At Gangsteel, we’re excited to present the detailed EN 10025 S355N specifications, outlining the properties of this high-strength, low-alloy structural steel under EN 10025-3. Renowned for its fine-grain structure, 355 MPa yield strength, and -20°C toughness, S355N is a top choice for structural projects like bridges, cranes, and building frameworks in moderate climates.
As part of the en 10025 3 normalized steel plate family, EN 10025 S355N delivers reliable performance. Gangsteel explores its chemical composition, mechanical properties, delivery conditions, and applications, comparing it to grades like en 10025 3 s420n normalized structural steel plate and en 10025 3 s460n normalized structural steel plate. For more details, visit our en 10025 3 s355n normalized structural steel plate page.
EN 10025 S355N is a high-strength, low-alloy structural steel under the EN 10025-3:2019 standard, with a minimum yield strength of 355 MPa for plates up to 16 mm thick. Its designation, also known as material number 1.0545, breaks down as:
The normalization process refines the grain structure, enhancing EN 10025 S355N specifications for strength, toughness, and weldability, ideal for moderate climates. Compared to en 10025 3 s460n normalized structural steel plate, S355N offers lower strength (355 MPa vs 460 MPa) but is more cost-effective for general structural applications.
Gangsteel ensures EN 10025 S355N meets stringent chemical composition standards for optimal performance:
|
Element |
Ladle Analysis (max %) |
Product Analysis (max %) |
Role in Properties |
|---|---|---|---|
|
Carbon (C) |
0.20 |
0.22 |
Enhances strength, kept low for weldability and toughness. |
|
Silicon (Si) |
0.50 |
0.55 |
Aids deoxidation, improves strength and microstructure. |
|
Manganese (Mn) |
0.90-1.65 |
0.85-1.75 |
Boosts strength and toughness for load-bearing capacity. |
|
Phosphorus (P) |
0.030 |
0.035 |
Minimized to reduce inclusions, enhancing toughness. |
|
Sulfur (S) |
0.025 |
0.030 |
Low levels prevent inclusions, improving weld quality. |
|
Nitrogen (N) |
0.025 |
0.027 |
Controlled to avoid brittleness, supporting toughness. |
|
Aluminum (Al) |
0.020 (min, total) |
0.015 (min, total) |
Refines grains for toughness, improves microstructure. |
|
Niobium (Nb) |
0.05 |
0.06 |
Promotes fine-grain structure, enhancing strength and toughness. |
|
Vanadium (V) |
0.10 |
0.12 |
Increases strength via precipitation hardening. |
|
Titanium (Ti) |
0.05 |
0.06 |
Refines grains, supports toughness. |
|
Chromium (Cr) |
0.30 |
0.35 |
Enhances corrosion resistance and strength. |
|
Nickel (Ni) |
0.50 |
0.55 |
Improves toughness in moderate climates. |
|
Molybdenum (Mo) |
0.10 |
0.12 |
Boosts strength and creep resistance. |
|
Copper (Cu) |
0.55 |
0.60 |
Enhances corrosion resistance and strength. |
Carbon Equivalent (CEV): Capped at 0.43% for plates up to 63 mm, calculated as CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15, ensuring excellent weldability, similar to en 10025 3 s420n normalized structural steel plate.
Gangsteel guarantees EN 10025 S355N specifications deliver top performance for structural applications:
|
Thickness (mm) |
Yield Strength (min, MPa) |
Tensile Strength (MPa) |
Elongation (min, %) |
Impact Energy (min, J @ -20°C) |
|---|---|---|---|---|
|
≤16 |
355 |
470-630 |
22 |
27 |
|
16<t≤40 |
345 |
470-630 |
22 |
27 |
|
40<t≤63 |
335 |
470-630 |
22 |
27 |
|
63<t≤80 |
325 |
470-630 |
22 |
27 |
|
80<t≤100 |
315 |
470-630 |
22 |
27 |
|
100<t≤150 |
295 |
450-610 |
22 |
27 |
|
150<t≤200 |
285 |
450-610 |
22 |
27 |
Gangsteel provides EN 10025 S355N with specifications outlined in EN 10025-3:
EN 10025 S355N specifications ensure excellent weldability with a low CEV (≤0.43%):
Gangsteel supplies EN 10025 S355N for projects that rely on its specifications:
For colder climates requiring -50°C toughness, consider en 10025 3 s355nl normalized structural steel plate.
Gangsteel is your trusted source for EN 10025 S355N:
Contact us for en 10025 3 s355n normalized structural steel plate.
What are the EN 10025 S355N specifications?
EN 10025 S355N specifications include a yield strength of ≥355 MPa, tensile strength of 470-630 MPa, ≥22% elongation, and ≥27 J impact toughness at -20°C.
How do EN 10025 S355N specifications perform in moderate climates?
EN 10025 S355N specifications, with ≥27 J impact toughness at -20°C, ensure reliability for bridges and cranes in temperate environments.
Is EN 10025 S355N weldable per its specifications?
Yes, EN 10025 S355N specifications include a CEV ≤0.43%, enabling easy welding with GMAW or SAW, often without preheating for thinner plates.
What applications use EN 10025 S355N specifications?
EN 10025 S355N specifications support bridges, cranes, building frameworks, and heavy machinery in moderate climates, leveraging high strength and ductility.
How do EN 10025 S355N specifications compare to S420N?
EN 10025 S355N has lower yield strength (355 MPa vs 420 MPa) than S420N, but offers higher elongation (≥22% vs ≥19%) for better formability.
What certifications support EN 10025 S355N specifications?
Gangsteel provides EN 10025 S355N with EN 10204 3.1/3.2, UT testing (EN 10160), and ABS/LR/BV/DNV approvals for global compliance.
ASTM A516 GR 70 equivalent materials is such as ASME SA516 GR 70, EN 10028 P355GH, and BS1501 224-490 A & B, sh
we supply high-quality A516 Gr 70 steel plate for pressure vessel applications and other standards like ASTM A2
EN10028-2 P355GH for High-Strength Low-Alloy Columbium-Vanadium Structural Steel EN10025-2 S355J2 Structural St
We export A240 304L Stainless Coil 2B, NO.1 No.4 surface, the thickness 0.1mm to 3mm, 3mm to 22mm, Mother mill