Weather resistant steel plate
JIS G3125 SPA-H Weathering Steel Sheet, Coil and Plate

JIS G3125 SPA-H — also written JIS G3125 SPA-H, SPAH, SPA H, JIS G 3125 SPA-H weathering steel, SPA-H corten steel and SPA-H atmospheric corrosion resistant steel — is the hot-rolled grade of JIS G 3125, the Japanese standard for superior atmospheric corrosion resisting rolled steels. It is a copper-chromium-nickel-phosphorus weathering steel supplied as plate, strip and sections up to 16 mm thick, with a minimum yield strength of 355 N/mm². Gangsteel supplies SPA-H as hot-rolled coil, cut-to-length sheet and plate for containers, rail wagons, facades and outdoor structures.
What is JIS G3125 SPA-H?
SPA-H stands for Steel, Phosphorus-Added, Hot-rolled. Unlike the JIS G 3114 SMA weldable weathering steels, which keep phosphorus at 0.035% max, SPA steels deliberately use 0.070–0.150% phosphorus. Phosphorus is one of the most effective elements for atmospheric corrosion resistance, so SPA-H develops a protective oxide layer quickly and is roughly comparable in behaviour to the “Cor-Ten A” type of steels. The price of the high phosphorus is reduced toughness and weldability in heavy sections, which is why the standard limits SPA-H to 16 mm.
JIS G3125 SPA-H Chemical Composition (Heat Analysis, %)
| Grade | C | Si | Mn | P | S | Cu | Cr | Ni |
|---|---|---|---|---|---|---|---|---|
| SPA-H | ≤0.12 | 0.20–0.75 | ≤0.60 | 0.070–0.150 | ≤0.035 | 0.25–0.55 | 0.30–1.25 | ≤0.65 |
| SPA-C | ≤0.12 | 0.20–0.75 | ≤0.60 | 0.070–0.150 | ≤0.035 | 0.25–0.55 | 0.30–1.25 | ≤0.65 |
Manganese may be raised to 1.0% maximum by agreement between purchaser and manufacturer, and other alloying elements may be added where necessary; any element added outside Table 2 has to be stated on the inspection document. JIS G 3125 specifies heat (ladle) analysis only and gives no separate product analysis limits. The high phosphorus window (0.070–0.150%) together with copper, chromium and nickel is what forms the dense, adherent rust layer that gives SPA steels their weather resistance.
JIS G3125 SPA-H Mechanical Properties
| Product and thickness | Yield point or proof stress, N/mm² | Tensile strength, N/mm² | Elongation, % | Test piece |
|---|---|---|---|---|
| Plate and strip, ≤6.0 mm | ≥355 | ≥490 | ≥22 | No. 5 |
| Plate and strip, >6.0 mm (up to 16 mm), and sections | ≥355 | ≥490 | ≥15 | No. 1A |
For plate and strip under 3 mm, a minimum tensile strength of 510 N/mm² may be applied by agreement. Two tension test pieces are taken when a test lot exceeds 50 t. A test lot for plate is one heat with the maximum thickness not more than twice the minimum; for strip, one heat and one thickness; for sections, one heat and one section shape.
Bend Test
| Product and thickness | Bend angle | Inside radius | Test piece |
|---|---|---|---|
| Plate and strip, ≤6.0 mm | 180° | 0.5 × thickness (1.0 × thickness by agreement) | No. 1 |
| Plate and strip >6.0 mm, and sections | 180° | 1.5 × thickness | No. 1 |
The bend test may be omitted by the manufacturer unless the purchaser specifies it, but the material must still meet the requirement if tested.
Delivery Condition and Heat Treatment
SPA-H is delivered in the hot-rolled condition: JIS G 3125 does not call for normalizing or any other heat treatment, and the strength comes from the chemistry and hot rolling. As-rolled material is shipped unoiled with its mill scale; when the purchaser asks for descaling (pickling or shot blasting) the steel is oiled for protection. Users who rely on bare weathering should remove the mill scale before exposure so that the protective patina develops uniformly.
| Item | Delivery condition per JIS G 3125 |
|---|---|
| Condition | Hot rolled (as rolled); no heat treatment is specified |
| Product forms | Plate, strip (coil) and sections, thickness up to 16 mm |
| Surface | As rolled with mill scale; descaled by pickling or shot blasting when ordered |
| Oiling | Descaled material is oiled; as-rolled plate, strip and sections are not oiled |
| Edges | Mill edge or cut edge, as ordered |
| Dimensions and tolerances | JIS G 3193 (plate and strip), JIS G 3192 (sections) |
Ordering Information
| Ordering item | What to state on the enquiry |
|---|---|
| Standard | JIS G 3125 (current edition: 2021) |
| Grade | SPA-H |
| Product form | Plate, strip (coil) or section |
| Dimensions | Thickness (up to 16 mm), width, length or coil |
| Edge | Mill edge or cut edge |
| Descaling | As rolled, or pickled / shot blasted |
| Mass | Quantity and maximum coil mass |
| Optional | Mn up to 1.0%, TS 510 N/mm² min under 3 mm, bend test, third-party inspection |
Comparable Grades
For comparison only, SPA-H is close in concept to Corten A and to EN 10025-5 S355J0WP (both phosphorus-enhanced weathering steels), and to the ASTM A242 Type 1 concept (ASTM A242). For thicker or more heavily welded structures, the low-phosphorus weathering grades JIS G3114 SMA490AW, ASTM A588 Grade B, S355J2W, Corten B or GB/T 4171 Q355NH are the usual choice.
Applications
Typical uses are freight container panels and frames, railway wagons and coaches, bus and truck bodies, chimneys and ducts, architectural cladding and facades, guard rails, bridges with thin members, and outdoor landscape steel.
Documents, Inspection and Lead Time
Every SPA-H shipment from Gangsteel is supplied with an inspection certificate (JIS G 0415 / EN 10204 type 3.1 by default) and marked with the grade symbol, heat or inspection number, dimensions, manufacturer and quantity or mass. Third-party inspection to EN 10204 3.2 by SGS, BV, TUV or another nominated agency can be arranged. Lead time is confirmed with each enquiry against the mill rolling schedule and any processing (descaling, slitting, cutting) required; send us the size list for a firm date.
FAQ
What is the difference between SPA-H and SMA weathering steel?
Both are weathering steels, but SPA-H (JIS G 3125) adds phosphorus at 0.070–0.150% to maximise atmospheric corrosion resistance, while SMA grades (JIS G 3114) keep phosphorus at 0.035% max and are designed as weldable structural steels with impact-tested qualities and thicknesses up to 200 mm. SPA-H is limited to 16 mm and has no impact requirement, so it is used for thin, lightweight structures such as containers and wagons rather than heavy welded bridges.
Is SPA-H the same as Corten A?
Not formally. Corten A is a trade name of a phosphorus-enhanced Cu-Cr-Ni steel, and SPA-H is a JIS designation with its own chemistry window and test rules. The two have very similar chemistry and minimum strength (355 N/mm² yield, 490 N/mm² tensile), so they are commonly treated as alternatives in container and wagon building. If a drawing calls for one, confirm with the designer before substituting the other.
Can SPA-H be welded?
Yes, in the thin gauges for which it is intended. The high phosphorus makes the weld metal and heat-affected zone more sensitive to hardening and cracking as thickness increases, so low-hydrogen consumables with matching weathering chemistry (for example Cu-Ni or Cu-Cr-Ni wire) should be used, and joint restraint kept low. For thicknesses above 16 mm or for heavily restrained structures, a JIS G 3114 SMA grade is the better choice.
What thickness range is covered by SPA-H?
JIS G 3125 applies SPA-H to hot-rolled plate, strip and sections up to and including 16 mm. The mechanical requirements change at 6.0 mm: up to 6.0 mm the minimum elongation is 22% (No. 5 test piece) and the bend radius 0.5t; above 6.0 mm the minimum elongation is 15% (No. 1A test piece) and the bend radius 1.5t.
Does SPA-H need painting?
In many outdoor environments SPA-H can be left unpainted once the scale is removed, because the patina slows further corrosion. In marine spray, permanently wet or chloride-rich environments the patina does not stabilise, and painting is still needed; container builders normally paint SPA-H, using its weathering chemistry to reduce corrosion under damaged coating.
What certificate comes with SPA-H from Gangsteel?
The default is a JIS G 0415 / EN 10204 type 3.1 inspection certificate with heat analysis, tension test and, when ordered, bend test results, plus the heat number and dimensions. Any alloying added beyond Table 2 is stated on the certificate. Third-party inspection (3.2) can be arranged.
Related Grades
JIS G3125 SPA-C | JIS G3125 standard overview | JIS G3114 weathering steels | Weather resistant steel
-
ASTM A588 Grade B|A588 Gr.B STE
Gangsteel is specialized in supplying ASTM A588 steel plate in A588 Grade B,A588 GradeA,A588 Grade C,A588 Grade
-
ASTM A588 Grade A|A588 Gr.A STE
Gangsteel is specialized in supplying ASTM A588 steel plate in A588 Grade A,A588 Grade B,A588 Grade C,A58
-
ASTM A588 Grade K|A588 Gr.K STE
Gangsteel is specialized in supplying ASTM A588 steel plate in A588 Grade K,A588 Grade A,A588 Grade B,A588 Grad
-
GB/T 4172 Q460NH Steel Plate su
GB/T 4172 Q460NH steel plate melds titanic strength with impervious weathering, galvanizing architects to erect