EN 10025-3 S460NL Standard Overview
At Gangsteel, we’re excited to share the key details of the EN 10025-3 S460NL standard, a cornerstone for high-strength, low-alloy structural steel designed for demanding applications in cold climates. S460NL, part of the en 10025 3 normalized steel plate family, is normalized or normalized rolled to deliver a fine-grain structure, making it ideal for offshore platforms, bridges, and wind turbine towers.
Gangsteel breaks down the EN 10025-3 S460NL standard, covering its specifications, chemical composition, mechanical properties, and applications, with comparisons to grades like en 10025 3 s420nl normalized structural steel plate and en 10025 3 s355nl normalized structural steel plate. For more details, visit our en 10025 3 s460nl normalized structural steel plate page.
What is the EN 10025-3 S460NL Standard?
The EN 10025-3 S460NL standard specifies a high-strength structural steel with a minimum yield strength of 460 MPa for plates up to 16 mm thick. Its designation breaks down as:
- S: Structural steel.
- 460: Minimum yield strength in MPa.
- NL: Normalized or normalized rolled, tested for impact toughness at -50°C.
This standard ensures a fine-grain microstructure for superior strength, toughness, and weldability, making EN 10025-3 S460NL ideal for cold environments. Compared to en 10025 3 s355nl normalized structural steel plate, S460NL offers higher strength for heavier structural demands.
Chemical Composition in the EN 10025-3 S460NL Standard
The EN 10025-3 S460NL standard defines a chemical composition optimized for strength and cold-weather performance:
|
Element |
Ladle Analysis (max %) |
Product Analysis (max %) |
|---|---|---|
|
Carbon (C) |
0.20 |
0.22 |
|
Silicon (Si) |
0.60 |
0.65 |
|
Manganese (Mn) |
1.00-1.70 |
0.95-1.80 |
|
Phosphorus (P) |
0.025 |
0.030 |
|
Sulfur (S) |
0.020 |
0.025 |
|
Nitrogen (N) |
0.025 |
0.027 |
|
Aluminum (Al) |
0.020 (min, total) |
0.015 (min, total) |
|
Niobium (Nb) |
0.05 |
0.06 |
|
Vanadium (V) |
0.20 |
0.22 |
|
Titanium (Ti) |
0.05 |
0.06 |
|
Chromium (Cr) |
0.30 |
0.35 |
|
Nickel (Ni) |
0.80 |
0.85 |
|
Molybdenum (Mo) |
0.10 |
0.12 |
|
Copper (Cu) |
0.55 |
0.60 |
Key Elements:
- Low Carbon: 0.20% max ensures clean welds and toughness.
- Manganese: 1.00-1.70% boosts strength for heavy structures.
- Aluminum & Niobium: Refine grains for -50°C toughness, a hallmark of EN 10025-3 S460NL.
- Low Sulfur & Phosphorus: Minimize inclusions for superior weld quality.
The Carbon Equivalent (CEV) is
capped at 0.48% for plates up to 63 mm, calculated as CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15, ensuring weldability, similar to en 10025 3 s420nl normalized structural steel plate.
Mechanical Properties in the EN 10025-3 S460NL Standard
The EN 10025-3 S460NL standard specifies mechanical properties for high-strength applications:
|
Thickness (mm) |
Yield Strength (min, MPa) |
Tensile Strength (MPa) |
Elongation (min, %) |
Impact Energy (min, J @ -50°C) |
|---|---|---|---|---|
|
≤16 |
460 |
540-720 |
17 |
27 |
|
16<t≤40 |
440 |
540-720 |
17 |
27 |
|
40<t≤63 |
430 |
540-720 |
17 |
27 |
|
63<t≤80 |
410 |
540-720 |
17 |
27 |
|
80<t≤100 |
400 |
540-720 |
17 |
27 |
|
100<t≤150 |
380 |
520-680 |
17 |
27 |
|
150<t≤200 |
370 |
520-680 |
17 |
27 |
- Yield Strength: Starts at 460 MPa for thin plates, ideal for heavy loads in structures like offshore platforms.
- Tensile Strength: 540-720 MPa ensures durability under high tensile forces.
- Elongation: ≥17% supports complex structural designs.
- Impact Toughness: ≥27 J at -50°C ensures reliability in cold climates, outperforming en 10025 3 s355n normalized structural steel plate.
- Hardness: Typically 170-210 HB (Brinell), balancing machinability and durability.
Delivery Conditions and Specifications
The EN 10025-3 S460NL standard includes:
- Standard: EN 10025-3:2019.
- Condition: Normalized or normalized rolled for consistent microstructure.
- Thickness Range: 6–200 mm, with custom options up to 250 mm.
- Widths: 2000, 2500, or 3000 mm.
- Lengths: Up to 12,000 mm.
- Surface: Hot-rolled, with optional priming for corrosion protection.
- Certifications: EN 10204 3.1/3.2 certificates, ultrasonic testing (UT) per EN 10160, and approvals from ABS, LR, BV, or DNV for marine and structural use.
- Z-Quality: Optional Z15, Z25, or Z35 per EN 10164 for through-thickness properties, reducing lamellar tearing risk, similar to en 10025 3 s420n normalized structural steel plate.
- Tolerances: Per EN 10029 for thickness, width, and length, ensuring precision.
Welding and Heat Treatment
The EN 10025-3 S460NL standard ensures excellent weldability with a low CEV (≤0.48%):
- Welding: Compatible with GMAW and SAW per EN 1011-2. Preheating (100-150°C) for plates >20 mm; post-weld heat treatment (PWHT) at 550-650°C optional for critical welds.
- Consumables: ER70S-6 for GMAW, EM12K flux with EH14 wire for SAW.
- Weld Quality: Matches en 10025 3 s460n normalized structural steel plate for reliable, high-strength joints.
The fine-grain structure and low impurities ensure minimal weld imperfections.
Applications in the EN 10025-3 S460NL Standard
The EN 10025-3 S460NL standard supports applications in:
- Offshore Platforms: Built for Arctic marine conditions with -50°C toughness.
- Wind Turbine Towers: Resists cyclic loads in cold climates like northern Europe.
- Bridges and Cranes: Load-bearing components in northern regions, such as Scandinavia.
- Heavy Machinery: Strong structural parts for extreme environments.
For less demanding projects, consider en 10025 3 s275nl normalized structural steel plate.
Why Choose Gangsteel?
Gangsteel is your trusted source for EN 10025-3 S460NL:
- Inventory: Extensive stock in China for rapid delivery.
- Sizes: Thicknesses from 6–200 mm, widths up to 3000 mm, lengths up to 12,000 mm.
- Delivery: Ships globally in 7-30 days.
- Certifications: EN 10204 3.1/3.2, UT testing (EN 10160), and ABS/LR/BV/DNV approvals.
- Processing: Cutting, welding, and bending tailored to your project needs.
Contact us for en 10025 3 s460nl normalized structural steel plate.
FAQ
What is the EN 10025-3 S460NL standard?
The EN 10025-3 S460NL standard specifies a high-strength steel with ≥460 MPa yield strength and -50°C toughness, ideal for cold-climate structures like offshore platforms.
What are the key properties in the EN 10025-3 S460NL standard?
The EN 10025-3 S460NL standard includes a yield strength of ≥460 MPa, tensile strength of 540-720 MPa, ≥17% elongation, and ≥27 J impact toughness at -50°C.
Is EN 10025-3 S460NL weldable?
Yes, the EN 10025-3 S460NL standard specifies a CEV ≤0.48%, enabling easy welding with GMAW or SAW and preheating (100-150°C for >20 mm) for strong joints.
What applications are covered by the EN 10025-3 S460NL standard?
The EN 10025-3 S460NL standard supports offshore platforms, wind towers, bridges, and cranes in cold climates, leveraging its strength and toughness.
How does EN 10025-3 S460NL compare to S355NL?
The EN 10025-3 S460NL standard specifies higher yield strength (460 MPa vs 355 MPa) than S355NL, with similar -50°C toughness, for more demanding projects.
What certifications support the EN 10025-3 S460NL standard?
Gangsteel provides EN 10025-3 S460NL with EN 10204 3.1/3.2, UT testing (EN 10160), and ABS/LR/BV/DNV approvals, ensuring compliance for global projects.
-
BHW35 Steel Plate for Sale | RF
BHW35 / 13MnNiMo5-4 (DIWA 353 family): identity, chemistry, mechanical properties, related grades, and RFQ note
-
ASTM A516 Grade 70 Equivalent:
ASTM A516 Grade 70 equivalents include ASME SA516 Gr 70, EN 10028-2 P355GH and BS 1501 224-490. Gangsteel compa
-
What is the difference between
we supply high-quality A516 Gr 70 steel plate for pressure vessel applications and other standards like ASTM A2
-
P355GH AND S355J2 Steel Plates
EN10028-2 P355GH for High-Strength Low-Alloy Columbium-Vanadium Structural Steel EN10025-2 S355J2 Structural St