Home > News >

UNS S30153 / ASTM A240 Type 301LN (EN 1.4318) is a low-carbon nitrogen-strengthened austenitic stainless plate/sheet (301LN) grade under ASTM A240/A240M; ASME SA240; EN 10088-2 1.4318. This specification page covers grade identity, chemistry, mechanical requirements, related grades, and RFQ practice. Accept material against the ordered edition and the mill test certificate.

Grade Identity and Delivery Condition

UNS S30153 / ASTM A240 Type 301LN (EN 1.4318) is supplied for projects that name this designation on the purchase order or calculation sheet. Standard delivery condition is Solution annealed; cold-rolled tempers when ordered. Gangsteel supplies export plate and related products with EN 10204 documentation. Do not accept an alternate heat-treatment route unless a written concession changes the specification requirement.

Chemical Composition - Heat Analysis (UNS S30153 / ASTM A240 Type 301LN (EN 1.4318))

Heat/cast analysis for UNS S30153 (301LN). Nitrogen strengthens while low carbon supports weldability vs classic 301.

ElementMin %Max % / requirement
C-<=0.030
Si-<=1.00
Mn-<=2.00
P-<=0.045
S-<=0.030
Cr16.018.0
Ni6.08.0
N0.070.20

Mechanical Properties (UNS S30153 / ASTM A240 Type 301LN (EN 1.4318))

Confirm thickness, specimen orientation, and any supplementary impact, UT, or hardness requirements on the PO.

PropertyRequirement
Tensile strength, min (A240 annealed)550 MPa
Yield strength (0.2% offset), min240 MPa
Elongation in 50 mm, min45%
Hardness, max (annealed)241 HBW
DeliverySolution annealed (unless temper ordered)

Related / Near-Equivalent Grades

Near-equivalents are for cross-reference only. They are not automatic code substitutes. Substitution requires engineer approval and matching certificate scope.

SystemGradeNote
EN1.4318 / X2CrNiN18-7European 301LN
AISI301LNCommon name
ASTMType 301Higher C classic 301 - not identical

Frequently Asked Questions

What is UNS S30153 / ASTM A240 Type 301LN (EN 1.4318)?

UNS S30153 / ASTM A240 Type 301LN (EN 1.4318) is a low-carbon nitrogen-strengthened austenitic stainless plate/sheet (301LN) under ASTM A240/A240M; ASME SA240; EN 10088-2 1.4318. It is ordered when drawings or the calculation sheet name this designation specifically.

What chemical composition applies to UNS S30153 / ASTM A240 Type 301LN (EN 1.4318)?

Controlled elements and limits are tabulated above from the governing standard. Always verify the heat analysis on the MTC against the ordered edition.

What mechanical properties should buyers expect for UNS S30153 / ASTM A240 Type 301LN (EN 1.4318)?

Tensile, yield, elongation, and related limits are tabulated above. Design allowables must come from the applicable pressure-vessel or structural code, not from a web summary.

What delivery condition is required for UNS S30153 / ASTM A240 Type 301LN (EN 1.4318)?

Standard delivery is Solution annealed; cold-rolled tempers when ordered. State it explicitly on the PO. Do not accept an alternate route without a written concession.

How does UNS S30153 / ASTM A240 Type 301LN (EN 1.4318) differ from near-equivalent grades?

Near-equivalents may differ in carbon or alloy bands, tensile class, impact temperature, or heat treatment. Substitution needs engineering approval and matching certificate scope.

How do I RFQ UNS S30153 / ASTM A240 Type 301LN (EN 1.4318) from Gangsteel?

Send UNS S30153 / ASTM A240 Type 301LN (EN 1.4318), thickness x width x length, quantity or tonnage, delivery condition, optional impact/UT/Z tests, EN 10204 3.1 or 3.2, destination, and any dual-mark needs. Gangsteel replies with mill options, lead time, and packing notes.

Ordering and Mill Certificates

State grade UNS S30153 / ASTM A240 Type 301LN (EN 1.4318), dimensions, quantity, delivery condition, optional NDT/PMI, and certificate (EN 10204 3.1 standard; 3.2 when third-party inspection is ordered). Gangsteel supplies export plate and related products with mill test certificates. Contact Gangsteel for stock and mill production RFQs.