ASTM A1011 SS Grade 70 hot rolled steel coil

ASTM A1011 SS Grade 70 — also written ASTM A1011 SS Grade 70, A1011M SS Grade 480, A1011 Structural Steel Grade 70 [480], SA-1011 SS Grade 70 — is a structural steel (SS) designation of ASTM A1011/A1011M for hot-rolled sheet and strip with a specified minimum yield strength of 70 ksi [480 MPa] and a minimum tensile strength of 85 ksi [550 MPa]. Gangsteel supplies SS Grade 70 as as-rolled or pickled-and-oiled coil, slit strip and cut-to-length sheet for structural parts made by bending, roll forming and welding.

What is ASTM A1011 SS Grade 70?

In A1011 the SS designations are carbon-manganese steels whose strength is guaranteed by tension testing. The grade number is the minimum yield strength in ksi (in A1011M the number in brackets is the yield in MPa). SS Grade 70 sits at the top in the SS series, which runs from Grade 30 to Grade 70 in the current edition.

ASTM A1011 SS Grade 70 Chemical Composition (Heat Analysis, %)

ASTM A1011/A1011M Table 2, SS, heat analysis, maximum %
DesignationCMnPSCuNiCrMoVCb (Nb)TiN
SS Grade 700.251.350.0350.040.200.200.150.060.0080.0080.025report

Aluminium and silicon are reported but not limited. Titanium is limited to the lesser of 3.4N + 1.5S or 0.025%. When copper-bearing steel is specified, copper is 0.20% minimum. Product (check) analysis tolerances follow ASTM A568/A568M.

ASTM A1011 SS Grade 70 Mechanical Properties

PropertyRequirement
Yield strength70 ksi [480 MPa] min
Tensile strength85 ksi [550 MPa] min
Elongation in 2 in [50 mm], 0.097 to <0.230 in [2.5 to <6.0 mm]≥13%
Elongation in 2 in [50 mm], 0.064 to <0.097 in [1.6 to <2.5 mm]≥12%
Elongation in 2 in [50 mm], 0.025 to <0.064 in [0.65 to <1.6 mm]≥7%
Elongation in 8 in [200 mm], <0.230 in [6.0 mm]≥8%

Tension test specimens are taken longitudinally, at full as-rolled thickness, from a location about halfway between the centre and the edge of the coil or sheet; on coils the producer tests from the coil end. Yield strength is determined by the 0.2% offset or 0.5% extension-under-load method. Two tension tests are made per heat or per 50 tons (one when less than 50 tons is produced), and when the thickest and thinnest material in a heat differ by 0.050 in [1.3 mm] or more, both extremes are tested.

Cold Bending

A1011 recommends a minimum inside radius of 4t for 90° cold bends in SS Grade 70 (non-mandatory Appendix X1, where t is the thickness). Tighter radii are possible on thinner gauges and with bends made across the rolling direction, but a trial is advised before committing a tool design.

Delivery Condition and Heat Treatment

ASTM A1011 SS Grade 70 is delivered in the hot-rolled condition. A1011 does not call for normalizing, quenching or any other post-rolling heat treatment: the strength and ductility are set on the hot strip mill by the chemistry, the finishing temperature, run-out-table cooling and the coiling temperature. The default surface is as rolled with its mill scale, and the purchaser may order the coil pickled (and oiled) or blast cleaned instead. Edges are supplied as mill edge unless cut edge is ordered, and general requirements such as dimensional tolerances, flatness and coil packaging follow ASTM A568/A568M for sheet or ASTM A749/A749M for strip.

ItemDelivery condition per ASTM A1011/A1011M
ConditionHot rolled (as rolled), coils or cut lengths
Surface finishAs rolled with mill scale (default); pickled, or blast cleaned when ordered
OilingAs-rolled material is shipped dry; pickled or blast-cleaned material is oiled unless ordered dry
EdgesMill edge or cut (slit / trimmed) edge
Product formsSheet (coils, cut-to-length sheets) and strip (narrow coils, slit strip)
General requirementsASTM A568/A568M for sheet; ASTM A749/A749M for strip
Heat treatmentNone required by A1011; properties come from hot rolling and controlled coiling

Ordering Information

Ordering itemWhat to state on the enquiry
StandardASTM A1011 or A1011M with year of issue (we work to the current edition unless a year is stated)
DesignationSS Grade 70, e.g. “ASTM A1011M-23, SS Grade 480, as rolled, mill edge, 3.0 x 1250 mm coil”
Copper bearingState when copper-bearing steel is required (Cu 0.20% min)
FinishAs rolled, pickled, or blast cleaned
OilingOiled or dry (pickled / blasted material is normally oiled)
EdgeMill edge or cut edge
DimensionsThickness, width, and length for cut lengths; coil ID, maximum OD and maximum coil mass for coils
ApplicationPart name or end use, so forming and surface requirements can be checked
ReportsHeat analysis and mechanical test report requirements, third-party inspection if any

Comparable Grades

For comparison only — the chemistry, test direction and thickness rules are not identical — SS Grade 70 is broadly comparable by minimum yield strength with the 480 MPa class of thermomechanically rolled strip such as S460MC and S500MC. Where higher toughness or better formability at the same strength is needed, the HSLAS designations of A1011 are the usual alternative.

Applications

Typical uses of SS Grade 70 include roll-formed structural sections, truck and trailer cross members, crane and lifting parts, storage racking uprights, tubes and pressed reinforcements where the weight can be cut by using higher strength.

Documents, Inspection and Lead Time

Every ASTM A1011 SS Grade 70 shipment from Gangsteel is supplied with a mill test certificate to EN 10204 type 3.1 that states the ASTM designation and year, the designation, grade, type or class, the heat number, the heat analysis and, for structural and high-strength designations, the tension test results, together with the purchase order number. Third-party inspection to EN 10204 type 3.2 by SGS, BV, TUV, LR or another agency nominated by the buyer can be arranged before shipment. Each coil or lift carries a tag with the specification, designation, heat number, size and mass.

Lead time is confirmed with each enquiry against the current hot strip mill rolling schedule, the thickness and width mix and any pickling, slitting or cut-to-length processing required, so please send the size list and quantity per item for a firm delivery date.

FAQ

What is the minimum yield strength of ASTM A1011 SS Grade 70?

The specified minimum yield strength is 70 ksi, which is 480 MPa in A1011M. There is no upper limit on yield for this grade. Yield is measured by the 0.2% offset or 0.5% extension-under-load method on longitudinal specimens, and the results are reported on the mill test certificate.

Why does the elongation requirement change with thickness?

A1011 measures elongation on a 2 in [50 mm] gauge length and recognises that thin sheet gives lower values on the same steel. For SS Grade 70 the minimum is 13% from 0.097 in up to 0.230 in, 12% from 0.064 in up to 0.097 in, and 7% from 0.025 in up to 0.064 in. On the 8 in [200 mm] gauge the minimum is 8%. Always check the figure for the band your thickness falls into.

Can SS Grade 70 be welded?

Yes. SS grades are carbon-manganese steels without deliberate microalloying, with carbon 0.25% max and manganese 1.35% max, so they weld by MIG/MAG, resistance and laser processes. For thicker gauges and higher grades a low-hydrogen procedure is good practice. A1011 does not specify a carbon equivalent; if you need one on the certificate, state the formula and limit on the order and we will confirm it against the heat.

Should I choose SS Grade 70 or an HSLAS grade?

SS grades reach their strength mainly with carbon and manganese, while HSLAS grades use microalloying (Nb, V or Ti) at lower carbon. At the same yield level, HSLAS Grade 70 Class 1 gives a higher minimum elongation and better bendability, and Class 2 a further improvement in formability and weldability. Choose SS where cost matters and the forming is moderate; choose HSLAS for tight bends, roll forming at high strength or improved toughness.

What finish and edges can Gangsteel supply?

We supply SS Grade 70 as rolled (black, dry), pickled and oiled, or blast cleaned, with mill edge or slit edge, as full coils, slit strip or cut-to-length sheets. Coil inside diameter, maximum outside diameter and maximum coil mass should be stated on the enquiry so that they match your uncoiler.

Related ASTM A1011 Designations

SS Grade 30 | SS Grade 33 | SS Grade 36 Type 1 | SS Grade 36 Type 2 | SS Grade 40 | SS Grade 45 Type 1 | SS Grade 45 Type 2 | SS Grade 50 | SS Grade 55 | SS Grade 60 | ASTM A1011/A1011M standard overview

Other Products