cost compared to sa 240/a 240 uns s31050 for high-temperature environments.

Case Study: A petrochemical plant in India used sa 240/a 240 uns s31060 sheets for furnace components, achieving a 20% cost reduction compared to sa 240/a 240 uns s30815 while maintaining reliable high-temperature performance.

Keywords: ASME SA240/ASTM A240 UNS S31060 stainless steel sheet, UNS S31060 sheet, 310S stainless steel, high-temperature stainless steel sheet


ASME SA240/ASTM A240 UNS S31060 Density

 

The density of ASME SA240/ASTM A240 UNS S31060 stainless steel sheet is approximately 7.89 g/cm³ (0.285 lb/in³). This density is typical for high-chromium and high-nickel austenitic stainless steels, reflecting the material's composition. The consistent density ensures predictable performance in applications requiring precise weight calculations, such as furnace components and heat exchangers. Compared to grades like sa 240/a 240 uns s30815 (7.80 g/cm³) and sa 240/a 240 uns s31050 (7.89 g/cm³), the density is similar, making UNS S31060 a reliable choice for weight-sensitive high-temperature applications.

Keywords: ASME SA240/ASTM A240 UNS S31060 density, UNS S31060 density, 310S density


ASME SA240/ASTM A240 UNS S31060 Corrosion Resistance

 

ASME SA240/ASTM A240 UNS S31060offers excellent corrosion resistance in high-temperature environments, such as petrochemical and power generation settings. Its 24.0-26.0% chromium and 19.0-22.0% nickel content provide a robust protective oxide layer, with a pitting resistance equivalent number (PREN) of ~24-26, suitable for applications like furnace linings and heat exchanger tubes. It outperforms sa 240/a 240 uns s30615 and sa 240/a 240 uns s30940 in high-temperature corrosion resistance due to its higher chromium and nickel content. For highly corrosive environments, such as chloride-rich conditions, grades like sa 240/a 240 uns s31050 or sa 240/a 240 uns s31254 are recommended.

Keywords: ASME SA240/ASTM A240 UNS S31060 corrosion resistance, UNS S31060 corrosion properties, 310S corrosion resistance


ASME SA240/ASTM A240 UNS S31060 Weldability

 

The low carbon content (≤ 0.08%) of ASME SA240/ASTM A240 UNS S31060 ensures good weldability by minimizing carbide precipitation and intergranular corrosion during welding, making it more weldable than sa 240/a 240 uns s31041. It can be welded using common techniques such as TIG, MIG, and shielded metal arc welding, with appropriate filler materials (e.g., 310S-specific fillers) to maintain corrosion resistance and strength. Compared to sa 240/a 240 uns s31040, UNS S31060 is slightly less weldable due to the absence of niobium stabilization but is more cost-effective. For applications requiring superior weldability, sa 240/a 240 uns s31050 is a better choice.

Keywords: ASME SA240/ASTM A240 UNS S31060 weldability, UNS S31060 welding properties, 310S weldability


ASME SA240/ASTM A240 UNS S31060 Stainless Steel Surface

 

The surface finish of ASME SA240/ASTM A240 UNS S31060 stainless steel sheet significantly impacts its aesthetic appeal, functionality, and application suitability. Gangsteel offers a variety of surface finishes to meet diverse project requirements, as detailed below:

Surface Finish

Definition/Feature

Summary of Manufacturing Method

Application/Use

NO.1

Silver white, matte

Hot rolled to specified thickness, followed by heat treatment and pickling

Chemical tank, pipe, no need for surface gloss purposes

2B

Stronger gloss than NO.2D

Cold rolled, heat treated, pickled, and lightly cold rolled by polishing rollers

Medical equipment, food industry, construction material, kitchen utensils, general materials

NO.2D/2BB

Silver white

Heat treatment and pickling after cold rolling

General materials, deep drawing materials

NO.3

Rough grinding

Polished with No.100 to No.120 abrasives (JIS R6001) or 100~200# grinding belt

Kitchen utensils, building construction, building materials

NO.4 (4K)

Intermediate grinding

Polished with No.150 to No.180 abrasives (JIS R6001) or 150~180# stone abrasive belt

Kitchen utensils, building construction, medical equipment, building materials

NO.240

Fine grinding

Grinding with 240# stone abrasive belt

Kitchenware

NO.320

Very fine grinding

Grinding with 320# abrasive belt

Kitchenware

NO.400

Gloss close to BA

Grinding with 400# polishing wheel

General timber, construction timber, kitchen utensils

HL

Hairline grinding, continuous polishing streaks

Polished with suitable grain size abrasive (150~240#) for hairline grinding

Building construction, buildings, construction materials

BA (No.6/BA1/BA0)

Bright as a mirror

Bright heat treatment after cold rolling, high surface reflectivity

Kitchen utensils, electric equipment, building construction, building materials

NO.7

Close to mirror polishing

Grinding with 600# rotary polishing wheel

For art and decoration

NO.8 (Mirror/8K)

Shining like a mirror

Grinding mirrors with polishing wheels

Building construction, reflector, for decoration

These surface finishes allow sa 240/a 240 uns s31060 to be tailored for aesthetic or functional requirements, such as the NO.1 finish for furnace components or the 2B finish for petrochemical applications.

Keywords: ASME SA240/ASTM A240 UNS S31060 surface finish, UNS S31060 stainless steel surface, 310S surface finishes


ASME SA240/ASTM A240 UNS S31060 Chemical Composition

 

The ASME SA240/ASTM A240 UNS S31060 chemical composition is optimized for high-temperature corrosion resistance and weldability, compliant with sa 240/a 240 uns stainless grades standards.

The high chromium (24.0-26.0%) and nickel (19.0-22.0%) content, combined with low carbon (≤ 0.08%), provide excellent corrosion resistance and weldability compared to sa 240/a 240 uns s31041.

Element

Percentage (%)

Chromium (Cr)

24.0 – 26.0

Nickel (Ni)

19.0 – 22.0

Carbon (C)

≤ 0.08

Manganese (Mn)

≤ 2.0

Silicon (Si)

≤ 1.50

Phosphorus (P)

≤ 0.045

Sulfur (S)

≤ 0.030

Iron (Fe)

Balance (~55%)

Keywords: ASME SA240/ASTM A240 UNS S31060 chemical composition, UNS S31060 composition, 310S chemistry, ASME SA240 Gr S31060 composition


ASME SA240/ASTM A240 UNS S31060 Mechanical Properties

 

The ASME SA240/ASTM A240 UNS S31060 mechanical properties offer a balance of moderate strength, good ductility, and excellent high-temperature corrosion resistance, suitable for high-temperature applications.

These properties ensure that ASME SA240/ASTM A240 UNS S31060 stainless steel sheet can withstand mechanical stresses in high-temperature environments. Solution annealing at 1040-1120°C (1904-2048°F) optimizes UNS S31060 mechanical properties for corrosion resistance and weldability.

Property

Value at 20°C

Tensile Strength (MPa)

≥ 515 (75 ksi)

Yield Strength (MPa)

≥ 205 (30 ksi)

Elongation (%)

≥ 40

Hardness (HBW)

≤ 217

Density

7.89 g/cm³ (0.285 lb/in³)

At Gangsteel, we’ve seen clients use sa 240/a 240 uns s31060 sheets in petrochemical reactors, where its corrosion resistance and weldability provide advantages over sa 240/a 240 uns s30909.

Keywords: ASME SA240/ASTM A240 UNS S31060 mechanical properties, UNS S31060 strength, 310S mechanical properties, ASME SA240 Gr S31060 mechanical properties


ASME SA240/ASTM A240 UNS S31060 Specifications and Forms

 

As a trusted uns stainless supplier, Gangsteel supplies sa 240/a 240 uns s31060 sheets, plates, coils, bars, and custom components, compliant with sa 240/a 240 uns stainless grades standards:

Our advanced manufacturing facilities ensure precision and quality, meeting the diverse needs of global projects, from standard sizes to custom-cut components.

Sheet and Plate

  • Thickness: 0.1 mm to 6 mm (sheet), 0.5 mm to 50 mm (plate)
  • Width: Up to 2000 mm
  • Length: 2000 mm to 12000 mm (or coiled for sheet)
  • Surface Finish: Hot-rolled, cold-rolled, annealed, pickled, 2B, No.1, No.4, BA, or customized (see Stainless Steel Surface section)
  • Standards: ASTM A240, ASME SA240
  • Applications: sa 240/a 240 uns s31060 sheets for heat exchanger tubes, UNS S31060 plates for furnace components

Coil

  • Thickness: 0.1 mm to 6 mm
  • Width: Up to 2000 mm
  • Standards: ASTM A240, ASME SA240
  • Applications: Continuous production for welded pipes and high-temperature components

Bar

  • Diameter: 6 mm to 300 mm
  • Length: Up to 12000 mm
  • Finish: Hot-rolled, cold-drawn, centerless ground
  • Standards: ASTM A479, ASME SA-479
  • Applications: ASME SA240/ASTM A240 UNS S31060 bars for structural components

Custom Components

  • Types: Flanges (ASME B16.5), fittings, CNC-machined parts, stainless cutting sheet part
  • Tolerances: ±0.05 mm for precision components
  • Applications: Tailored solutions for petrochemical and power generation industries

Note: Need a specific size or finish? Gangsteel offers custom solutions, including precision cutting and heat treatments, to meet sa 240/a 240 uns stainless grades requirements. Contact us at admin@gangsteel.com for bespoke ASME SA240/ASTM A240 UNS S31060 material specifications.

Keywords: ASME SA240/ASTM A240 UNS S31060 stainless steel sheet specifications, UNS S31060 sheet specifications, ASME SA 240 Gr S31060 coil, ASME SA 240 Gr S31060 bar


Applications of ASME SA240/ASTM A240 UNS S31060 Stainless Steel Sheet

 

ASME SA240/ASTM A240 UNS S31060 stainless steel sheetis tailored for industries requiring excellent high-temperature corrosion resistance and good weldability. Its low-carbon austenitic structure ensures durability in demanding environments.

Key ASME SA240/ASTM A240 UNS S31060 applications include:

  • Petrochemical: sa 240/a 240 uns s31060 sheets for welded reactors and heat exchanger tubes.
  • Power Generation: UNS S31060 plates for boiler components and furnace linings.
  • Furnace Manufacturing: ASME SA240/ASTM A240 UNS S31060 bars for high-temperature furnace components.
  • Chemical Processing: Piping and fittings for high-temperature applications.
  • General-Purpose: Welded components requiring corrosion resistance and high-temperature performance.

Case Study: A power generation facility in India used sa 240/a 240 uns s31060 sheets for boiler tubes, achieving a 15% cost reduction compared to sa 240/a 240 uns s31050 while maintaining reliable high-temperature performance.

Keywords: ASME SA240/ASTM A240 UNS S31060 applications, UNS S31060 uses, 310S applications, ASME SA240 Gr S31060 applications


ASME SA240/ASTM A240 UNS S31060 vs Related Grades

 

To aid in material selection, here’s a comparison of sa 240/a 240 uns s31060 with sa 240/a 240 uns s30615, sa 240/a 240 uns s30815, sa 240/a 240 uns s30909, sa 240/a 240 uns s30940, sa 240/a 240 uns s31040, sa 240/a 240 uns s31041, sa 240/a 240 uns s31050, sa 240/a 240 uns s31254, and sa 240/a 240 uns s31266:

This comparison highlights the unique advantages of each grade, helping you select the optimal material for your project requirements.

Property

ASME SA240/ASTM A240 UNS S31060

ASME SA240 UNS S30615

ASME SA240 UNS S30815

ASME SA240 UNS S30909

ASME SA240 UNS S30940

ASME SA240 UNS S31040

ASME SA240 UNS S31041

ASME SA240 UNS S31050

ASME SA240 UNS S31254

ASME SA240 UNS S31266

UNS Number

S31060

S30615

S30815

S30909

S30940

S31040

S31041

S31050

S31254

S31266

Type

Austenitic

Austenitic

Austenitic

Austenitic

Austenitic

Austenitic

Austenitic

Austenitic

Austenitic

Austenitic

Chromium Content

24.0-26.0%

18.0-19.5%

20.0-22.0%

22.0-24.0%

22.0-24.0%

24.0-26.0%

24.0-26.0%

24.0-26.0%

19.5-20.5%

23.0-25.0%

Nickel Content

19.0-22.0%

13.5-15.0%

10.0-12.0%

12.0-15.0%

12.0-15.0%

19.0-22.0%

19.0-22.0%

21.0-23.0%

17.5-18.5%

21.0-24.0%

Manganese Content

≤ 2.0

≤ 2.0

≤ 0.80

≤ 2.0

≤ 2.0

≤ 2.0

≤ 2.0

≤ 2.0

≤ 1.0

≤ 2.0

Molybdenum Content

-

0.80-1.20%

-

-

-

-

-

2.0-3.0%

6.0-6.5%

5.2-6.2%

Nitrogen Content

-

0.15-0.25%

0.14-0.20%

-

-

-

-

0.10-0.16%

0.18-0.22%

0.35-0.60%

Carbon Content

≤ 0.08%

≤ 0.05%

0.05-0.10%

0.04-0.10%

≤ 0.08%

≤ 0.08%

0.04-0.10%

≤ 0.030%

≤ 0.020%

≤ 0.020%

Corrosion Resistance

Good in high-temperature environments

Excellent in high-temperature environments

Excellent in high-temperature environments

Good in high-temperature environments

Good in high-temperature environments

Good in high-temperature environments

Good in high-temperature environments

Excellent in chemical environments

Exceptional in chloride environments

Exceptional in severe corrosive environments

Strength

Moderate

High (High-temperature)

High (High-temperature)

High (High-temperature)

Moderate

Moderate

High (High-temperature)

High (Chemical resistance)

High (Corrosion resistance)

Very High (Corrosion resistance)

Temp Range

Up to 1100°C (2012°F)

Up to 950°C (1742°F)

Up to 1150°C (2102°F)

Up to 1000°C (1832°F)

Up to 1000°C (1832°F)

Up to 1100°C (2012°F)

Up to 1100°C (2012°F)

Up to 1100°C (2012°F)

Up to 400°C (752°F)

Up to 400°C (752°F)

Cost (USD/kg)

6-9

6-9

6-9

5-8

5-8

6-9

6-9

7-10

8-12

9-14

Applications

High-temperature equipment

High-temperature equipment, chemical processing

Furnace components, petrochemical

Heat exchangers, furnace components

High-temperature welded structures

High-temperature welded structures

High-temperature equipment

Chemical processing, high-temperature

Marine, chemical processing

Severe corrosive environments, marine

  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30615: S31060 offers higher chromium and nickel for better high-temperature corrosion resistance, while sa 240/a 240 uns s30615 provides better corrosion resistance in moderately corrosive environments due to molybdenum.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30815: S31060 is more cost-effective and weldable, while sa 240/a 240 uns s30815 offers superior high-temperature strength and oxidation resistance due to cerium.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30909: S31060 provides better weldability due to lower carbon content, while sa 240/a 240 uns s30909 offers higher high-temperature strength.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30940: S31060 offers higher chromium and nickel for better corrosion resistance, while sa 240/a 240 uns s30940 is more cost-effective for similar applications.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31040: S31060 is more cost-effective, while sa 240/a 240 uns s31040 offers better weldability due to niobium stabilization.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31041: S31060 provides better weldability due to lower carbon content, while sa 240/a 240 uns s31041 offers higher high-temperature strength.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31050: S31060 is more cost-effective for high-temperature applications, while sa 240/a 240 uns s31050 excels in chemical environments due to molybdenum.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31254: S31060 is optimized for high-temperature environments, while sa 240/a 240 uns s31254 provides exceptional corrosion resistance in chloride environments.
  • ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31266: S31060 is more cost-effective for high-temperature applications, while sa 240/a 240 uns s31266 offers superior corrosion resistance in severe environments.

Conclusion: Choose sa 240/a 240 uns s31060 for cost-effective, high-temperature corrosion-resistant applications, sa 240/a 240 uns s30615 or sa 240/a 240 uns s30815 for high-temperature oxidation resistance, sa 240/a 240 uns s30909 or sa 240/a 240 uns s31041 for high-temperature strength, sa 240/a 240 uns s30940 or sa 240/a 240 uns s31040 for weldable high-temperature structures, or sa 240/a 240 uns s31050, sa 240/a 240 uns s31254, or sa 240/a 240 uns s31266 for corrosion-resistant applications.

Keywords: ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30615, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30815, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30909, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S30940, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31040, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31041, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31050, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31254, ASME SA240/ASTM A240 UNS S31060 vs ASME SA240 UNS S31266, 310S comparison


ASME SA240/ASTM A240 UNS S31060 Equivalent Materials

 

ASME SA240/ASTM A240 UNS S31060aligns with international standards for global compatibility, ensuring seamless integration into projects worldwide.

The equivalent grades allow for flexibility in sourcing materials across different regions, making ASME SA240/ASTM A240 UNS S31060 a versatile choice for high-temperature applications.

Standard

Grade

UNS

S31060

W.Nr.

1.4845

EN

X8CrNi25-21

ASTM

A240

ASME

SA240

Note: ASME SA240/ASTM A240 UNS S31060 equivalent grades comply with sa 240/a 240 uns stainless grades standards, offering interchangeability with sa 240/a 240 uns s31040 for similar applications.

Keywords: ASME SA240/ASTM A240 UNS S31060 equivalent, UNS S31060 equivalent, ASME SA 240 Gr S31060 material standards, EN X8CrNi25-21


ASME SA240/ASTM A240 UNS S31060 Allowable Stress

 

The allowable stress values for ASME SA240/ASTM A240 UNS S31060, per ASME BPVC Section II, Part D, ensure reliable performance in high-temperature environments.

These values reflect the material’s ability to withstand mechanical stresses at elevated temperatures while maintaining corrosion resistance.

Temperature (°C)

Allowable Stress (MPa)

100

130

200

120

300

110

400

100

500

90

Note: These values ensure sa 240/a 240 uns s31060 performs reliably in petrochemical and furnace applications.

Keywords: ASME SA240/ASTM A240 UNS S31060 allowable stress, UNS S31060 strength, ASME SA240 Gr S31060 material stress


ASME SA240/ASTM A240 UNS S31060 Price

 

The ASME SA240/ASTM A240 UNS S31060 price per kg ranges from USD 6-9 per kg (FOB), influenced by several factors:

The excellent high-temperature corrosion resistance and weldability of ASME SA240/ASTM A240 UNS S31060 make it a valuable choice for petrochemical and power generation applications.

  • Alloy Content: High chromium and nickel content increase costs compared to sa 240/a 240 uns s30940 but reduce costs compared to sa 240/a 240 uns s31050.
  • Market Demand: High demand in petrochemical and furnace industries drives UNS S31060 price.
  • Product Form: ASME SA240/ASTM A240 UNS S31060 sheets may cost more than coils due to processing complexity.
  • Global Supply Chain: Freight and raw material availability impact ASME SA240/ASTM A240 UNS S31060 cost.

For a precise ASME SA240/ASTM A240 UNS S31060 price per kg or bulk discounts, contact Gangsteel at admin@gangsteel.com.

Keywords: ASME SA240/ASTM A240 UNS S31060 price per kg, UNS S31060 cost, 310S price


Related Stainless Steel Grades

 

As a leading uns stainless supplier, Gangsteel offers a wide range of sa 240/a 240 uns stainless grades to complement sa 240/a 240 uns s31060 for various applications:

This diverse portfolio ensures clients can find the ideal material for their specific project needs, from corrosion resistance to high-temperature performance.

Note: These grades complement sa 240/a 240 uns s31060 in high-temperature and corrosion-resistant applications. Contact Gangsteel for a full catalog to find the perfect material for your project.

Keywords: ASME SA240/ASTM A240 UNS S31060 related grades, UNS S31060 stainless steel grades, 310S grades


FAQ

 

Q: What is the main difference between ASME SA240/ASTM A240 UNS S31060 and ASME SA240 UNS S31050?

A: ASME SA240/ASTM A240 UNS S31060 is more cost-effective for high-temperature applications, while sa 240/a 240 uns s31050 offers superior corrosion resistance and weldability due to molybdenum and nitrogen additions.

Q: Is ASME SA240/ASTM A240 UNS S31060 suitable for furnace applications?

A: Yes, its excellent high-temperature corrosion resistance and good weldability make it ideal for furnace components compared to sa 240/a 240 uns s30909.

Q: How does the price of ASME SA240/ASTM A240 UNS S31060 compare to ASME SA240 UNS S31050?

A: ASME SA240/ASTM A240 UNS S31060 is typically 20-30% less expensive than sa 240/a 240 uns s31050 due to the absence of molybdenum, offering cost-effective performance for high-temperature applications.

Keywords: ASME SA240/ASTM A240 UNS S31060 FAQ, UNS S31060 stainless steel questions, 310S FAQ


Contact Us

 

For sa 240/a 240 uns s31060 quotes, technical data sheets, or custom solutions, contact Gangsteel at admin@gangsteel.com. Explore our sa 240/a 240 uns stainless grades portfolio for more options.

Keywords: ASME SA240/ASTM A240 UNS S31060 supplier, Gangsteel stainless steel exporter, UNS S31060 sheet supplier

 

Other Products