EN 10025-6 Steel Plate
EN 10025-6 S550QL1 Quenched & Tempered Steel Plate
EN 10025-6 S550QL1 Quenched and Tempered High Strength Steel Plate – Manufacturer and Exporter
Gangsteel supplies EN 10025-6 S550QL1 quenched and tempered high yield strength structural steel plate. S550QL1 is specified for welded, heavily loaded structures that need high yield strength and guaranteed toughness at –60 °C. For the full family of Q, QL and QL1 grades, see the EN 10025-6 category and the Low Alloy High Strength Steel section.
What is EN 10025-6 S550QL1 Steel Plate?
S550QL1 is a quenched and tempered structural steel grade defined in EN 10025-6. For nominal thicknesses up to 50 mm it has a minimum yield strength of 550 MPa. The steel number is 1.8986. The designation is read as follows:
- S — structural steel
- 550 — specified minimum yield strength in MPa for t ≤ 50 mm
- Q — quenched and tempered delivery condition
- L1 — quality with specified impact properties down to –60 °C
The same strength class is also supplied as S550Q (impact tested at –20 °C) and S550QL (impact tested at –40 °C). Adjacent EN 10025-6 grades in the same QL1 quality include S500QL1 and S620QL1. The number “550” must not be used as a design yield strength at every thickness: above 50 mm the specified minimum yield strength is reduced.
This page states which edition each table follows. EN 10025-6:2004+A1:2009 and EN 10025-6:2019+A1:2022 are not identical. The purchaser should name the required edition on the order, together with thickness, impact orientation and any optional tests.
Chemical Composition of S550QL1
The values below are maximum contents for heat analysis according to EN 10025-6:2004+A1:2009. The QL1 quality tightens phosphorus and sulphur relative to S550Q (P max 0.020 % and S max 0.010 %), and it is impact-tested at a lower temperature than S550QL.
| Element | Maximum % (heat analysis) | Element | Maximum % (heat analysis) |
|---|---|---|---|
| C | 0.20 | Ni | 2.0 |
| Si | 0.80 | Cu | 0.50 |
| Mn | 1.70 | Mo | 0.70 |
| P | 0.020 | Nb | 0.06 |
| S | 0.010 | N | 0.015 |
| B | 0.005 | Ti | 0.05 |
| Cr | 1.50 | V | 0.12 |
| — | — | Zr | 0.15 |
At least one grain-refining element (Nb, Ti, V, Zr, or aluminium) shall be present. The 0.015 % minimum applies to soluble aluminium; this is regarded as attained if the total aluminium content is at least 0.018 %. Carbon equivalent is limited by the standard and increases with product thickness; the applicable CEV limit should be taken from the edition named on the order.
Mechanical Properties of S550QL1
Elongation is for the proportional gauge length L0 = 5.65√S0. Impact values are longitudinal minima for the QL1 quality.
| Nominal thickness t | Minimum yield strength ReH (MPa) | Tensile strength Rm (MPa) | Minimum elongation A (%) | Longitudinal impact energy | Edition |
|---|---|---|---|---|---|
| 3 mm ≤ t ≤ 50 mm | 550 | 640–820 | 16 | 30 J at –60 °C (also 60 J at 0 °C / 50 J at –20 °C / 40 J at –40 °C) | 2004+A1:2009 and 2019+A1:2022 |
| 50 mm < t ≤ 100 mm | 530 | 640–820 | 16 | 30 J at –60 °C (also 60 J at 0 °C / 50 J at –20 °C / 40 J at –40 °C) | 2004+A1:2009 and 2019+A1:2022 |
| 100 mm < t ≤ 150 mm | 490 | 590–770 | 16 | 30 J at –60 °C (also 60 J at 0 °C / 50 J at –20 °C / 40 J at –40 °C) | 2004+A1:2009 |
| Test temperature | Longitudinal minimum average (J) |
|---|---|
| 0 °C | 60 |
| –20 °C | 50 |
| –40 °C | 40 |
| –60 °C | 30 |
Routine QL1 verification is normally the longitudinal Charpy V-notch test at –60 °C. Transverse testing is an ordering option and should be stated on the purchase order.
The tensile rows follow the 3–150 mm bands of EN 10025-6:2004+A1:2009. EN 10025-6:2019+A1:2022 extends the product scope for S550 grades to a maximum nominal thickness of 200 mm. The applicable property line for a plate thicker than 150 mm should be taken from the edition named on the order.
Actual results are reported on the mill test certificate for the delivered plate. The design check must use the requirement that applies to the ordered thickness, not the “550” in the grade name.
Production and Quality Control at Gangsteel
Gangsteel arranges production of EN 10025-6 S550QL1 plate in the quenched and tempered condition. Inspection scope should be written into the purchase order. Typical items buyers specify include:
- Heat analysis and mechanical testing to the named edition of EN 10025-6
- Charpy V-notch testing at –60 °C, with orientation and specimen size as agreed
- Ultrasonic testing to EN 10160 when required
- Through-thickness properties to EN 10164 (Z15 / Z25 / Z35) when required by the joint design
- Inspection documents to EN 10204 (commonly 3.1, or 3.2 when contractually required)
- Third-party inspection when the contract requires it
Z-quality, ultrasonic class and certificate type are not automatic with the grade name. For company and quality-system information, see About Us.
Available Sizes and Delivery Conditions
- Standard thickness range: 3 mm to 150 mm under EN 10025-6:2004+A1:2009. EN 10025-6:2019+A1:2022 extends the product scope for S550 grades to 200 mm. Available mill thickness should be confirmed for the edition named on the order.
- Width and length: supplied to the agreed dimensional standard (commonly EN 10029 for plate). Do not assume a fixed commercial size range.
- Delivery condition: quenched and tempered (Q).
Cutting, beveling or surface preparation can be discussed against drawings. Stock and lead time depend on thickness and quantity and should be confirmed at enquiry.
Main Applications of S550QL1
S550QL1 is selected when a higher yield strength than S500 is required and the design calls for guaranteed impact properties at –60 °C. Typical uses include mobile and industrial lifting structures, heavy transport frames, mining equipment and other welded assemblies where plate thickness or mass can be reduced relative to lower grades.
Equivalent Grades Comparison
The following designations are often compared with S550QL1 in procurement. They are approximate comparators, not interchangeable substitutes. Chemistry, thickness limits, impact temperature, testing and documentation must be checked against the project specification.
| Standard / designation | Grade | Relationship to S550QL1 | Note |
|---|---|---|---|
| EN 10025-6 | S550QL1 (1.8986) | Official standard grade | Specify the edition on the order |
| EN 10025-6, same strength, different quality | S550Q / S550QL | Same strength class; different impact test temperature | Not interchangeable without a toughness review |
| GB/T 16270 | Q550F, also Q550D / Q550E | Approximate Chinese QT analogue (F quality ≈ –60 °C impact class) | Different standard; confirm chemistry, thickness and tests |
A broader view of the EN 10025-6 family is on the EN 10025-6 category page. GB/T 16270 product pages are listed under GB/T 16270 high strength plate.
Related Products
- Same strength class: EN 10025-6 S550Q and EN 10025-6 S550QL
- Adjacent QL1 grades: S500QL1 and S620QL1
- Approximate Chinese QT analogue: GB/T 16270 Q550F
- Family overview: EN 10025-6 steel plate and Low Alloy High Strength Steel
Welding and Fabrication Recommendations
S550QL1 is intended to be weldable, but procedures must be qualified for this strength level. Generic procedures written for conventional S355-type steels are not sufficient. Recommended practice is to:
- Base preheat, interpass temperature and heat input on the actual heat chemistry, carbon equivalent, combined thickness and joint restraint — not on a generic temperature taken from another grade
- Use low-hydrogen consumables and controlled storage and handling
- Qualify the welding procedure (WPS/WPQR) for strength, toughness and hydrogen-cracking resistance in the heat-affected zone
- Treat any post-weld heat treatment as a design and procedure decision, because excessive temperature can reduce the properties obtained by quenching and tempering
- Use cutting, grinding and cold-forming allowances appropriate to high-strength quenched and tempered plate, including a larger bending radius than for lower-strength grades
Final fabrication parameters should be agreed with the mill or a qualified welding engineer for the actual plate thickness and joint design.
Why Choose Gangsteel as Your S550QL1 Supplier
- Supply of EN 10025-6 Q, QL and QL1 grades, with documentation to the edition named on the order
- Support for optional testing (ultrasonic class, Z-quality, third-party inspection) when specified
- Technical discussion of thickness, toughness quality and related grades such as S550Q or S500QL1
- Cutting or processing to drawing when agreed at order
Please contact Gangsteel with the required edition, thickness, quantity, impact test conditions and any optional tests. We will confirm availability and documentation against that enquiry.
Frequently Asked Questions
What is the difference between S550Q, S550QL and S550QL1?
These grades belong to the same EN 10025-6 strength class. S550Q is impact-tested at –20 °C; S550QL is impact-tested at –40 °C; S550QL1 is impact-tested at –60 °C. QL and QL1 also have tighter phosphorus and sulphur limits than Q. They should not be substituted for one another unless the design toughness requirement has been reviewed.
Which edition of EN 10025-6 should be specified?
The tensile table on this page follows the 3–150 mm bands of EN 10025-6:2004+A1:2009. EN 10025-6:2019+A1:2022 is the current European edition and extends this strength level to 200 mm. Name the edition and the required thickness on the order.
Can S550QL1 replace GB/T 16270 Q550F?
Only as an agreed substitution. Q550F is often compared with S550QL1 on strength class and impact-quality letter, but the standards, chemistry, thickness limits and test requirements differ. Use the grade named in the project specification, or obtain written approval for a substitute.
Why is the yield strength lower on thicker plate?
EN 10025-6 reduces the specified minimum yield strength as thickness increases: 550 MPa for 3 mm ≤ t ≤ 50 mm; 530 MPa for 50 mm < t ≤ 100 mm; 490 MPa for 100 mm < t ≤ 150 mm in the 2004+A1:2009 table. Design calculations must use the value for the actual thickness.
Does the grade automatically include ultrasonic testing or a 3.2 certificate?
No. Those are options to be stated on the order, together with any Z-quality or third-party inspection requirement.
What information is needed for a quotation?
Please send the edition of EN 10025-6, grade and quality (S550QL1 unless another quality is required), thickness, quantity, dimensional standard, impact test conditions, inspection document type, and any ultrasonic, Z-quality or third-party requirements via the contact page.
This article is based on EN 10025-6:2004+A1:2009 for the chemical and mechanical tables above, and on the published scope of EN 10025-6:2019+A1:2022 for the current maximum thickness of S550 grades. It also reflects Gangsteel’s experience in supplying quenched and tempered structural plate. It is not a substitute for the official standard or for the mill test certificate of the delivered plate.
-
EN 10025-6 S460QL Quenched &
Gangsteel is specialized in supplying EN10025-6 steel plate in S460 QL. EN 10025-6 S460QL,S460 QL,S460QL STEEL
-
EN 10025-6 S460Q Quenched &
Gangsteel is specialized in supplying EN10025-6 steel plate in Grade S460 Q. S460Q,EN10025-6 S460Q,S460 Q
-
EN 10025-6 S690Q,S690 Q,S690Q S
Gangsteel is specialized in supplying EN10025-6 steel plate in S690Q. S690Q,EN10025-6 S690Q,S690 Q
-
EN 10025-6 S890Q,S890 Q,S890Q S
Gangsteel is specialized in supplying EN 10025-6 steel plate in S890Q. EN 10025-6 S890Q,S890 Q,S890Q STEEL PLA