CCS FH40 (also written CCS/FH40, CCS Grade FH40, CCS F40 or FH40 steel plate) is a higher-strength hull structural steel plate certified by the China Classification Society (CCS) to CCS Rules for Materials and Welding (2024), Part 1, Chapter 3, Section 3. The figure 40 is the strength level (minimum yield 390 MPa, tensile 510–660 MPa) and the letter F sets the Charpy V-notch test temperature of −60°C. The steel is killed and fine-grain treated, and the grade corresponds to FH40 in IACS UR W11 and FH40 in ASTM A131.

Gangsteel, a steel plate exporter, supplies CCS FH40 plate with CCS class certificates; the requirements below are taken directly from the current CCS rules.

Related CCS grades: CCS AH40 steel plate, CCS DH40 steel plate, CCS EH40 steel plate, CCS FH32 steel plate, CCS FH36 steel plate.

CCS FH40 chemical composition

CCS FH40 chemical composition, heat (ladle) analysis, %
Element Heat analysis
C ≤ 0.16
Mn 0.90–1.60 (≥ 0.70 for t ≤ 12.5 mm)
Si ≤ 0.50
P ≤ 0.025
S ≤ 0.025
Al (acid soluble) ≥ 0.015
Nb 0.02–0.05
V 0.05–0.10
Ti ≤ 0.02
Nb + V + Ti ≤ 0.12
Cu ≤ 0.35
Cr ≤ 0.20
Ni ≤ 0.80
Mo ≤ 0.08
N ≤ 0.009 (≤ 0.012 if Al is present)

 

Source: CCS Rules for Materials and Welding (2024), Part 1, Chapter 3, Table 3.3.2.1. Al, Nb and V are grain-refining elements: when used in combination, the individual minimum contents do not apply. Total Al ≥ 0.020% may be reported instead of acid-soluble Al. TMCP plates must also meet the Ceq limits below. CCS specifies the chemical composition as a heat (ladle) analysis only; the Rules give no product (check) analysis tolerances for these plates, so no product-analysis column is shown. If a product analysis is required, agree the tolerances in the order.

CCS FH40 mechanical properties and impact test

CCS FH40 tensile and Charpy V-notch requirements
Grade Yield ReH min (MPa) Tensile Rm (MPa) Elongation A5 min (%) Test temp. KV avg min, t ≤ 50 mm, L / T (J) 50 < t ≤ 70 mm, L / T (J) 70 < t ≤ 150 mm, L / T (J)
CCS FH40 390 510–660 20 −60°C 39 / 26 46 / 31 55 / 37

Source: CCS Rules for Materials and Welding (2024), Part 1, Chapter 3, Table 3.3.4.3. L = longitudinal, T = transverse. Impact tests are normally made longitudinally; transverse values must be guaranteed by the mill.

CCS FH40 maximum carbon equivalent for TMCP plates
Thickness t ≤ 50 mm 50 < t ≤ 100 mm 100 < t ≤ 150 mm
Ceq max (%) 0.40 0.42 0.45

Ceq = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15, from the ladle analysis (Table 3.3.2.3(1)). For non-TMCP plates a Ceq limit may be agreed.

CCS FH40 thickness range and delivery condition

The CCS rules for CCS FH40 cover plates and wide flats up to 150 mm thick (sections and bars up to 50 mm). FH40 plates must be normalized or TMCP (or quenched and tempered), with an impact test on each piece. The required Charpy energy increases above 50 mm and again above 70 mm.

CCS FH40 equivalent grades

CCS FH40 equivalent grades of other classification societies
Standard / society Equivalent grade
IACS UR W11 FH40
ABS AB/FH40
DNV VL F40
LR LR FH40
BV BV FH40
ASTM A131 FH40
China GB/T 712 FH40

The IACS member societies use the same unified requirements, so these grades match in chemistry and properties. A plate still needs the certificate of the vessel’s own class society; one plate can carry dual or multiple class certification only when each society’s surveyor witnesses the tests.

CCS FH40 FAQ

What does FH40 mean?

F sets the toughness grade (Charpy test at −60°C), H means higher strength, and 40 is the strength level: minimum yield 390 MPa.

What is the yield strength of CCS FH40?

Minimum 390 MPa, tensile strength 510–660 MPa and minimum elongation 20%.

What is the impact test temperature of CCS FH40?

−60°C. Minimum average energy is 39 J longitudinal / 26 J transverse up to 50 mm, 46/31 J for 50–70 mm and 55/37 J for 70–150 mm.

What is CCS FH40 equivalent to?

FH40 of IACS UR W11, ABS AB/FH40, DNV VL F40, LR and BV FH40, ASTM A131 FH40 and GB/T 712 FH40.

What is the difference between AH40, DH40, EH40 and FH40?

They share the same chemistry limits (FH has tighter C, P and S limits, an N limit and a higher Ni allowance) and the same strength. Only the Charpy test temperature changes: 0°C (A), −20°C (D), −40°C (E) and −60°C (F).

What is the difference between CCS FH40 and ABS FH40?

Both are the same IACS UR W11 grade, so in practice they are interchangeable technically; the difference is the class certificate.

What is the carbon equivalent (CEV) of CCS FH40?

For TMCP plates Ceq must not exceed 0.40% up to 50 mm, 0.42% for 50–100 mm and 0.45% for 100–150 mm. For other conditions a Ceq limit may be agreed with the buyer.

What thickness range does CCS cover for FH40?

Plates and wide flats up to 150 mm; sections and bars up to 50 mm.

Equivalent steel grade of CCS/FH40

DNV

GL

LR

BV

RINA

NK

KR

ABS

NV F40

GL-F40

LR/FH40

BV/FH40

RI/F40

K F40

R F40

AB/F40

If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 Related steel grades: CCS/AH40, CCS/DH40, CCS/EH40, CCS/FH36

CCS Steel Plate Grade

General Strength

CCS/A

CCS/B

CCS/D

CCS/E

High Strength

CCS/A32

CCS/D32

CCS/E32

CCS/F32

CCS/A36

CCS/D36

CCS/E36

CCS/F36

CCS/A40

CCS/D40

CCS/E40

CCS/F40

Extra Strength

CCS/A420

CCS/D420

CCS/E420

CCS/F420

CCS/A460

CCS/D460

CCS/E460

CCS/F460

CCS/A500

CCS/D500

CCS/E500

CCS/F500

CCS/A550

CCS/D550

CCS/E550

CCS/F550

CCS/A620

CCS/D620

CCS/E620

CCS/F620

CCS/A690

CCS/D690

CCS/E690

CCS/F690

 

 

ASTM equivalent: ASTM A131 FH40 steel plate

LR equivalent: LR FH40 steel plate