Weather resistant steel plate
JIS G3125 SPA-C Cold Rolled Weathering Steel Sheet and Coil

JIS G3125 SPA-C — also written JIS G3125 SPA-C, SPAC, SPA C, JIS G 3125 SPA-C cold-rolled weathering steel and SPA-C corten sheet — is the cold-rolled grade of JIS G 3125, the Japanese standard for superior atmospheric corrosion resisting rolled steels, supplied as sheet and strip from 0.6 to 2.3 mm with a minimum yield strength of 315 N/mm². Gangsteel supplies SPA-C cold-rolled coils and sheets for thin weather-resistant panels and formed parts.
What is JIS G3125 SPA-C?
SPA-C stands for Steel, Phosphorus-Added, Cold-rolled. It has exactly the same chemistry as SPA-H — phosphorus 0.070–0.150% with copper, chromium and nickel — but it is cold reduced and annealed, which gives a smoother surface, tighter thickness tolerances and higher elongation (26% min) in gauges where hot-rolled strip is not practical. Its strength is lower than SPA-H because of the annealed microstructure.
JIS G3125 SPA-C Chemical Composition (Heat Analysis, %)
| Grade | C | Si | Mn | P | S | Cu | Cr | Ni |
|---|---|---|---|---|---|---|---|---|
| SPA-C | ≤0.12 | 0.20–0.75 | ≤0.60 | 0.070–0.150 | ≤0.035 | 0.25–0.55 | 0.30–1.25 | ≤0.65 |
| SPA-H | ≤0.12 | 0.20–0.75 | ≤0.60 | 0.070–0.150 | ≤0.035 | 0.25–0.55 | 0.30–1.25 | ≤0.65 |
Manganese may be raised to 1.0% maximum by agreement between purchaser and manufacturer, and other alloying elements may be added where necessary; any element added outside Table 2 has to be stated on the inspection document. JIS G 3125 specifies heat (ladle) analysis only and gives no separate product analysis limits. The high phosphorus window (0.070–0.150%) together with copper, chromium and nickel is what forms the dense, adherent rust layer that gives SPA steels their weather resistance.
JIS G3125 SPA-C Mechanical Properties
| Product and thickness | Yield point or proof stress, N/mm² | Tensile strength, N/mm² | Elongation, % | Test piece |
|---|---|---|---|---|
| Cold-rolled sheet and strip, 0.6 to 2.3 mm | ≥315 | ≥450 | ≥26 | No. 5 |
Two tension test pieces are taken when a test lot exceeds 50 t. A test lot for cold-rolled material is one heat with the same thickness and the same rolling and heat-treatment conditions.
Bend Test
| Product and thickness | Bend angle | Bend | Test piece |
|---|---|---|---|
| Cold-rolled sheet and strip, 0.6 to 2.3 mm | 180° | Inside spacing of one sheet thickness (vise method) | No. 1, 15–50 mm wide |
The bend test may be omitted by the manufacturer unless the purchaser specifies it, but the material must still meet the requirement if tested.
Delivery Condition and Heat Treatment
SPA-C is delivered cold rolled, in the annealed state produced by the manufacturer’s own cold-rolling and annealing route; JIS G 3125 does not prescribe a heat treatment, but each test lot is formed from material with the same rolling and heat-treatment conditions. Sheets and coils are oiled for protection in transit, and dimensional and flatness tolerances follow JIS G 3141, with tolerance class A by default.
| Item | Delivery condition per JIS G 3125 |
|---|---|
| Condition | Cold rolled and annealed by the manufacturer’s process; no separate heat treatment is specified |
| Product forms | Cold-rolled sheet and strip (coil), 0.6 to 2.3 mm |
| Surface | Cold-rolled finish |
| Oiling | Oiled |
| Tolerances | JIS G 3141, thickness tolerance A and flatness tolerance A unless agreed otherwise |
Ordering Information
| Ordering item | What to state on the enquiry |
|---|---|
| Standard | JIS G 3125 (current edition: 2021) |
| Grade | SPA-C |
| Product form | Cold-rolled sheet or strip (coil) |
| Dimensions | Thickness (0.6 to 2.3 mm), width, length or coil |
| Edge | Mill edge or cut edge |
| Tolerances | JIS G 3141, class A unless otherwise agreed |
| Mass | Quantity and maximum coil mass |
| Optional | Mn up to 1.0%, bend test, third-party inspection |
Comparable Grades
For comparison only, SPA-C is the cold-rolled counterpart of SPA-H and of hot-rolled phosphorus-enhanced weathering steels such as Corten A and S355J0WP. In the American system, ASTM A606 covers both hot- and cold-rolled high-strength weathering sheet.
Applications
Typical uses are container roof and side panels in thin gauge, railway coach interiors and roof sheets, exhaust and duct components, electrical cabinets and enclosures for outdoor service, and architectural panels where a uniform weathered surface is wanted on thin sheet.
Documents, Inspection and Lead Time
Every SPA-C shipment from Gangsteel is supplied with an inspection certificate (JIS G 0415 / EN 10204 type 3.1 by default) and marked with the grade symbol, heat or inspection number, dimensions, manufacturer and quantity or mass. Third-party inspection to EN 10204 3.2 by SGS, BV, TUV or another nominated agency can be arranged. Lead time is confirmed with each enquiry against the mill rolling schedule and any processing (descaling, slitting, cutting) required; send us the size list for a firm date.
FAQ
What is the difference between SPA-C and SPA-H?
The chemistry is identical; the difference is the product route. SPA-H is hot rolled, up to 16 mm, with 355 N/mm² minimum yield and 490 N/mm² minimum tensile. SPA-C is cold rolled and annealed, 0.6 to 2.3 mm, with 315 N/mm² yield, 450 N/mm² tensile and 26% minimum elongation. SPA-C gives a better surface and tighter tolerances for thin panels; SPA-H is used where higher strength or thicker sections are needed.
Can SPA-C be formed and welded?
Yes. With 26% minimum elongation and a 180° bend requirement of one sheet thickness inside spacing, SPA-C accepts ordinary press forming and roll forming. In thin gauge it welds well by resistance spot welding and MIG/MAG; weathering-type filler wire should be used if the weld is to be left bare.
Why is SPA-C limited to 2.3 mm?
JIS G 3125 restricts the cold-rolled grade to 0.6–2.3 mm, the range in which cold reduction gives a real advantage in surface and tolerance. For thicker weather-resistant sheet, hot-rolled SPA-H (up to 16 mm) is ordered instead.
Does SPA-C need painting?
It can be used bare where the environment lets the patina stabilise, but most SPA-C goes into painted products such as container panels and enclosures, where the weathering chemistry slows corrosion under damaged paint and at cut edges. In marine or permanently wet service, painting is required.
What certificate comes with SPA-C?
An inspection certificate to JIS G 0415 / EN 10204 type 3.1 with heat analysis, tension test results and, if ordered, bend test results is the default. Third-party inspection is available on request.
Related Grades
JIS G3125 SPA-H | JIS G3125 standard overview | JIS G3114 weathering steels | Weather resistant steel
-
ASTM A588 Grade B|A588 Gr.B STE
Gangsteel is specialized in supplying ASTM A588 steel plate in A588 Grade B,A588 GradeA,A588 Grade C,A588 Grade
-
ASTM A588 Grade A|A588 Gr.A STE
Gangsteel is specialized in supplying ASTM A588 steel plate in A588 Grade A,A588 Grade B,A588 Grade C,A58
-
ASTM A588 Grade K|A588 Gr.K STE
Gangsteel is specialized in supplying ASTM A588 steel plate in A588 Grade K,A588 Grade A,A588 Grade B,A588 Grad
-
GB/T 4172 Q460NH Steel Plate su