Product List
Gangsteel Material Solution
Email: admin@gangsteel.com
Sales: jack@gangsteel.com
Gangsteel – China's Leading Mill-Direct Supplier & Exporter of EN 10025-4 S275ML Thermomechanically Rolled Weldable Fine Grain Structural Steel Plates
As a seasoned Chinese steel exporter dedicated to empowering global builders with dependable materials, Gangsteel stocks premium en 10025 4 s275ml steel plate from our expansive 15,000+ ton inventory. EN 10025-4 S275ML is a foundational high-strength, fine-grain structural steel developed through TMCP (Thermomechanical Controlled Processing), offering a minimum yield strength of 275 MPa and reliable low-temperature toughness to -50°C. Available in thicknesses 6–200 mm, widths up to 4200 mm, and lengths to 18 m, our plates are manufactured by top mills like HBIS and Baowu, complete with PED/CE marking (2014/68/EU) and EN 10204-3.1/3.2 test reports. Third-party validations from DNV, ABS, Lloyd’s, BV, or TÜV ensure seamless integration into international standards.
EN 10025-4 S275ML is a thermomechanically rolled (TMCP) weldable fine-grain structural steel specified in the European EN 10025-4:2004 standard (updated 2019), designed for economical strength in cold-prone settings. The "S" denotes structural purpose, "275" the nominal yield in MPa for thin gauges, "M" the thermomechanical state, and "L" enhanced impact at -50°C (≥27J Charpy V-notch). TMCP—controlled deformation and cooling—forms a consistent ferrite structure, yielding 5–10% better performance than S235JR or S275J0 in EN 10025-2, with 8–12% thinner sections for lighter footprints.
Core strengths include low carbon equivalent (CEV ≤ 0.38) for welding without preheat up to 100 mm thick, strong HAZ crack resistance, and optional Z-direction (Z25/Z35) to avoid delamination in joints. Unlike normalized EN 10025-3 S275NL, S275M's TMCP reduces stresses and improves uniformity for mild dynamics. It meets Eurocode 3 and EN 1090 for fabrication, powering from refrigerated warehouses to basic marine aids. Gangsteel focuses on S275ML stock (key 10–70 mm thick) for fast 3–7 day delivery, supporting ventures like Nordic storage and coastal walkways.
This grade's value stems from its budget-friendly entry to TMCP benefits, ideal for SMEs where S355ML might over-spec at 25–35% higher cost. S275ML's high elongation (≥24%) suits cold forming (radius 2t), perfect for prefab in housing surges. Amid volatile markets, Gangsteel's mill links stabilize supply, with digital MTCs for full provenance.
S275ML's makeup stresses cleanliness and balance, limiting P/S for toughness, with light alloying for weld synergy. Al-killed for sparse oxides.
|
Element |
C |
Si |
Mn |
P |
S |
Nb |
V |
Al min |
Ti |
Cr |
Ni |
Mo |
Cu |
N |
CEV max |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
|
S275ML |
0.13 |
0.50 |
1.50 |
0.025 |
0.020 |
≤0.05 |
≤0.08 |
0.020 |
≤0.05 |
≤0.30 |
≤0.30 |
≤0.10 |
≤0.55 |
≤0.015 |
0.38 |
*CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; typical 0.27–0.33 for easy multi-run with E43xx. Nb/V pin grains to ASTM 10–12 for -50°C hold. For standard temp, see en 10025 4 s275m steel plate. Ca-Si optional for shape control, boosting feed rates.
S275ML's TMCP crafts a bendable matrix with pearlite aids, locking ReH and KV <4% scatter. Transverse confirmed; longitudinal 4–8% superior.
|
Thickness (mm) |
Yield Strength ReH (MPa) min |
Tensile Strength Rm (MPa) |
Elongation A5 (%) min |
Impact Energy KV2 (J, Long.) at -50°C min |
|---|---|---|---|---|
|
≤16 |
275 |
370–530 |
24 |
27 |
|
16<t≤40 |
265 |
370–530 |
24 |
27 |
|
40<t≤63 |
255 |
370–530 |
24 |
27 |
|
63<t≤100 |
235 |
370–530 |
25 |
27 |
|
100<t≤150 |
215 |
350–530 |
25 |
27 |
|
150<t≤200 |
195 |
350–530 |
26 |
27 |
Hardness: 115–155 HBW. DBTT < -50°C. Fatigue: 140 MPa (10^7 cycles, R=0). UT EN 10160 S1/E1; MT optional. S275M moves KV to -20°C ≥40J.
In EN 10025-4's TMCP spectrum, S275ML anchors the low-end with chill tolerance at entry pricing. This table juxtaposes it with peers—S275M (mild twin), S355M/ML (step-up), S420M/ML (elite)—focusing on power, cold hold, weld ease, and fit.
|
Property/Grade |
S275M |
S275ML |
S355M/ML |
S420M/ML |
|---|---|---|---|---|
|
Yield Strength (MPa, t≤16 mm) |
275 |
275 |
355 |
420 |
|
Impact Temp (Longitudinal) |
-20°C |
-50°C |
-20°C (M) / -50°C (ML) |
-20°C (M) / -50°C (ML) |
|
Min KV (J) |
40J |
27J |
40J / 27J |
40J / 27J |
|
CEV Max |
0.38 |
0.38 |
0.39 |
0.43 |
|
Elongation A5 Min (%) |
24 |
24 |
22 |
19 |
|
Tensile Range (MPa) |
370-530 |
370-530 |
470-630 |
520-680 |
|
Weld Preheat Threshold (mm, no preheat) |
Up to 100 |
Up to 100 |
Up to 80 |
Up to 60 |
|
Weight Saving vs. S275J2 |
8-12% |
8-12% |
15-20% |
20-25% |
|
Cost Premium vs. S275J2 (USD/ton) |
+30-50 |
+50-70 |
+80-120 |
+150-200 |
|
Primary Applications |
Light frames, sheds |
Cold storage, marine aids |
Bridges, wind bases |
Cranes, pipes |
|
Availability (Gangsteel Stock) |
Highest |
High |
Very High |
Medium |
S275ML trails S275M by 20 USD/ton sans chill, suiting frosty vaults over sheds, but trails S355ML's 30% yield for 15% thinner in trusses—at 40% cost bump. Vs. S420ML, it prioritizes stretch (higher A%) and weld (lower CEV) for light fab vs. heavies. S275ML grabs 35% of EN 10025-4's base share (Eurofer stats), Gangsteel's SME favorite.
S275ML matches ease global shifts, TMCP aiding rolled precision.
|
Standard |
Grade Equivalent |
Key Notes |
Typical Substitution Scenario |
|---|---|---|---|
|
ASTM/ASME |
A283 Gr.C + Z25 (carbon steel) |
Yield near; LT test for -40°C. |
US cold sheds, AISC basic. |
|
JIS G 3101 |
SS400 (mild) |
Base equiv; scale per JIS G 0404. |
Asian utility frames. |
|
GB/T 700 |
Q235D |
KV at -20°C; dual China-EU. |
Domestic chill with exports. |
|
BS EN 10025-2 |
S275J0 |
S275ML adds TMCP fine-grain. |
UK low-temp general. |
|
EN 10025-3 |
S275NL (N alt) |
ReH same; S275ML stress-low. |
Ambient to cold swaps. |
Note: Approxs; S275ML for -50°C. Related: en 10025 4 s275m steel plate.
S275ML's chill poise and yield simplify Eurocode 3 shear proofs, trimming 10% vs. S235J2 in braces while padding impacts. Key fields:
Tips: Use E31xx fillers; heat ≤1.8 kJ/cm HAZ. Form 1.8t cold; heat 700–850°C. Green: 100% recycle, 15% CO2 drop vs. HR TMCP. Gangsteel does plasma cuts (±1.5 mm) and zinc (35 µm) for fixings.
Gangsteel masters S275ML:
To 78+ hubs: Oslo (10 days), Vancouver (15 days), flexible.
Based on monthly export volumes to Europe, Middle East, and Asia-Pacific, these grades dominate inquiries. Each en 10025 4 High Strength Structural Steel variant is backed by immediate availability and custom processing.
Explore full specs, current pricing, and stock levels via our dedicated pages above.
Q1: S275ML from S275M?
A: KV only: S275ML ≥27J -50°C for ice, S275M ≥40J -20°C. Rest match—ML < -20°C EN 1991-1-3 snow.
Q2: S275ML preheat?
A: No; CEV ≤0.38 to 100 mm E43xx. Bulk: 40–90°C EN 1011. CET per batch PQR.
Q3: S275ML vessels?
A: Yes—PED I low EN 10028. t-scale; VI EN 10228.
Q4: S275ML vs. S235JR?
A: 50–70 USD/ton TMCP, 10% thin recoup. FOB: ~520–620 USD/ton (12 mm).
Q5: Z S275ML?
A: Z25 std; Z35 for pulls. EN 10164 Cl.1.
Q6: S275ML = A283C?
A: Yield akin (275 vs. 240 MPa); S275ML grain fine. AISC w/ LT.
Q7: S275ML custom?
A: Stock 1–3 days. Mod 2–4 days. Mill 3 weeks; rush <3 MT.
Join Gangsteel for EN 10025-4 S275ML ease.
Email: admin@gangsteel.com WhatsApp/WeChat/Mobile: +86 135 9887 9167 Website: https://gangsteel.net/
Gangsteel—Chill Foundations Firm. Stock solid, starts swift.
EN 10025-4 S355ML is a thermomechanically rolled (TMCP) weldable fine-grain structural steel defined by the Eur
EN 10025-4 S420ML is a thermomechanically rolled (TMCP) weldable fine-grain structural steel per the European E
EN 10025-4 S460ML is a thermomechanically rolled (TMCP) weldable fine-grain structural steel standard under the
EN 10025-4 S460M represents the pinnacle of thermomechanically rolled structural steels, offering superior stre