API 5L Steel Plate
API 5L A25 Line Pipe: Grades, Chemistry and Properties
API 5L A25 — also written A25 line pipe, L175 and API Spec 5L A25 — is a finished-pipe designation. Gangsteel separates starting flat material from pipe certification when reviewing enquiries, and checks the specified edition, product specification level and manufacturing route before quoting.

Edition boundary: numerical tables on this page use API Spec 5L, 46th edition (April 2018). API published the 47th edition on 2 June 2026. The older numerical tables are identified for legacy-contract comparison and must not be presented as verified 47th-edition requirements. State the governing edition on the order. API 5L specifies finished line pipe, not a stand-alone plate product.
What Is API 5L A25?
A25 / L175 is a PSL 1 grade, not a PSL 2 high-strength pipe grade. A25 is a distinct low-strength grade, not an abbreviation of Grade A. Its specified minimum yield strength is 175 MPa rather than the Grade A level.
| Item | Requirement |
|---|---|
| Grade / designation | A25 / L175 |
| PSL | PSL 1 |
| Outside diameter | D ≤141.3 mm |
| Chemistry table wall-thickness scope | t ≤25.0 mm |
| End condition | Ordered end condition under applicable PSL 1 provisions |
Chemical Composition: Heat and Product Analyses
| Pipe route | C maximum | Mn maximum | P | S maximum |
|---|---|---|---|---|
| Seamless | 0.21 | 0.60 | ≤0.030 | 0.030 |
| Welded | 0.21 | 0.60 | ≤0.030 | 0.030 |
The table applies to both heat and product analyses under its specified conditions. The rephosphorized range must not be replaced with the ordinary low-phosphorus maximum. Do not infer a silicon, microalloy or carbon-equivalent acceptance limit from an empty cell in another grade’s table.
Mechanical Properties
| Property | Requirement |
|---|---|
| Minimum yield strength Rt0.5 | 175 MPa |
| Minimum tensile strength Rm | 310 MPa |
| Weld-seam tensile strength where applicable | 310 MPa minimum |
| Elongation | Calculated using the applicable Table 6 specimen-area formula; not a universal fixed percentage |
Delivery and Heat Treatment
The permitted PSL 1 conditions for these grades are as-rolled, normalizing rolled, normalized or normalizing formed. The selected route and finished-pipe inspection must meet the purchase order; normalized starting material is not proof that a pipe has been normalized after every manufacturing operation.
| Control | Value / requirement |
|---|---|
| Permitted condition family | As-rolled / normalizing rolled / normalized / normalizing formed |
| Outside-diameter ceiling | 141.3 mm |
| Chemistry table wall thickness | 25.0 mm maximum |
| Heat-treatment setpoints | Controlled by the pipe manufacturing procedure; no universal setpoint is quoted |
Select end preparation and joining method for the actual line design. This lower-strength PSL 1 grade is not an automatic choice for sour service, low-temperature fracture control or high-pressure transmission simply because it appears in API 5L.
Equivalent Designations and Engineering Substitution
L175 is the paired SI designation within this edition of API 5L for A25. It is not a declaration of equivalence to a structural plate or another pipe standard. Compare product form, delivery condition, chemistry, tensile test basis, toughness, inspection and the governing edition before accepting an alternative. A plate or coil certificate cannot replace the finished-pipe test record.
Applications, Fabrication and Ordering
Finished pipe is ordered for the intended transportation service and project design. When the enquiry is for plate or strip intended for welded-pipe production, state that scope explicitly and agree starting-material properties, tolerances, edge preparation and inspection. The pipe producer remains responsible for qualifying the finished-pipe route. Service suitability, including any sour-service or low-temperature requirements, is assessed separately from the base grade.
Frequently Asked Questions
Is API 5L A25 a finished steel plate grade?
No. API 5L A25 is a line-pipe designation. Starting plate or strip can be procured for a pipe-making route only under an explicit material specification. It does not become finished certified pipe before forming, welding where relevant and pipe testing.
Which edition supplies the numerical data on this page?
The tables are explicitly based on API Spec 5L, 46th edition, April 2018. API published the 47th edition in June 2026. Use the edition named in the purchase order and do not assume these older figures have been verified against the newer text.
What does L175 mean?
L175 is the paired SI steel designation for A25 in the stated edition. For PSL 2, the condition letter remains part of the steel name. A matching strength designation does not remove the need to specify route, dimensions and inspection.
Is A25 available as PSL 1 and PSL 2?
The 46th-edition base table lists this grade under PSL 1, not PSL 2. Do not add a PSL 2 suffix to a quote without a valid separately agreed specification.
Can one elongation percentage be used for every pipe size?
No. The applicable tensile table calculates minimum elongation from the defined specimen area and specified minimum tensile strength. Test-piece geometry and the standard’s calculation rules must be identified before comparing results.
Can the chemistry table be extended to thicker walls?
Not by simple extrapolation. The quoted chemistry tables are for t ≤25.0 mm. For greater wall thickness, use the contract edition’s agreement provisions and the qualified manufacturing route rather than inventing a wider guaranteed range.
Does the designation guarantee HIC, SSC or offshore qualification?
No. Additional service conditions, annex provisions and project tests must be invoked explicitly. Base-grade tensile and chemistry data alone do not establish sour-service or offshore acceptance.
How should an enquiry for A25 be written?
State API Spec 5L, its edition, A25 / L175, PSL, condition where applicable, pipe route, outside diameter, wall thickness, lengths, ends, coating and inspection requirements. Identify whether the purchase is finished pipe or starting flat material. Lead time is confirmed from the actual enquiry.
Related: API 5L grade overview · Pipeline products
For an enquiry, state the complete material designation and edition, product form, dimensions, quantity, inspection document, testing options, packing and destination. Availability and delivery time are confirmed against the actual enquiry; this page is not an inventory or lead-time guarantee.
The original generated product-form image is illustrative. Appearance does not identify a steel grade or prove certification.
-
API 5L X70|X70 STEEL PLATE
Gangsteel is specialized in supplying API 5L steel plate in X70,API X70,API 5L X70.