Clad Steel Plate
A516 Grade 70 + 304L Stainless Clad Steel Plate
A516 Grade 70 + 304L Stainless Clad Steel Plate combines an A516 pressure-vessel backing with a low-carbon 304L corrosion-resistant face. The two layers have separate chemistry, thermal requirements and jobs in the design; the composite must be qualified as a bonded plate. Gangsteel builds the enquiry around separate backing and facing certificates, the finished bond and the actual fabrication requirements.

Material Pair and Engineering Use
This is a practical candidate for chemical process shells, storage equipment and other fabricated components where 304L is compatible with the wetted service. It reduces the amount of stainless used through the wall, but the economic result depends on area, thickness ratio, forming and weld-restoration requirements. It is not a blanket recommendation for chloride-rich media.
| Part | Designation | Role |
|---|---|---|
| Backing | ASTM A516/A516M-25 Grade 70 [485] | Pressure-retaining strength and structural wall thickness |
| Facing | ASTM A240/A240M-25a 304L (S30403) | Selected corrosion-resistant surface |
| Composite | ASTM A264; contractual edition stated in order | Bonded product, not two loosely assembled plates |
The clad-standard scope follows ASTM's A264-12(2026) listing. The clause-level manufacturing and test discussion uses the accessible A264-12(2019) text; the purchase order must name the contractual edition. Component data below identify their own editions and are not a claim of automatic ASME certification.
Backing Steel Chemical Composition
| Backing thickness | C max | Mn | Si | P max | S max |
|---|---|---|---|---|---|
| ≤12.5 mm | 0.27 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >12.5–50 mm | 0.28 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >50–100 mm | 0.30 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >100 mm | 0.31 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
Thickness in this table is the backing-steel thickness, not the sum of the layers. For each 0.01 percentage-point reduction below the specified carbon maximum, A516/A516M-25 permits a 0.06 percentage-point increase above the manganese maximum, up to 1.50% on heat analysis and 1.60% on product analysis. Product-analysis manganese and silicon ranges differ from heat analysis; compare the correct certificate column. Special supplementary chemistry provisions must be stated in the order.
Corrosion-Resistant Facing Chemical Composition
| Element | Requirement |
|---|---|
| C | ≤0.030 |
| Mn | ≤2.00 |
| Si | ≤0.75 |
| P | ≤0.045 |
| S | ≤0.030 |
| Cr | 18.0–20.0 |
| Ni | 8.0–12.0 |
| N | ≤0.10 |
| Fe | Balance |
Mechanical Properties: Backing, Facing and Bond
| Layer / reference | Applicable reference condition | Yield / Rp0.2 min, MPa | Tensile, MPa | Elongation min |
|---|---|---|---|---|
| A516/A516M-25 Grade 70 [485] backing | All qualified plate thicknesses; no fixed maximum thickness in A516 | 260 | 485–620 | 21% in 50 mm; 17% in 200 mm; A20 adjustments apply |
| 304L S30403 facing; ASTM A240/A240M-25a | Annealed flat product | 170 | 485 min | 40% in 50 mm |
The cladding row describes the separately specified flat-product reference condition. It is not a requirement to extract a tiny tensile coupon from every finished facing. Finished clad-plate tensile acceptance follows the clad specification and the selected test section. Do not add the two tensile strengths or substitute bond shear strength for backing tensile strength. Cladding strength can enter vessel calculations only when the construction code and design permit it.
| Test decision | Application to this material pair | Order action |
|---|---|---|
| Tensile section | The Grade 70 [485] backing minima, 485 MPa tensile and 260 MPa yield, satisfy the cited 485/275 MPa strength thresholds. Total gage still determines the applicable section. | At total gage up to 1.5 in. (about 38 mm), the composite section is the general route unless the corrosion-only provision is used. Above that gage use backing-only testing. |
| Backing-only option | When the facing is for corrosion allowance only, it need not be included in the tensile specimen. | Identify this basis and retain the backing tensile limits; a face-excluded test is not a test of the facing. |
| Required bond test | Where the purchaser specifies the interface shear route, the minimum is 20 ksi (140 MPa). | Specify the coupon requirement, facing thickness and any agreed thin-facing procedure; this is not 140 MPa plate tensile strength. |
| Area integrity | One mechanical bond specimen does not sample all of the 304L face. | Agree ultrasonic method, coverage, acceptance class and the treatment of areas that will become formed or welded edges. |
The ASTM clad specification uses inch-pound values as controlling requirements. The 0.075 in. (1.9 mm) shear-coupon facing provision and any agreed testing at or below that thickness must be considered before choosing a thin corrosion layer. The standard overview explains the general test hierarchy in more detail.
Fabrication Considerations for This Pair
Low carbon reduces susceptibility to chromium-carbide sensitization, but does not make every bonding or fabrication heat cycle harmless. Evaluate the final stainless condition, the backing toughness and the weld restoration together. A 304 certificate alone does not establish 304L compliance; dual certification requires both sets of requirements to be met.
Order the base and minimum finished facing thicknesses separately. There is no universal standard layer ratio for this pair. A drawing notation such as 20 + 3 mm means 20 mm backing plus 3 mm facing only if that order is explicitly stated; it is an illustration of notation, not a stock-size or capacity claim. Assess forming strain, cut-edge restoration and any local thinning before fixing the purchase allowance.
Bonding Process, Delivery and Heat Treatment
Explosion bonding joins prepared metal surfaces by a controlled high-velocity collision. Hot-roll bonding establishes the metallurgical bond during rolling of a prepared assembly; explosion bonding followed by rolling is a separate combined route. These are integrally bonded plates, not loose liners, adhesive laminates or chromium-carbide weld-overlay wear plates.
For austenitic stainless facing, A264-12(2019) describes heat treatment for carbide solution followed by individual air cooling unless otherwise specified or agreed. For plate made without hot rolling, components may be treated separately before bonding. Duplex stainless requires an agreed heat-treated condition; it is not covered by an assumed austenitic cycle.
| Parameter | Required order definition | Technical note |
|---|---|---|
| Bonding route | Explosion bonded, hot-roll bonded, or combined route | Route capability depends on the material pair, area, layer ratio and final condition. No blanket stock range is implied. |
| Thickness | Backing thickness + minimum facing thickness, in mm; identify one or two clad faces | Reserve facing allowance for grinding, forming and weld restoration. Total thickness alone is insufficient. |
| Final thermal condition | Named delivery condition and any simulated fabrication/PWHT cycle | Test in the representative final condition; agree number and duration of simulated cycles where required. |
| Heat-treatment temperature / hold | Qualified procedure for the selected pair and thickness | No single temperature, hold time or cooling rate is specified here for all clad plates. |
| Surface and cutting | As agreed: pickled, ground or specified finish; edge machining and protection | Prevent carbon-steel contamination of the corrosion-resistant face. |
| Lead time | Confirmed against the enquiry and agreed inspection plan | Not a fixed number of days for every thickness or bonding route. |
For an A516 backing, A516/A516M-25 normally requires normalization above 1.5 in. [40 mm]; thinner plate may be normalized when ordered. That backing rule does not authorize a final composite furnace cycle without checking the facing and clad-standard requirements. The two standards use different rounded metric values for 1.5 in.; do not substitute the 40 mm heat-treatment boundary for the clad-standard tensile boundary.
Inspection and Certification
Gangsteel separates incoming-material traceability, finished-plate mechanical qualification and bond-area examination in the inspection plan. Keep the backing heat number, facing heat/lot, plate identity and final thermal history linked through cutting. State the examination stage, coverage and acceptance class before manufacture; a certificate description such as "UT tested" without a method and class is incomplete.
| Check | What to specify | Acceptance concern |
|---|---|---|
| Chemistry and identity | Backing and facing specifications; heat analysis and product analysis if ordered | Do not report an averaged composite chemistry as either layer. |
| Tensile testing | Composite or backing-only section under the governing clad standard | State specimen section, direction and final test condition. |
| Bond examination | Ultrasonic method, acceptance class, coverage and edge/cut-zone requirements | Map reportable unbonded areas; distinguish scanning coverage from bonded-area percentage. |
| Bond mechanical test | Shear or alternative bend route where applicable | Record specimen location and criterion; do not relabel shear as tensile. |
| Forming / corrosion tests | Required bends, intergranular corrosion or project-specific tests by agreement | A low-carbon designation does not replace a specified corrosion test. |
| Additional service tests | Backing impact, HIC/SSC and simulated PWHT only when required by specification/code/order | No automatic sour-service, low-temperature or hydrogen-service qualification. |
| Documentation | Layer certificates, test reports, UT map, thermal records and agreed inspection release | An inspection certificate does not itself approve the vessel design. |
Frequently Asked Questions
Why choose 304L rather than ordinary 304 for a clad vessel?
The lower carbon limit is useful when the wetted face sees welding or other thermal exposure that could promote carbide precipitation. It does not eliminate the need to assess the final thermal history, specified corrosion testing and actual medium.
Does a 304L face make the plate suitable for seawater?
No general seawater guarantee follows from the grade. Chloride concentration, temperature, oxygen conditions, crevices and cleaning cycles matter. The process engineer must select the corrosion barrier; 316L or a higher alloy may still be insufficient in demanding service.
Is this an A516 plate with paint or a loose stainless liner?
Neither. It is a metallurgically bonded A264 product with a separately specified 304L layer. Painting, electroplating and mechanically retained sheet linings do not have the same product definition or bond-test requirements.
What is the chemical difference between ASTM 304L and the GB S30403 example?
The A240/A240M-25a 304L table here specifies 18.0–20.0% chromium. The separate GB/T 4237-2015 S30403 example uses its own 17.50–19.50% range and proof-strength requirement. A shared cross-reference code is not permission to exchange certificates.
Can I count the 304L facing as pressure-retaining wall thickness?
Only if the governing construction code and approved design allow it, with the associated manufacturing and welding requirements. For a corrosion-only face, define the backing-only strength basis rather than adding the two layers indiscriminately.
How is the carbon steel protected at a cut nozzle opening?
The plate edge exposes both constituent materials. The fabricator must detail any stainless weld restoration or other corrosion-side treatment so that process fluid does not bypass the selected barrier. A factory bond examination does not qualify that local fabrication detail.
What changes if I order an explosion-bonded rather than hot-rolled 304L plate?
The agreed route changes the manufacturing sequence and may change how the constituent heat treatments are combined. Both routes must still produce the ordered layer chemistry, final-condition properties and accepted bond; the process name alone is not a quality class.
Is 304L clad plate stocked for immediate shipment?
No blanket stock or dispatch interval is represented here. Gangsteel confirms the programme after reviewing plate area, base/facing thickness, quantity, thermal condition and the required witnessed tests. Give the minimum remaining stainless thickness rather than total gage alone.
Related Materials
ASTM A264 standard overview; Clad Steel Plate combinations; pressure-vessel backing steels.