NV A40 steel plate, also written as DNV A40, DNV Grade A40, VL A40 (newer DNV Rules designation), AH40 or DNV AH40 ship steel plate, is the higher-strength hull structural steel of DNV Rules for Classification of Ships (IACS UR W11 higher-strength family) with 390 MPa minimum yield, 510-650 MPa tensile strength and Charpy V-notch toughness at 0°C [32°F]. In the grade name, "A" is the toughness class, and "40" refers to the strength level (historically about 40 kgf/mm²); the market name AH40 adds "H" for higher strength. Gangsteel, a steel plate exporter, supplies DNV NV A40 / AH40 plates cut to size for shipbuilding, offshore platforms and marine structures.

Data source: Per IACS UR W11 (ordinary/higher-strength hull structural steel) as adopted in DNV hull structural steel rules. Official mill/certificate grade is NV A40 (VL A40 under current DNV Rules); AH40 is the common IACS market name. Verify the current DNV edition before ordering.

NV A40 / AH40 Chemical Composition (Heat Analysis)

 

ElementCMnSiPSAl (acid sol.)
NV A40 / AH40, %0.18 max0.90-1.600.10-0.500.035 max0.035 max0.015 min
ElementNbVTiCuCrNi / Mo
NV A40 / AH40, %0.02-0.050.05-0.100.02 max0.35 max0.20 max0.40 max / 0.08 max

Per IACS UR W11 / DNV hull structural steel rules (higher-strength grades). Nb, V and Al grain-refining elements may be used singly or in combination; when used in combination the individual minima do not apply. Where acid-soluble Al is not less than 0.015%, the Si minimum does not apply. Carbon equivalent: Ceq = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15 (%).

Product Analysis (Check Analysis)

 

IACS UR W11 / DNV rules do not separately tabulate product (check) analysis limits for higher-strength grades. When product analysis is required, the finished plate shall meet the heat limits subject to ASTM A6/A6M Table A permitted variations (same practice as other IACS societies).

ElementHeat analysis limitProduct analysis (heat ± A6)
C0.18 max0.22 max
Mn0.90-1.600.81–1.72
Si0.10-0.500.04–0.56
P0.035 max0.045 max
S0.035 max0.045 max
Al (acid sol.)0.015 minno A6 Table A tolerance; product value not tabulated
Nb0.02-0.050.010–0.060
V0.05-0.100.040–0.110
Ti0.02 max0.03 max
Cu0.35 max0.38 max
Cr0.20 max0.24 max
Ni0.40 max0.43 max
Mo0.08 max0.09 max

Per IACS UR W11 / DNV hull structural steel rules. Product analysis applies only when specified; for a range, results may not vary both above and below it.

NV A40 Mechanical Properties

 

GradeYield strength, minTensile strengthElongation, min
NV A40390 MPa [57 ksi]510-650 MPa [74-94 ksi]20%

Per IACS UR W11 / DNV hull structural steel rules. Yield and tensile values apply for the full thickness range covered by the grade (typically up to 100 mm for these ship plates).

Charpy V-Notch Impact Requirements (0°C [32°F])

 

ThicknessTest temperatureLongitudinal, avg minTransverse, avg min
t≤50 mm0°C [32°F]39 J26 J
50<t≤70 mm0°C [32°F]46 J31 J
70<t≤100 mm0°C [32°F]55 J37 J

Per IACS UR W11 / DNV hull structural steel rules. Average of three full-size Charpy V-notch specimens; not more than one value below the average and none below 70% of it. Longitudinal values shown; transverse values apply when required by the rules or purchase order. Thicker plates (above 100 mm) may be supplied by agreement with adjusted impact requirements.

Delivery Condition and Deoxidation

Deoxidation: Killed, fine-grain practice. Delivery condition: A-class (NV A40 / AH40) grades may be as-rolled, controlled rolled, normalized or TMCP depending on thickness; thicker plates usually N or TMCP. Optional extras by agreement include ultrasonic testing, Z-direction (Z15/Z25/Z35) through-thickness testing and third-party DNV survey.

Thickness Coverage

Higher-strength DNV NV A/D/E/F 32/36/40 plates are commonly supplied from about 6 mm to 100 mm thick (up to 150 mm by agreement). Width 1500-4000 mm and length 6000-18000 mm are typical.

Equivalent Steel Grades of NV A40

 

Society / StandardEquivalent grade
DNVNV A40 / VL A40 (AH40)
LR (Lloyd's Register)LR AH40 steel plate
ABSABS AH40 steel plate
CCSCCS AH40 steel plate
GLGL AH40 steel plate
BVBV AH40 steel plate
NKNK A40 steel plate
KRKR A40 steel plate
RINARINA AH40 steel plate

IACS member societies harmonize ordinary and higher-strength hull grades under UR W11; dual certification (for example DNV + ABS, or DNV + ASTM A131) is common when ordered that way.

FAQ about DNV A40 / NV A40 Steel Plate

What is DNV A40 (NV A40) steel plate?

It is a higher-strength hull structural steel under DNV Rules for Classification of Ships (IACS UR W11), with 390 MPa minimum yield, 510-650 MPa tensile strength and Charpy toughness at 0°C [32°F]. The mill certificate grade is NV A40 (VL A40 in newer DNV Rules); AH40 is the common market name.

What does NV A40 / AH40 stand for?

NV (or VL) is the DNV grade prefix. The letter A is the toughness class (Charpy at 0°C [32°F]), and 40 is the strength level (historically about 40 kgf/mm², now 390 MPa min yield). AH40 adds "H" for higher strength in the IACS market naming.

What is the yield strength of DNV NV A40?

Minimum 390 MPa (57 ksi), tensile 510-650 MPa (74-94 ksi), elongation about 20% min.

What is the impact test temperature for NV A40?

Charpy V-notch at 0°C [32°F]. Longitudinal average minima are 39 J up to 50 mm, 46 J for 50-70 mm and 55 J for 70-100 mm.

What is the difference between NV A40 and other 40-class grades?

Same 390 MPa strength class. NV A40 at 0°C [32°F]; NV D40 at -20°C [-4°F]; NV E40 at -40°C [-40°F]; NV F40 at -60°C [-76°F]. Delivery condition follows the toughness letter rules.

What is the difference between NV A40 and NV A32?

Same A-class toughness (Charpy at 0°C [32°F]). NV A40 is strength class 40 (390 MPa min yield); NV A32 is strength class 32 (315 MPa min yield).

Is NV A40 the same as ABS AH40 or LR AH40?

Requirements are essentially harmonized under IACS UR W11. ABS AH40, LR AH40 and ASTM A131 AH40 (where listed) are counterparts; dual certification is common when ordered with the required surveys.

Is DNV NV A40 weldable?

Yes. Controlled carbon and Ceq give good weldability; preheat may be required for thick sections depending on Ceq and restraint.

What heat treatment is required for NV A40?

A-class (NV A40 / AH40) grades may be as-rolled, controlled rolled, normalized or TMCP depending on thickness; thicker plates usually N or TMCP.

What thickness is available for DNV A40?

Typical supply is about 6-100 mm thick (up to 150 mm by agreement), 1500-4000 mm wide and 6000-18000 mm long.

Other DNV Steel Plate Grades

DNV Grade A steel plate | DNV Grade B steel plate | DNV Grade D steel plate | DNV Grade E steel plate | DNV A32 steel plate | DNV A36 steel plate | DNV D32 steel plate | DNV D36 steel plate | DNV D40 steel plate | DNV E32 steel plate | DNV E36 steel plate | DNV E40 steel plate | DNV F32 steel plate | DNV F36 steel plate | DNV F40 steel plate | DNV AH36 steel plate | DNV EH40 steel plate

Equivalent Class Society Grades

DNV NV A40 / AH40 corresponds to the same grade under the other IACS member classification societies and ASTM A131: LR AH40 steel plate, ABS AH40 steel plate, CCS AH40 steel plate, GL AH40 steel plate, BV AH40 steel plate, NK A40 steel plate, KR A40 steel plate, RINA AH40 steel plate.