GB/T 713 Q345R steel plate

GB/T 713 Q345R steel plate, also written as Q345R pressure vessel steel plate, GB713 Q345R, Q345R boiler steel plate, formerly 16MnR, is a C-Mn pressure vessel / boiler plate grade under GB/T 713 / GB/T 713.2. Minimum yield is 345 MPa for thickness 3–16 mm, tensile typically 510-640 MPa in that band, with Charpy V-notch at 0°C. Gangsteel (HENAN GANG IRON AND STEEL) produces and exports Q345R plates cut to size with mill test certificates for boilers, pressure vessels, heat exchangers and petrochemical equipment.

Data source: Per GB/T 713 / GB/T 713.2-2023 (Steel plate, sheet and strip for pressure equipments — Part 2: Non-alloy and alloy steel with specified temperature properties; buyers still search “GB/T 713”). Official mill/certificate grade is Q345R. Verify the contracted edition and purchase-order supplements before ordering.

GB/T 713 Q345R Chemical Composition (Heat Analysis)

 

ElementCSiMnPSAlt
Q345R, %0.20 max0.55 max1.20-1.700.025 max0.010 maxper edition
ElementCuNiCrMoNbV/Ti
Q345R, %0.30 max0.30 max0.30 max0.08 max0.050 max0.050/0.030 max

Per GB/T 713.2 heat analysis. Cu+Ni+Cr+Mo ≤0.70%. For t>60 mm, C upper limit may rise to 0.22%.

GB/T 713 Q345R Mechanical Properties

 

ThicknessYield ReL, minTensile RmElongation A, minImpact KV2
3–16 mm345 MPa510-640 MPa21%0°C, ≥41 J
>16–36 mm325 MPa500-630 MPa21%0°C, ≥41 J
>36–60 mm315 MPa490-620 MPa21%0°C, ≥41 J
>60–100 mm305 MPa490-620 MPa20%0°C, ≥41 J
>100–150 mm285 MPa480-610 MPa20%0°C, ≥41 J
>150–250 mm265 MPa470-600 MPa20%0°C, ≥40 J

Per GB/T 713.2. Use Rp0.2 when yield is not distinct. -20°C impact may replace 0°C when specified.

Delivery Condition, Heat Treatment and Tests

Hot-rolled, normalized-rolled, normalized, or normalized + tempered by thickness and order. Killed steel. Optional UT, Z-test, HIC/NACE, elevated-temperature tensile, PWHT simulation and 3.1/3.2 MTC.

Thickness and Size Coverage

Commonly 6–200 mm (up to 250 mm by edition/capability), width 1500-4000 mm, length 6000-18000 mm.

Applications of GB/T 713 Q345R

Workhorse Chinese C-Mn plate for medium/high-pressure boilers, vessels, heat exchangers, separators, reactors, tanks and petrochemical equipment.

Equivalent / Related Grades of GB/T 713 Q345R

 

StandardComparable grade (approximate)
GB/T 713Q345R
ASTM/ASMEASTM A516 / A516 Grade 70 / SA516 Gr.70 (approx.; dual cert by agreement)
EN 10028-2P265GH / P355GH family (approx.)
Related GB/T 713Q245R | Q370R | Q420R | Q460R | 18MnMoNbR

Equivalents are engineering references only. Dual certification requires the stricter combined limits on the PO and MTC.

FAQ about GB/T 713 Q345R Steel Plate

What is GB/T 713 Q345R steel plate?

It is a C-Mn boiler and pressure vessel steel under GB/T 713 / GB/T 713.2. a C-Mn pressure vessel / boiler plate grade under GB/T 713 / GB/T 713.2. Minimum yield is 345 MPa for thickness 3–16 mm, tensile typically 510-640 MPa in that band, with Charpy V-notch at 0°C. Gangsteel lists the official mill/certificate grade as Q345R. See the full GB/T 713 Q345R page for chemistry and mechanical tables.

What is the yield and tensile strength of Q345R?

345 MPa min at 3–16 mm; 325/315/305/285/265 MPa in thicker bands up to 250 mm. Typical tensile bands are shown in the mechanical properties table on this page; confirm the contracted GB/T 713.2 edition before design.

What impact test temperature applies to GB/T 713 Q345R?

0°C standard (KV2 typically ≥41 J); -20°C by agreement. Always state the required Charpy temperature and energy on the purchase order.

What delivery condition / heat treatment does Q345R use?

Hot-rolled, normalized-rolled, normalized, or normalized + tempered by thickness and order. Killed steel. Optional UT, Z-test, HIC/NACE, elevated-temperature tensile, PWHT simulation and 3.1/3.2 MTC.

How does Q345R compare with other GB/T 713 QxxxR grades?

All sit in the GB/T 713.2 non-alloy / microalloy vessel family. Sister carbon grades: Q245R / Q370R / Q420R / Q460R. Hub: GB/T 713 Steel Plate.

Is Q345R the same as ASTM A516 / ASME SA516?

No. They are often compared for design but chemistry, impact and delivery rules differ. See ASTM A516 and A516 Grade 70 / SA516 Gr.70. Dual certification needs the stricter combined limits on the PO and MTC.

What mill certificate does Gangsteel supply for Q345R?

EN 10204 3.1 as standard; 3.2 with third-party inspection when ordered. MTC lists heat analysis, mechanical tests, delivery condition and any optional UT / Z / HIC / elevated-temperature results.

What thickness can Gangsteel produce for Q345R?

Commonly 6–200 mm (up to 250 mm by edition/capability), width 1500-4000 mm, length 6000-18000 mm. Browse the GB/T 713 hub for the full grade list.

Related GB/T 713 / Pressure Vessel Grades

GB/T 713 Steel Plate | Q345R | Q245R | 15CrMoR | ASTM A516 | ASTM A387 | ASTM A537 | Pressure Vessel Steel Plate | Boiler Steel Plate