BV FH40 steel plate, also written as BV/FH40, BV Grade FH40, Bureau Veritas FH40 or FH40 ship steel plate, is the higher-strength hull structural steel of Bureau Veritas Rules for the Classification of Steel Ships (IACS UR W11 higher-strength family) with 390 MPa minimum yield, 510-650 MPa tensile strength and Charpy V-notch toughness at -60°C [-76°F]. In the grade name, "F" is the toughness class, "H" means higher strength and "40" refers to the strength level (historically about 40 kgf/mm²). Gangsteel, a steel plate exporter, supplies BV FH40 / Grade FH40 plates cut to size for shipbuilding, offshore platforms and marine structures.

Data source: Per IACS UR W11 (ordinary/higher-strength hull structural steel) as adopted in Bureau Veritas hull structural steel rules. Official mill/certificate grade is BV FH40 (BV Grade FH40). Verify the current BV edition before ordering.

BV FH40 Chemical Composition (Heat Analysis)

 

ElementCMnSiPSAl (acid sol.)
BV FH40, %0.18 max0.90-1.600.10-0.500.035 max0.035 max0.015 min
ElementNbVTiCuCrNi / Mo
BV FH40, %0.02-0.050.05-0.100.02 max0.35 max0.20 max0.40 max / 0.08 max

Per IACS UR W11 / Bureau Veritas hull structural steel rules (higher-strength grades). Nb, V and Al grain-refining elements may be used singly or in combination; when used in combination the individual minima do not apply. Where acid-soluble Al is not less than 0.015%, the Si minimum does not apply. Carbon equivalent: Ceq = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15 (%).

Product Analysis (Check Analysis)

 

IACS UR W11 / BV rules do not separately tabulate product (check) analysis limits for higher-strength grades. When product analysis is required, the finished plate shall meet the heat limits subject to ASTM A6/A6M Table A permitted variations (same practice as other IACS societies).

ElementHeat analysis limitProduct analysis (heat ± A6)
C0.18 max0.22 max
Mn0.90-1.600.81–1.72
Si0.10-0.500.04–0.56
P0.035 max0.045 max
S0.035 max0.045 max
Al (acid sol.)0.015 minno A6 Table A tolerance; product value not tabulated
Nb0.02-0.050.010–0.060
V0.05-0.100.040–0.110
Ti0.02 max0.03 max
Cu0.35 max0.38 max
Cr0.20 max0.24 max
Ni0.40 max0.43 max
Mo0.08 max0.09 max

Per IACS UR W11 / Bureau Veritas hull structural steel rules. Product analysis applies only when specified; for a range, results may not vary both above and below it.

BV FH40 Mechanical Properties

 

GradeYield strength, minTensile strengthElongation, min
BV FH40390 MPa [57 ksi]510-650 MPa [74-94 ksi]20%

Per IACS UR W11 / Bureau Veritas hull structural steel rules. Yield and tensile values apply for the full thickness range covered by the grade (typically up to 100 mm for these ship plates).

Charpy V-Notch Impact Requirements (-60°C [-76°F])

 

ThicknessTest temperatureLongitudinal, avg minTransverse, avg min
t≤50 mm-60°C [-76°F]39 J26 J
50<t≤70 mm-60°C [-76°F]46 J31 J
70<t≤100 mm-60°C [-76°F]55 J37 J

Per IACS UR W11 / Bureau Veritas hull structural steel rules. Average of three full-size Charpy V-notch specimens; not more than one value below the average and none below 70% of it. Longitudinal values shown; transverse values apply when required by the rules or purchase order. Thicker plates (above 100 mm) may be supplied by agreement with adjusted impact requirements.

Delivery Condition and Deoxidation

Deoxidation: Killed, fine-grain practice. Delivery condition: F-class (FH40) grades are supplied normalized or TMCP (often with Ni alloying for -60°C toughness); as-rolled delivery is not permitted. Optional extras by agreement include ultrasonic testing, Z-direction (Z15/Z25/Z35) through-thickness testing and third-party Bureau Veritas survey.

Thickness Coverage

Higher-strength BV AH/DH/EH/FH 32/36/40 plates are commonly supplied from about 6 mm to 100 mm thick (up to 150 mm by agreement). Width 1500-4000 mm and length 6000-18000 mm are typical.

Equivalent Steel Grades of BV FH40

 

Society / StandardEquivalent grade
BV (Bureau Veritas)BV FH40 steel plate (BV/FH40)
LR (Lloyd's Register)LR FH40 steel plate
ABSABS FH40 steel plate
CCSCCS FH40 steel plate
ASTM A131/A131MASTM A131 FH40 steel plate
GLGL FH40 steel plate
DNVDNV F40 steel plate
NKNK F40 steel plate
KRKR F40 steel plate
RINARINA FH40 steel plate

IACS member societies harmonize ordinary and higher-strength hull grades under UR W11; dual certification (for example BV + ABS, or BV + ASTM A131) is common when ordered that way.

FAQ about BV FH40 Steel Plate

What is BV FH40 steel plate?

It is a higher-strength hull structural steel under Bureau Veritas Rules for the Classification of Steel Ships (IACS UR W11), with 390 MPa minimum yield, 510-650 MPa tensile strength and Charpy toughness at -60°C [-76°F]. The mill certificate grade is BV FH40 (BV Grade FH40).

What does BV FH40 / Grade FH40 stand for?

BV is Bureau Veritas. The letter F is the toughness class (Charpy at -60°C [-76°F]), H means higher strength, and 40 is the strength level (historically about 40 kgf/mm², now 390 MPa min yield).

What is the yield strength of BV FH40?

Minimum 390 MPa (57 ksi), tensile 510-650 MPa (74-94 ksi), elongation about 20% min.

What is the impact test temperature for BV FH40?

Charpy V-notch at -60°C [-76°F]. Longitudinal average minima are 39 J up to 50 mm, 46 J for 50-70 mm and 55 J for 70-100 mm.

What is the difference between BV FH40 and other 40-class grades?

Same 390 MPa strength class. BV AH40 at 0°C [32°F]; BV DH40 at -20°C [-4°F]; BV EH40 at -40°C [-40°F]; BV FH40 at -60°C [-76°F]. Delivery condition follows the toughness letter rules.

What is the difference between BV FH40 and BV FH32?

Same F-class toughness (Charpy at -60°C [-76°F]). BV FH40 is strength class 40 (390 MPa min yield); BV FH32 is strength class 32 (315 MPa min yield).

Is BV FH40 the same as ABS FH40 or LR FH40?

Requirements are essentially harmonized under IACS UR W11. ABS FH40, LR FH40, DNV F40 and ASTM A131 FH40 (where listed) are counterparts; dual certification is common when ordered with the required surveys.

Is BV FH40 weldable?

Yes. Controlled carbon and Ceq give good weldability; preheat may be required for thick sections depending on Ceq and restraint.

What heat treatment is required for BV FH40?

F-class (FH40) grades are supplied normalized or TMCP (often with Ni alloying for -60°C toughness); as-rolled delivery is not permitted.

What thickness is available for BV FH40?

Typical supply is about 6-100 mm thick (up to 150 mm by agreement), 1500-4000 mm wide and 6000-18000 mm long.

Other BV Steel Plate Grades

BV Grade A steel plate | BV Grade B steel plate | BV Grade D steel plate | BV Grade E steel plate | BV AH32 steel plate | BV AH36 steel plate | BV AH40 steel plate | BV DH32 steel plate | BV DH36 steel plate | BV DH40 steel plate | BV EH32 steel plate | BV EH36 steel plate | BV EH40 steel plate | BV FH32 steel plate | BV FH36 steel plate

Equivalent Class Society Grades

BV FH40 corresponds to the same grade under the other IACS member classification societies and ASTM A131: LR FH40 steel plate, ABS FH40 steel plate, CCS FH40 steel plate, ASTM A131 FH40 steel plate, GL FH40 steel plate, DNV F40 steel plate, NK F40 steel plate, KR F40 steel plate, RINA FH40 steel plate.

Other Products