RINA steel plate
RINA Grade B Steel Plate | Grade B Shipbuilding Steel Plate
RINA Grade B steel plate, also written as RI/B, RINA B, Registro Italiano Navale Grade B or Grade B ship steel plate, is the ordinary-strength hull structural steel of RINA Rules for the Classification of Ships (IACS UR W11 ordinary-strength family) with 235 MPa minimum yield, 400-520 MPa tensile strength and Charpy V-notch toughness at 0°C [32°F]. Gangsteel, a steel plate exporter, supplies RINA Grade B / RI/B plates cut to size for shipbuilding, offshore platforms and marine structures.
Data source: Per IACS UR W11 (ordinary/higher-strength hull structural steel) as adopted in RINA (Registro Italiano Navale) hull structural steel rules. Official mill/certificate grade is RINA Grade B (RI/B). Verify the current RINA edition before ordering.
RINA Grade B Chemical Composition (Heat Analysis)
| Element | Heat analysis |
|---|---|
| C | 0.21 max |
| Mn | 0.80 min |
| Si | 0.35 max |
| P | 0.035 max |
| S | 0.035 max |
Per IACS UR W11 / RINA hull structural steel rules (ordinary-strength grades). Grade A uses a manganese minimum tied to carbon (Mn ≥ 2.5×C) and a C + Mn/6 limit of 0.40%. Grades D and E require fine-grain practice with acid-soluble Al not less than 0.015% when used as the grain-refining element.
Product Analysis (Check Analysis)
When product analysis is required, the finished plate shall meet the heat limits subject to ASTM A6/A6M Table A permitted variations (same practice as other IACS societies), unless a limit is min-only or calculated.
| Element | Heat analysis limit | Product analysis (heat ± A6) |
|---|---|---|
| C | 0.21 max | 0.25 max |
| Mn | 0.80 min | 0.74 min (A6 lower) |
| Si | 0.35 max | 0.40 max |
| P | 0.035 max | 0.045 max |
| S | 0.035 max | 0.045 max |
Per IACS UR W11 / RINA hull structural steel rules. Product analysis applies only when specified.
RINA Grade B Mechanical Properties
| Grade | Yield strength, min | Tensile strength | Elongation, min |
|---|---|---|---|
| RINA Grade B | 235 MPa [34 ksi] | 400-520 MPa [58-75 ksi] | 22% |
Per IACS UR W11 / RINA hull structural steel rules. Yield and tensile values apply for the full thickness range covered by the grade (typically up to 100 mm for these ship plates).
Charpy V-Notch Impact Requirements (0°C [32°F])
| Thickness | Test temperature | Longitudinal, avg min | Transverse, avg min |
|---|---|---|---|
| t≤50 mm | 0°C [32°F] | 27 J | 20 J |
| 50<t≤70 mm | 0°C [32°F] | 34 J | 24 J |
| 70<t≤100 mm | 0°C [32°F] | 41 J | 27 J |
Per IACS UR W11 / RINA hull structural steel rules. Average of three full-size Charpy V-notch specimens when impact testing is required; not more than one value below the average and none below 70% of it. For Grade A, impact testing is typically required only above 50 mm. Thicker plates (above 100 mm) may be supplied by agreement with adjusted impact requirements.
Delivery Condition and Deoxidation
Grade B is killed steel. Delivery may be as-rolled, controlled rolled, normalized or TMCP by thickness. Optional extras by agreement include ultrasonic testing, Z-direction (Z15/Z25/Z35) through-thickness testing and third-party RINA survey.
Thickness Coverage
Ordinary-strength RINA Grade A/B/D/E plates are commonly supplied from about 6 mm to 100 mm thick (up to 150 mm by agreement). Width 1500-4000 mm and length 6000-18000 mm are typical.
Equivalent Steel Grades of RINA Grade B
| Society / Standard | Equivalent grade |
|---|---|
| RINA (Registro Italiano Navale) | RINA Grade B steel plate (RI/B) |
| ABS | ABS Grade B steel plate |
| CCS | CCS Grade B steel plate |
| GL | GL Grade B steel plate |
| LR (Lloyd's Register) | LR Grade B steel plate |
| NK | NK Grade B steel plate |
| KR | KR Grade B steel plate |
| BV | BV Grade B steel plate |
IACS member societies harmonize ordinary-strength hull grades under UR W11; dual certification is common when ordered that way.
FAQ about RINA Grade B Steel Plate
What is RINA Grade B steel plate?
It is an ordinary-strength hull structural steel under RINA (Registro Italiano Navale) Rules for the Classification of Ships (IACS UR W11), with 235 MPa minimum yield, 400-520 MPa tensile strength and Charpy toughness requirements at 0°C [32°F] (by thickness). The mill certificate grade is RINA Grade B (RI/B).
What does RINA Grade B / RI/B stand for?
RINA is Registro Italiano Navale (also abbreviated RI on mill certificates). Grade B is the ordinary-strength toughness class tested at 0°C [32°F] (impact may be waived for Grade A at t≤50 mm per UR W11).
What is the yield strength of RINA Grade B?
Minimum 235 MPa (34 ksi), tensile 400-520 MPa (58-75 ksi), elongation about 22% min.
What is the impact test temperature for RINA Grade B?
Charpy V-notch at 0°C [32°F]. See the impact table for longitudinal/transverse minima by thickness band.
What is the difference between RINA Grades A, B, D and E?
Same 235 MPa ordinary-strength class. Toughness class differs: A at +20°C (often waived ≤50 mm), B at 0°C, D at -20°C, E at -40°C.
How does Grade B differ from higher-strength RINA AH32 / AH36?
Grade B is ordinary strength (235 MPa). RINA AH32/AH36/AH40 families are higher-strength (315/355/390 MPa) under the same UR W11 framework.
Is RINA Grade B weldable?
Yes. Ordinary-strength ship plates are widely welded with standard procedures; follow approved WPS for thickness and Ceq.
What heat treatment is required for RINA Grade B?
Grade B is killed steel. Delivery may be as-rolled, controlled rolled, normalized or TMCP by thickness.
What thickness is available for RINA Grade B?
Typical supply is about 6-100 mm thick (up to 150 mm by agreement), 1500-4000 mm wide and 6000-18000 mm long.
Other RINA Steel Plate Grades
RINA Grade A steel plate | RINA Grade D steel plate | RINA Grade E steel plate | RINA AH32 steel plate | RINA AH36 steel plate | RINA AH40 steel plate | RINA DH32 steel plate | RINA DH36 steel plate | RINA DH40 steel plate | RINA EH32 steel plate | RINA EH36 steel plate | RINA EH40 steel plate | RINA FH32 steel plate | RINA FH36 steel plate | RINA FH40 steel plate
Equivalent Class Society Grades
RINA Grade B corresponds to the same ordinary-strength grade under other IACS member classification societies: ABS Grade B steel plate, CCS Grade B steel plate, GL Grade B steel plate, LR Grade B steel plate, NK Grade B steel plate, KR Grade B steel plate, BV Grade B steel plate, RINA Grade B steel plate.
-
RINA DH36 Steel Plate | DH36 Sh
RINA DH36 (RI/DH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at -20C, chemistry and
-
RINA AH36 Steel Plate | AH36 Sh
RINA AH36 (RI/AH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at 0C, chemistry and e
-
RINA FH32 Steel Plate | FH32 Sh
RINA FH32 (RI/FH32) shipbuilding steel plate: 315 MPa yield, 440-590 MPa tensile, Charpy at -60C, chemistry and
-
RINA Grade A Steel Plate | Grad
RINA Grade A (RI/A) shipbuilding steel plate: 235 MPa yield, 400-520 MPa tensile, Charpy at +20C, chemistry and