Clad Steel Plate
ASTM A264 Stainless Clad Steel Plate: 304L and 316L
ASTM A264 covers carbon steel or low-alloy steel plate integrally and continuously bonded on one or both sides to stainless chromium-nickel steel facing, including the specified austenitic or duplex grades covered by its material provisions. Gangsteel treats the backing, facing and metallurgical bond as three separate parts of a clad-plate enquiry, so that corrosion selection is not confused with pressure-retaining strength.

Scope, Grade Structure and Edition Basis
The clad-standard scope follows ASTM's A264-12(2026) listing. The clause-level manufacturing and test discussion uses the accessible A264-12(2019) text; the purchase order must name the contractual edition. Component data below identify their own editions and are not a claim of automatic ASME certification.
304L and 316L are common austenitic choices, but A264 is not a single grade and does not mean that every plate has 316L corrosion performance. Its 2019 material provisions also address duplex stainless. Grade, UNS, component product specification and thermal condition must remain explicit. Chromium-only Type 410 facing belongs under A263; a nickel-base alloy facing belongs under A265.
| Order element | What must be named | Example, not a unique standard grade |
|---|---|---|
| Backing steel | Standard, edition, grade and delivery condition | A516/A516M-25 Grade 70 [485] |
| Corrosion-resistant facing | Alloy designation and component product standard | 304L / S30403 to ASTM A240/A240M-25a |
| Bonded product | Clad specification, edition and required bond examination | ASTM A264 with contractual edition and test plan |
| Geometry | Backing + minimum facing thickness; size and clad face count | Specified on the drawing; not inferred from alloy name |
Chemical Composition: Keep the Layers Separate
There is no single chemical-composition row for every A264 plate. The following defined material pair is an engineering example, not a new composite grade and not a substitute for the ordered layer certificates.
| Backing thickness | C max | Mn | Si | P max | S max |
|---|---|---|---|---|---|
| ≤12.5 mm | 0.27 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >12.5–50 mm | 0.28 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >50–100 mm | 0.30 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >100 mm | 0.31 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
Thickness in this table is the backing-steel thickness, not the sum of the layers. For each 0.01 percentage-point reduction below the specified carbon maximum, A516/A516M-25 permits a 0.06 percentage-point increase above the manganese maximum, up to 1.50% on heat analysis and 1.60% on product analysis. Product-analysis manganese and silicon ranges differ from heat analysis; compare the correct certificate column. Special supplementary chemistry provisions must be stated in the order.
| Element | Requirement |
|---|---|
| C | ≤0.030 |
| Mn | ≤2.00 |
| Si | ≤0.75 |
| P | ≤0.045 |
| S | ≤0.030 |
| Cr | 18.0–20.0 |
| Ni | 8.0–12.0 |
| N | ≤0.10 |
| Fe | Balance |
Mechanical Properties and the Bond Interface
| Layer / reference | Applicable reference condition | Yield / Rp0.2 min, MPa | Tensile, MPa | Elongation min |
|---|---|---|---|---|
| A516/A516M-25 Grade 70 [485] backing | All qualified plate thicknesses; no fixed maximum thickness in A516 | 260 | 485–620 | 21% in 50 mm; 17% in 200 mm; A20 adjustments apply |
| 304L S30403 facing; ASTM A240/A240M-25a | Annealed flat product | 170 | 485 min | 40% in 50 mm |
The cladding row describes the separately specified flat-product reference condition. It is not a requirement to extract a tiny tensile coupon from every finished facing. Finished clad-plate tensile acceptance follows the clad specification and the selected test section. Do not add the two tensile strengths or substitute bond shear strength for backing tensile strength. Cladding strength can enter vessel calculations only when the construction code and design permit it.
| Item | Condition / parameter | Meaning for the order |
|---|---|---|
| Composite tension section | Total gage ≤1.5 in. (about 38 mm), backing specified minimum tensile ≤70 ksi (485 MPa), and backing specified minimum yield ≤40 ksi (275 MPa) | All three conditions apply. Composite tensile maximum may be up to 5 ksi (35 MPa) above the backing specification maximum. |
| Backing-only tension section | Any of the three limits is exceeded | Backing tensile requirements apply without the composite upper allowance. |
| Corrosion-only cladding | Cladding is for corrosion allowance only | The cladding need not be included in the tensile test; backing requirements then govern. State the design basis. |
| Specified interface shear test | 20 ksi (140 MPa) minimum when required by purchaser | A bond-interface shear criterion; never the tensile strength of the backing or finished vessel. |
| Shear coupon feasibility | The standard identifies 0.075 in. (1.9 mm) cladding; testing at or below this thickness needs purchaser/manufacturer agreement | Specify minimum facing thickness and the test method together. |
| Alternative bond bend test | Use the alternative procedure when specified/agreed under the standard | A separate bond assessment, not a calculation from a tensile table. |
The inch-pound requirements are controlling in these ASTM clad standards; parenthesized metric figures are conversions. Plate tensile tests, bond tests and ultrasonic bond-integrity examination answer different questions. One successful shear coupon does not prove the entire plate area is bonded.
Bonding Process, Delivery and Heat Treatment
Explosion bonding joins prepared metal surfaces by a controlled high-velocity collision. Hot-roll bonding establishes the metallurgical bond during rolling of a prepared assembly; explosion bonding followed by rolling is a separate combined route. These are integrally bonded plates, not loose liners, adhesive laminates or chromium-carbide weld-overlay wear plates.
For austenitic stainless facing, A264-12(2019) describes heat treatment for carbide solution followed by individual air cooling unless otherwise specified or agreed. For plate made without hot rolling, components may be treated separately before bonding. Duplex stainless requires an agreed heat-treated condition; it is not covered by an assumed austenitic cycle.
| Parameter | Required order definition | Technical note |
|---|---|---|
| Bonding route | Explosion bonded, hot-roll bonded, or combined route | Route capability depends on the material pair, area, layer ratio and final condition. No blanket stock range is implied. |
| Thickness | Backing thickness + minimum facing thickness, in mm; identify one or two clad faces | Reserve facing allowance for grinding, forming and weld restoration. Total thickness alone is insufficient. |
| Final thermal condition | Named delivery condition and any simulated fabrication/PWHT cycle | Test in the representative final condition; agree number and duration of simulated cycles where required. |
| Heat-treatment temperature / hold | Qualified procedure for the selected pair and thickness | No single temperature, hold time or cooling rate is specified here for all clad plates. |
| Surface and cutting | As agreed: pickled, ground or specified finish; edge machining and protection | Prevent carbon-steel contamination of the corrosion-resistant face. |
| Lead time | Confirmed against the enquiry and agreed inspection plan | Not a fixed number of days for every thickness or bonding route. |
For an A516 backing, A516/A516M-25 normally requires normalization above 1.5 in. [40 mm]; thinner plate may be normalized when ordered. That backing rule does not authorize a final composite furnace cycle without checking the facing and clad-standard requirements. The two standards use different rounded metric values for 1.5 in.; do not substitute the 40 mm heat-treatment boundary for the clad-standard tensile boundary.
Inspection and Certification
Gangsteel separates incoming-material traceability, finished-plate mechanical qualification and bond-area examination in the inspection plan. Keep the backing heat number, facing heat/lot, plate identity and final thermal history linked through cutting. State the examination stage, coverage and acceptance class before manufacture; a certificate description such as "UT tested" without a method and class is incomplete.
| Check | What to specify | Acceptance concern |
|---|---|---|
| Chemistry and identity | Backing and facing specifications; heat analysis and product analysis if ordered | Do not report an averaged composite chemistry as either layer. |
| Tensile testing | Composite or backing-only section under the governing clad standard | State specimen section, direction and final test condition. |
| Bond examination | Ultrasonic method, acceptance class, coverage and edge/cut-zone requirements | Map reportable unbonded areas; distinguish scanning coverage from bonded-area percentage. |
| Bond mechanical test | Shear or alternative bend route where applicable | Record specimen location and criterion; do not relabel shear as tensile. |
| Forming / corrosion tests | Required bends, intergranular corrosion or project-specific tests by agreement | A low-carbon designation does not replace a specified corrosion test. |
| Additional service tests | Backing impact, HIC/SSC and simulated PWHT only when required by specification/code/order | No automatic sour-service, low-temperature or hydrogen-service qualification. |
| Documentation | Layer certificates, test reports, UT map, thermal records and agreed inspection release | An inspection certificate does not itself approve the vessel design. |
Frequently Asked Questions
Does A264 include duplex stainless or only 304L and 316L?
Its 2019 material provisions explicitly address duplex stainless and require an agreed heat-treated condition for duplex clad plate. The actual duplex grade and its thermal requirements must be named; they cannot be inferred from a general A264 label.
Is 304L automatically equivalent to the Chinese S30403 plate specification?
No. The common UNS designation and the GB unified code do not erase differences in product standards, chemistry limits and proof-strength requirements. State the actual standard and edition for the supplied facing instead of substituting a cross-reference name.
Can an A264 purchase order say only stainless clad with no facing grade?
That is not a complete technical definition. 304L, 316L and the duplex alternatives have different chemistry and thermal requirements. Specify the exact grade/UNS and product-standard edition so that the intended corrosion barrier is traceable.
Is the austenitic heat-treatment discussion also a duplex heat-treatment recipe?
No. The cited A264 text addresses duplex separately through an agreed heat-treated condition. The manufacturer and purchaser must establish a suitable final condition rather than copying an austenitic solution-treatment statement to a duplex product.
Is the 140 MPa figure a required tensile strength for every A264 plate?
It is neither a tensile property nor an unconditional test on every order. The cited clause gives the interface shear minimum when the purchaser requires that test. The backing, facing and composite-section tensile requirements remain separate.
May the stainless face be removed from the A264 tensile specimen?
For cladding used as corrosion allowance only, the cited provision allows it not to be included, with the backing requirements then governing. State that design/test basis explicitly; do not describe the result as an isolated facing tensile test.
How should an A264 order address stainless sheet seams used before explosion bonding?
The standard permits a fabricated facing component made from separately welded alloy sheets for explosively bonded products, subject to its requirements. If the construction code, design-strength credit or project specification restricts such seams, communicate those restrictions before manufacture.
Which enquiry details determine an A264 delivery commitment?
State the backing grade, 304L/316L or exact other facing, editions, layer thicknesses, clad sides, finish, total usable area, quantity, thermal condition and inspection class. Corrosion tests and witness points also affect production. Gangsteel confirms lead time against those requirements.
Related Clad Plate Selection
See the defined A516 Grade 70 + 304L combination; Clad Steel Plate range; pressure-vessel steel plate.