HC220I — also written EN 10268 HC220I, 1.0346 steel and HC220I cold-rolled sheet — is a isotropic high-strength flat-steel grade. Gangsteel treats the grade, thickness, test direction and surface specification as one order definition, rather than selecting coil solely by its yield number.

EN 10268 HC220I Cold Rolled Steel Sheet and Coil product-form illustration

EN 10268:2006+A1:2013 covers uncoated cold-rolled flat products for cold forming, with thickness ≤3 mm. The products are sheet, wide strip, slit wide strip, narrow strip and cut lengths. This is not a hot-rolled heavy-plate specification and does not, by itself, specify a galvanized coating.

What Distinguishes HC220I?

The isotropic family controls directional forming behaviour. It is considered for stretch-formed panels where balanced response matters; a yield-strength match to an LA sheet does not reproduce the same strain distribution in the tool.

Material identity and product scope
Item Definition
Grade / steel number HC220I / 1.0346
Data basis EN 10268:2006+A1:2013
Product thickness ≤3 mm
Product surface Uncoated; coating is separately specified
Delivery Skin-passed; normally oiled

HC220I Chemical Composition

Table 1 ladle analysis; mass %
Element Value Limit type
C .07 maximum
Si .5 maximum
Mn .6 maximum
P .05 maximum
S .025 maximum
Al .015 minimum
Ti .05 maximum

These are ladle-analysis requirements, not a nominal recipe or measured values for a particular coil. Do not apply a maximum sign to the aluminium minimum. No separate numerical product-analysis tolerance is represented by this table. Under this edition, specific inspection and testing may not be specified for product analysis or surface finish.

Where listed in the grade definition, the additional dispersoidal elements may be used alone or in combination within their limits. Vanadium and boron may also be added, but the sum of the four dispersoidal elements must not exceed 0.22%. For I grades, titanium may be replaced by niobium or boron.

HC220I Mechanical Properties

Table 2 transverse specimens; as-delivered condition, thickness ≤3 mm
Property Requirement Qualification
0.2% proof strength Rp0.2 220–270 MPa Use lower yield point ReL if a pronounced yield occurs
Tensile strength Rm 300–380 MPa Transverse
Elongation A80 ≥34% Initial gauge length 80 mm; thickness reductions below apply
Thickness and time qualifications for the mechanical table
Condition Rule
0.5 < t ≤0.7 mm Minimum A80 reduced by 2 percentage points, to 32%
t ≤0.5 mm Minimum A80 reduced by 4 percentage points, to 30%
Formability r and n minima, where specified Applicable only at t ≥0.5 mm
t >2 mm Specified minimum transverse r, where applicable, reduced by 0.2
Mechanical-property validity At least 6 months from product availability

The minimum r-value and n-value provisions are formability controls where they appear in the grade table. Part-specific suitability and an agreed maximum scrap rate may be contracted instead of acceptance by the tabulated mechanical properties. Such a contract must be explicit; it is not a blanket waiver of the order.

Delivery Condition, Heating and Surface

The standard specifies skin-passed delivery. The manufacturer selects the steelmaking and manufacturing processes unless otherwise agreed; this is not a quenched-and-tempered plate route. Material is normally supplied with a uniform neutral non-drying oil film. Specify a different protection or an unoiled surface explicitly, and coordinate it with storage and downstream cleaning.

Delivery and process parameters
Parameter Requirement
Condition Skin-passed
Maximum product thickness 3 mm
Dimensional tolerances, rolled width ≥600 mm EN 10131
Dimensional tolerances, rolled width <600 mm EN 10140
Surface quality B stretcher-strain freedom, where that quality applies 6 months from agreed availability

For rolled width ≥600 mm, specify surface quality A or B using the applicable surface definitions. For widths below 600 mm, the surface provisions of EN 10139 apply. A coating requirement is additional to this uncoated substrate specification; do not substitute galvanized-sheet designations for the base grade.

Equivalent Materials and Legacy Names

1.0346 is the steel number identifying HC220I in this standard. It is not an ASTM or JIS equivalence. Coated grades, hot-rolled EN 10149 steels and dual-phase automotive steels can share a strength class while differing in chemistry, microstructure, test direction, surface and forming response. Substitution needs a technical comparison and purchaser approval.

Applications, Forming and Welding

HC220I is evaluated for cold-formed sheet components where its 220–270 MPa proof-strength range and 34% baseline transverse A80 meet the design and forming plan. The isotropic family controls directional forming behaviour. It is considered for stretch-formed panels where balanced response matters; a yield-strength match to an LA sheet does not reproduce the same strain distribution in the tool. Review bend orientation, edge quality, lubrication and springback with the toolmaker. Tensile elongation is not a direct prediction of a punched-edge stretch limit or a guaranteed minimum bend radius.

Specify the welding method at enquiry. Clean off oil where required by the welding procedure, qualify resistance-spot or other welding parameters for the actual gauge and surface, and control heat input and electrode condition. This uncoated carbon-steel substrate requires an appropriate corrosion-protection system in service. Keep coils dry and protected during transport and storage.

Frequently Asked Questions

Is HC220I a thick steel plate grade?

No. The numerical data here apply to EN 10268 uncoated cold-rolled flat products up to 3 mm thick. HC220I should be offered as sheet, strip, coil or the corresponding cut lengths, not as heavy structural plate.

What are the specified strength values of HC220I?

The transverse Rp0.2 range is 220–270 MPa and Rm is 300–380 MPa. The baseline A80 minimum is 34%, subject to the stated thin-gauge reductions. Record thickness and test direction together with the result.

Are the chemistry figures heat or product analysis?

They are the Table 1 ladle-analysis limits. Aluminium is a minimum while the other values shown are maxima. A product analysis is not simply accepted by inventing a tolerance or treating the ladle table as measured coil chemistry.

Why does test direction matter when comparing suppliers?

The main table uses transverse specimens. LA grades may instead be ordered to the longitudinal alternative by agreement. A quote based on a different direction can look stronger or more ductile without being directly comparable; identify the agreed direction in the purchase order.

Can this material be ordered galvanized under EN 10268 alone?

No. The stated standard covers an uncoated substrate. A metallic or organic coating, coating mass and its associated delivery specification have to be agreed separately. The same strength number in a coated designation is not an automatic grade substitution.

Does the standard specify a universal heat-treatment furnace cycle?

No universal annealing or quenching setpoint is quoted for this skin-passed cold-rolled product. The manufacturer controls the processing route to achieve the ordered properties. Heating during fabrication can alter the as-delivered state.

How should the surface and storage condition be specified?

Identify surface quality and finish, oiling or other temporary protection, coil/bundle limits and the intended coating operation. Store under dry protected conditions. Surface quality and freedom from stretcher strains have specific scope and time limits, not an unlimited cosmetic warranty.

What information does Gangsteel need to quote HC220I?

Provide HC220I / 1.0346, EN 10268:2006+A1:2013, thickness, width, coil or sheet dimensions, quantity, test direction, surface and oiling requirements. State inspection documents and the forming/welding application. Availability and delivery time are confirmed against the enquiry.

Related: EN 10268 full grade matrix · Carbon and forming steels

For an enquiry, state the complete material designation and edition, product form, dimensions, quantity, inspection document, testing options, packing and destination. Availability and delivery time are confirmed against the actual enquiry; this page is not an inventory or lead-time guarantee.