ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables) is frequently cross-referenced to related ASTM/ASME, EN, and other designations. This equivalents page leads with that cross-reference map, then summarizes chemistry and mechanical limits used to judge dual marking. Near-equivalents are not automatic code substitutes.

Equivalents and Cross-Reference Map

Use the table for RFQ orientation and dual-cert discussions. True dual certification exists only when one heat meets every chemical and mechanical limit of each named specification on the same MTC. Class society, PED, or ASME dossier wording still controls acceptance.

SystemGradeNote
ASMESA517 Grade FASME twin
ASTMA517 Grade B / E / QOther Q&T chemistries - not interchangeable
RelatedA514 Grade FStructural Q&T cousin - different product scope

Substitution caveat: Do not swap grades based on marketing strength bands alone. Chemistry, heat treatment, impact temperature, and product form must be reviewed by the responsible engineer before any concession.

Chemical Composition - Base Grade (ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables))

Heat analysis for Grade F. Product analysis ranges are slightly wider per A517/A517M. Confirm ordered edition on the MTC (V/Ti/B/Cu bands vary slightly by reprint). Family overview pages. Chem/mech below are ASTM A517 Grade F. Other A517 grades (A/B/E/H/P/Q/S) differ - confirm ordered grade.

Element / ruleRequirement
C (heat)0.10-0.20
Mn (heat)0.60-1.00
P, max0.025
S, max0.025
Si (heat)0.15-0.35
Ni (heat)0.70-1.00
Cr (heat)0.40-0.65
Mo (heat)0.40-0.60
V (heat)0.03-0.08
Ti (heat)0.002-0.05
B (heat)0.0005-0.006
Cu (heat)0.15-0.50

Mechanical Properties (ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables))

Confirm thickness, specimen orientation, and any supplementary impact, UT, or hardness requirements on the PO.

PropertyRequirement
Tensile (t<=65 mm)115-135 ksi [795-930 MPa]
Yield min (t<=65 mm)100 ksi [690 MPa]
Tensile (65 < t <= 150 mm)105-135 ksi [725-930 MPa]
Yield min (65 < t <= 150 mm)90 ksi [620 MPa]
Elongation in 50 mm, min (t<=65 mm)16%
Elongation in 50 mm, min (t>65 mm)14%
DeliveryQuenched and tempered

Frequently Asked Questions

What are the common equivalents for ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables)?

Buyers typically cross-reference ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables) with the related designations listed in the map above. Related grades in the same family are not automatic substitutes.

Is a near-equivalent always acceptable on an ASME or PED dossier?

No. The material specification listed on the calculation sheet, PED appraisal, or purchaser material list controls acceptance. Certificate marks must match unless a formal concession is approved.

How should dual marking be requested for ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables)?

List every required standard on the purchase order and ask the mill to print all approved designations on one MTC only when the heat qualifies against each. Gangsteel confirms which heats can honestly carry those marks before allocation.

What is a safe way to compare ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables) with near-equivalents?

Compare chemistry ranges, tensile/yield windows, impact temperature if specified, delivery/heat-treatment practice, and product form side by side. Name-alike grades can still fail dossier acceptance.

Does a sibling class or grade count as an equivalent?

Sibling classes (for example Class 1 vs Class 2, or Grade A vs B) share a family but intentionally different strength or toughness tiers. Ordering the wrong tier undercuts the design assumption.

How do I RFQ ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables) when equivalents are also named?

State ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables) as the governing grade, then list any dual marks required. Include dimensions, quantity, delivery condition, optional tests, certificate type, destination, and which mark governs acceptance.

Ordering and Mill Certificates

State grade ASTM A517 / A517M quenched-and-tempered alloy PV plate family (Grade F example tables), dimensions, quantity, delivery condition, optional NDT/PMI, and certificate (EN 10204 3.1 standard; 3.2 when third-party inspection is ordered). Gangsteel supplies export plate and related products with mill test certificates. Contact Gangsteel for stock and mill production RFQs.

Other Products