ASME SA542 Type C Class 1, also written SA542 Type C Class 1, SA542-C Cl.1, and companion ASTM A542 Type C Class 1. This designation is quenched-and-tempered chromium-molybdenum pressure-vessel plate under ASME SA-542/SA-542M. Type C sets the heat-analysis chemistry (Cr-Mo-V on the 2.75–3.25% Cr band with Ti and B). Class 1 sets the tensile line: yield strength min 85 ksi [585 MPa], tensile strength 105–125 ksi [725–860 MPa], elongation min 14% in 2 in. [50 mm]. A542/SA542 uses Type and Class only (no Grade number). Confirm the ASTM or ASME edition named on the purchase order before mill release. gangsteel produce and export this Type and Class cut to size; EN 10204 3.1 or 3.2 mill certificates and impact/PWHT/NDE supplements are supplied when written on the order.

ASME SA542 Type C Class 1 Chemical Composition

Heat-analysis limits for Type C. Product-analysis tolerances and footnotes follow the contracted edition of ASME SA-542/SA-542M. Values below are heat analysis, %.

Element (heat analysis) Type C, %
Carbon (C) 0.10–0.15
Manganese (Mn) 0.30–0.60
Phosphorus (P), max 0.025
Sulfur (S), max 0.025
Silicon (Si), max 0.13
Chromium (Cr) 2.75–3.25
Molybdenum (Mo) 0.90–1.10
Copper (Cu), max 0.25
Nickel (Ni), max 0.25
Vanadium (V) 0.20–0.30
Titanium (Ti) 0.015–0.035
Boron (B) 0.001–0.003

Type C is a Cr-Mo-V chemistry on the 2.75–3.25% Cr band with vanadium and controlled titanium and boron. It is not interchangeable with Type A/B 2¼Cr-1Mo without engineering approval.

ASME SA542 Type C Class 1 Mechanical Properties

Property Class 1
Tensile strength 105–125 ksi [725–860 MPa]
Yield strength, min 85 ksi [585 MPa]
Elongation in 2 in. [50 mm], min, % 14

Class tensile values are Class-based, not Type-specific, within the combinations permitted by ASME SA-542/SA-542M. Apply ASTM A20/A20M elongation adjustment where thickness requires. Charpy impact (where not already Class-required), PWHT simulation, and NDE follow the purchase order and applicable ASME Section requirements when specified.

Application Areas

ASME SA542 Type C Class 1 is selected for welded pressure equipment that needs quenched-and-tempered Cr-Mo-V (higher Cr; Ti-B) plate at the Class 1 strength line. Typical engineered uses include:

  • Heavy-wall pressure vessels and reactors in refining and petrochemical service where the design specifies A542/SA542 Type C Class 1 (or dual-marked companion designation when Code-ordered).
  • Hydroprocessing and hydrotreating equipment shells, heads, and thick-section components that require this Cr-Mo or Cr-Mo-V alloy content with quenched-and-tempered mechanical properties rather than a normalized-and-tempered Cr-Mo specification alone.
  • High-integrity boilers and pressure vessels where the purchaser’s material specification names Type C chemistry and Class 1 tensile limits.
  • Repair, replacement, and project plate cut to size for fabricators working to ASME Section VIII or project vessel specifications that call out A542/SA542 Type C Class 1.

Final fitness for a given design temperature, hydrogen service, PWHT cycle, or sour-service supplement is project-specific. Order the exact Type, Class, edition, and test package required by the vessel drawing and Code.

Delivery Condition

Under ASME SA-542/SA-542M, Type C Class 1 plate is normally furnished in the quenched-and-tempered (QT) condition so that Class 1 tensile and yield requirements are met at delivery. As-rolled or normalized-only shipment does not meet this Class unless the purchaser performs the full quench-and-temper cycle under the specification (see Heat Treatment Process).

Item Requirement Order confirmation
Standard final condition Quenched and tempered (QT) to Class 1 mechanical properties State QT delivery on the PO unless another route is agreed in writing
Purchaser heat-treatment exception Purchaser may perform final QT when permitted by ASME SA-542/SA-542M; manufacturer pre-shipment temper still applies (see Heat Treatment Process) Name who performs final QT and required mill temper before shipment
Marking ASME SA-542 (or ASTM A542 when product-ordered) with Type C and Class 1; dual marking by agreement when editions align Confirm ASTM, ASME, or dual marking on the order
Certification Mill test documentation for heat/product analysis and mechanical results as ordered EN 10204 3.1 or 3.2, and any third-party witness, subject to enquiry and order confirmation
Supplementary tests Impact, PWHT simulation, NDE, and other project extras when specified List each supplement, acceptance, and temperature on the PO

Certificate form, analysis reporting, and supplements are not assumed as open guarantees: confirm them with the enquiry and order. Delivery marking must show Type C Class 1 as ordered.

Heat Treatment Process

Plate heat treatment for ASME SA542 Type C Class 1 is distinct from vessel post-weld heat treatment (PWHT). The plate route is austenitize, quench, and temper to Class 1. Fabrication PWHT follows the applicable ASME Section and the fabricator’s WPS and must be ordered separately when simulated or recorded on plate tests.

Step Requirement Order confirmation
Austenitize Heating for quench as required to develop Class 1 properties after temper No fixed temperature, hold time, or rate is stated here; confirm mill practice against the contracted edition if required on the PO
Quench Cooling from austenitizing to produce the as-quenched structure for temper Quench medium and parameters follow mill practice within the specification; name any purchaser limit on the order
Temper (final QT by manufacturer) Minimum tempering temperature for Type C Class 1: 1050°F [565°C] Confirm Class 1 temper requirement and any higher project minimum on the PO
Manufacturer temper when purchaser performs final QT If the purchaser performs the quench-and-temper cycle, the manufacturer shall temper before shipment at not lower than 1050°F [565°C] for Types A, B, C, and D State purchaser final QT and required pre-shipment temper on the order
Vessel PWHT (not plate delivery temper) Separate from plate QT; governed by Code, drawing, and WPS Order PWHT simulation or recorded cycles only when written on the PO

Only the minimum temper of 1050°F [565°C] for Type C Class 1 is given from the verified specification data used for this page. Austenitizing temperature (unless a Type minimum is listed above), quench medium, hold times, and heating/cooling rates are not fixed on this page and remain subject to mill practice and order confirmation. Impact test temperature and acceptance, when required, must be named on the order.

Size and Supply Range

ASME SA-542/SA-542M states a minimum thickness of 3/16 in. [5 mm]. Maximum thickness is limited by the ability of the plate to meet the specified mechanical properties after quench and temper. Width and length are cut to the dimensions stated on the purchase order, within mill and processing capability for the order. Available thickness, width, length, lead time, certificate type (EN 10204 3.1 or 3.2), and any cutting or test extras are subject to enquiry and order confirmation. State thickness × width × length, Type C Class 1, edition, and required supplements on the RFQ.

Comparison with ASTM A533

Both ASME SA542 Type C Class 1 and ASTM A533 Grade A Class 1 (also written A533 Type A Class 1) are quenched-and-tempered alloy steel plates for welded pressure vessels, but they are not interchangeable.

Item ASME SA542 Type C Class 1 ASTM A533 Grade A Class 1
Alloy family Cr-Mo-V (Type C: higher Cr; Ti-B) Mn-Mo (Type/Grade A: no specified nickel)
Naming Type + Class (no Grade number) Type/Grade + Class (commercial orders often say Grade A)
Heat treatment Quenched and tempered Quenched and tempered
This page Class 1 yield, min 85 ksi [585 MPa] 50 ksi [345 MPa] (A533 Class 1)
This page Class 1 tensile 105–125 ksi [725–860 MPa] 80–100 ksi [550–690 MPa] (A533 Class 1)
Elongation in 50 mm, min 14% 18% (A533 Class 1)

See the ASTM A533 Steel Plate hub for other A533 grades and classes. A533 Class numbers do not map one-to-one onto A542 Class numbers. Do not substitute A533 Grade A Class 1 for ASME SA542 Type C Class 1 (or the reverse) without a design and purchasing change.

Equivalent / Related Materials

The table lists companion designations and chemistry-family related materials. Rows marked “similar / related” are engineering cross-references only—not proven drop-in equivalents and not automatic Code interchangeability. Dual certification requires the stricter combined limits on the purchase order and MTC.

Standard / region Designation Relationship Reference
American (ASTM companion) ASTM A542 Type C Class 1 Companion designation when editions align; dual marking by agreement Order ASTM A542 Type C Class 1 when the vessel specification requires the ASTM name
American (related Cr-Mo) ASTM A387 / ASME SA387 Grade 22 Class 1 / Class 2 Related Cr-Mo / Cr-Mo-V elevated-temperature family; typically normalized-and-tempered elevated-temperature material—not an A542 QT Class substitute A387 Grade 22 Class 1 · A387 Grade 22 Class 2 · A387 hub
American (related QT) ASTM A533 Grade A Class 1 Also quenched-and-tempered vessel plate; Mn-Mo chemistry—related product family only A533 Grade A Class 1 · A533 hub
Chinese GB (similar / related) GB/T 713 12Cr2Mo1VR Related Cr-Mo-V vessel grade family; not a proven one-to-one QT Class interchange with this A542 Type/Class GB/T 713 12Cr2Mo1VR · GB/T 713 hub
Chinese GB (2¼Cr-1Mo related) GB/T 713 12Cr2Mo1R Related 2¼Cr-1Mo vessel grade family; not an automatic substitute for Type C GB/T 713 12Cr2Mo1R
Japanese JIS No confirmed direct equivalent Related Cr-Mo plate designation SCMV4 (JIS G4109) is a chemistry-family reference only and is not interchangeable with ASME SA542 Type C Class 1 —

No automatic one-to-one equivalent across EN/JIS/GB is claimed for ASME SA542 Type C Class 1. Order and certify the designation required by the vessel specification.

FAQ

1. What is ASME SA542 Type C Class 1?

It is quenched-and-tempered pressure-vessel plate under ASME SA-542/SA-542M. Type C fixes the Cr-Mo-V (higher Cr; Ti-B) heat-analysis chemistry. Class 1 fixes strength: yield min 85 ksi [585 MPa], tensile 105–125 ksi [725–860 MPa], elongation 14% min in 50 mm. Plates are supplied to order with mill certificates when this Type and Class are named on the purchase order.

2. How does ASME SA542 Type C Class 1 relate to ASTM A542 Type C Class 1?

For the same Type and Class, ASTM A542 and ASME SA-542 are companion designations used for product versus Code ordering. Chemistry and Class tensile limits are intended to align when the contracted editions match. Order the name required by the vessel specification; dual marking is by agreement.

3. What mechanical values apply to Class 1?

Class 1 tensile strength is 105–125 ksi [725–860 MPa]; yield min 85 ksi [585 MPa]; elongation in 50 mm min 14%. These Class values apply to Types ordered to Class 1 under the permitted combinations in ASME SA-542/SA-542M. Thickness-dependent elongation adjustment follows A20/A20M when required.

4. What distinguishes Type C / which Type–Class combinations are allowed?

Type C is a Cr-Mo-V chemistry on the higher-Cr band with titanium and boron controls. It differs from Type A/B 2¼Cr-1Mo and from Type D/E. Not every Type may be ordered to every Class; specify a permitted Type and Class combination from ASTM A542/A542M as named on the drawing and purchase order.

5. Is ASME SA542 Type C Class 1 interchangeable with A387 Grade 22 or A533 Grade A Class 1?

No automatic swap. A387 Grade 22 is a different Cr-Mo pressure-vessel heat-treatment specification. A533 Grade A Class 1 is a Mn-Mo quenched-and-tempered specification. ASME SA542 Type C Class 1 must be ordered and certified as A542/SA542 Type C Class 1.

6. What thickness and certificate options should be confirmed on the order?

Specification minimum thickness is 3/16 in. [5 mm]; maximum thickness depends on meeting Class 1 after quench and temper. Confirm thickness × width × length, edition, impact/PWHT/NDE, and EN 10204 3.1 or 3.2 by enquiry and order confirmation.

Related Links

RFQ: thickness × width × length, Type C Class 1, ASME SA-542/SA-542M edition, impact/PWHT/NDE, 3.1 or 3.2 — admin@gangsteel.com / jack@gangsteel.com.

Other Products