ASME SA387 / ASTM A387 Grade 2 Class 1 is a 0.5Cr-0.5Mo pressure-vessel plate grade under ASTM A387/A387M; ASME SA387. This specification page covers grade identity, chemistry, mechanical requirements, related grades, and RFQ practice. Accept material against the ordered edition and the mill test certificate.

Grade Identity and Delivery Condition

ASME SA387 / ASTM A387 Grade 2 Class 1 is supplied for projects that name this designation on the purchase order or calculation sheet. Standard delivery condition is Annealed, N+T, or accelerated cool + temper; Grade 2 tempering generally >=620 deg C. Gangsteel supplies export plate and related products with EN 10204 documentation. Do not accept an alternate heat-treatment route unless a written concession changes the specification requirement.

Chemical Composition - Heat Analysis (ASME SA387 / ASTM A387 Grade 2 Class 1)

Heat analysis for Grade 2. Class 1 and Class 2 share chemistry. Confirm ordered A387/SA387 edition for P/S.

Element / ruleRequirement
C (heat)0.05-0.21
Mn (heat)0.55-0.80
P, max0.025
S, max0.025
Si (heat)0.15-0.40
Cr (heat)0.50-0.80
Mo (heat)0.45-0.60

Mechanical Properties (ASME SA387 / ASTM A387 Grade 2 Class 1)

Confirm thickness, specimen orientation, and any supplementary impact, UT, or hardness requirements on the PO.

PropertyRequirement
Tensile strength55-80 ksi [380-550 MPa]
Yield strength, min33 ksi [230 MPa]
Elongation in 200 mm, min18%
Elongation in 50 mm, min22%
Delivery / HTPer A387/SA387; Grade 2 tempering generally >=620 deg C

Related / Near-Equivalent Grades

Near-equivalents are for cross-reference only. They are not automatic code substitutes. Substitution requires engineer approval and matching certificate scope.

SystemGradeNote
ASTMA387 Grade 2 Class 2Higher tensile class, same chem
RelatedA387 Grade 12 / A204Different Cr or Mo-only bands
EN 10028-216Mo3 (approx., Mo-only)Not identical

Frequently Asked Questions

What is ASME SA387 / ASTM A387 Grade 2 Class 1?

ASME SA387 / ASTM A387 Grade 2 Class 1 is a 0.5Cr-0.5Mo pressure-vessel plate under ASTM A387/A387M; ASME SA387. It is ordered when drawings or the calculation sheet name this designation specifically.

What chemical composition applies to ASME SA387 / ASTM A387 Grade 2 Class 1?

Controlled elements and limits are tabulated above from the governing standard. Always verify the heat analysis on the MTC against the ordered edition.

What mechanical properties should buyers expect for ASME SA387 / ASTM A387 Grade 2 Class 1?

Tensile, yield, elongation, and related limits are tabulated above. Design allowables must come from the applicable pressure-vessel or structural code, not from a web summary.

What delivery condition is required for ASME SA387 / ASTM A387 Grade 2 Class 1?

Standard delivery is Annealed, N+T, or accelerated cool + temper; Grade 2 tempering generally >=620 deg C. State it explicitly on the PO. Do not accept an alternate route without a written concession.

How does ASME SA387 / ASTM A387 Grade 2 Class 1 differ from near-equivalent grades?

Near-equivalents may differ in carbon or alloy bands, tensile class, impact temperature, or heat treatment. Substitution needs engineering approval and matching certificate scope.

How do I RFQ ASME SA387 / ASTM A387 Grade 2 Class 1 from Gangsteel?

Send ASME SA387 / ASTM A387 Grade 2 Class 1, thickness x width x length, quantity or tonnage, delivery condition, optional impact/UT/Z tests, EN 10204 3.1 or 3.2, destination, and any dual-mark needs. Gangsteel replies with mill options, lead time, and packing notes.

Ordering and Mill Certificates

State grade ASME SA387 / ASTM A387 Grade 2 Class 1, dimensions, quantity, delivery condition, optional NDT/PMI, and certificate (EN 10204 3.1 standard; 3.2 when third-party inspection is ordered). Gangsteel supplies export plate and related products with mill test certificates. Contact Gangsteel for stock and mill production RFQs.