WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate) is frequently cross-referenced to related ASTM/ASME, EN, and other designations. This equivalents page leads with that cross-reference map, then summarizes chemistry and mechanical limits used to judge dual marking. Near-equivalents are not automatic code substitutes.
Equivalents and Cross-Reference Map
Use the table for RFQ orientation and dual-cert discussions. True dual certification exists only when one heat meets every chemical and mechanical limit of each named specification on the same MTC. Class society, PED, or ASME dossier wording still controls acceptance.
| System | Grade | Note |
|---|---|---|
| GB/T 16270 | Q690D / Q690E family | Nearest national QT HSLA family - not automatic substitute |
| EN 10025-6 | S690QL family | Approx. strength class - confirm |
| Mill | WQ690D | Related Wuyang QT designation |
Substitution caveat: Do not swap grades based on marketing strength bands alone. Chemistry, heat treatment, impact temperature, and product form must be reviewed by the responsible engineer before any concession.
Chemical Composition - Base Grade (WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate))
Heat analysis per WXG301-2008 Table 1 for WH80Q. Ceq limits by thickness (e.g. <=50 mm Ceq<=0.50). Confirm mill edition on MTC.
| Element / rule | Requirement |
|---|---|
| C, max | 0.18 |
| Si, max | 0.50 |
| Mn, max | 1.80 |
| P, max | 0.020 |
| S, max | 0.010 |
| Cr, max | 0.80 |
| Ni, max | 1.20 |
| Mo, max | 0.60 |
| Nb, max | 0.07 |
| V, max | 0.08 |
| Ti, max | 0.03 |
| B, max | 0.003 |
Mechanical Properties (WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate))
Confirm thickness, specimen orientation, and any supplementary impact, UT, or hardness requirements on the PO.
| Property | Requirement |
|---|---|
| Yield Rp0.2, min (t<=50 mm) | 685 MPa |
| Yield Rp0.2, min (50 < t <=100 mm) | 665 MPa |
| Tensile Rm, min (t<=100 mm) | 760 MPa |
| Elongation A, min | 14% |
| Impact KV2 long. (quality D, -20 C) | 34 J min |
| Delivery / HT | Quenched and tempered (see WXG301 thickness rules) |
Frequently Asked Questions
What are the common equivalents for WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate)?
Buyers typically cross-reference WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate) with the related designations listed in the map above. Related grades in the same family are not automatic substitutes.
Is a near-equivalent always acceptable on an ASME or PED dossier?
No. The material specification listed on the calculation sheet, PED appraisal, or purchaser material list controls acceptance. Certificate marks must match unless a formal concession is approved.
How should dual marking be requested for WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate)?
List every required standard on the purchase order and ask the mill to print all approved designations on one MTC only when the heat qualifies against each. Gangsteel confirms which heats can honestly carry those marks before allocation.
What is a safe way to compare WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate) with near-equivalents?
Compare chemistry ranges, tensile/yield windows, impact temperature if specified, delivery/heat-treatment practice, and product form side by side. Name-alike grades can still fail dossier acceptance.
Does a sibling class or grade count as an equivalent?
Sibling classes (for example Class 1 vs Class 2, or Grade A vs B) share a family but intentionally different strength or toughness tiers. Ordering the wrong tier undercuts the design assumption.
How do I RFQ WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate) when equivalents are also named?
State WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate) as the governing grade, then list any dual marks required. Include dimensions, quantity, delivery condition, optional tests, certificate type, destination, and which mark governs acceptance.
Ordering and Mill Certificates
State grade WH80Q (Wuyang / Wugang quenched-and-tempered high-strength plate), dimensions, quantity, delivery condition, optional NDT/PMI, and certificate (EN 10204 3.1 standard; 3.2 when third-party inspection is ordered). Gangsteel supplies export plate and related products with mill test certificates. Contact Gangsteel for stock and mill production RFQs.
-
BHW35 Steel Plate for Sale | RF
BHW35 / 13MnNiMo5-4 (DIWA 353 family): identity, chemistry, mechanical properties, related grades, and RFQ note
-
ASTM A516 Grade 70 Equivalent:
ASTM A516 Grade 70 equivalents include ASME SA516 Gr 70, EN 10028-2 P355GH and BS 1501 224-490. Gangsteel compa
-
What is the difference between
we supply high-quality A516 Gr 70 steel plate for pressure vessel applications and other standards like ASTM A2
-
P355GH AND S355J2 Steel Plates
EN10028-2 P355GH for High-Strength Low-Alloy Columbium-Vanadium Structural Steel EN10025-2 S355J2 Structural St