Clad Steel Plate
A516 Grade 70 + 410 Stainless Clad Steel Plate
A516 Grade 70 + 410 Stainless Clad Steel Plate combines a carbon-manganese pressure-vessel backing with a chromium stainless facing. The backing is specified for strength; the Type 410 face is selected for the process environment and its compatible fabrication condition. Gangsteel builds the enquiry around separate backing and facing certificates, the finished bond and the actual fabrication requirements.

Material Pair and Engineering Use
This pairing is considered for process equipment where a chromium stainless wetted surface is appropriate and a solid stainless wall is unnecessary. It is not a universal substitute for 304L or 316L. The designer must assess the actual fluid, temperature and fabrication sequence rather than select the face solely by chromium percentage.
| Part | Designation | Role |
|---|---|---|
| Backing | ASTM A516/A516M-25 Grade 70 [485] | Pressure-retaining strength and structural wall thickness |
| Facing | ASTM A240/A240M-25a 410 (S41000) | Selected corrosion-resistant surface |
| Composite | ASTM A263; contractual edition stated in order | Bonded product, not two loosely assembled plates |
The clad-standard scope follows ASTM's A263-12(2026) listing. The clause-level manufacturing and test discussion uses the accessible A263-12(2019) text; the purchase order must name the contractual edition. Component data below identify their own editions and are not a claim of automatic ASME certification.
Backing Steel Chemical Composition
| Backing thickness | C max | Mn | Si | P max | S max |
|---|---|---|---|---|---|
| ≤12.5 mm | 0.27 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >12.5–50 mm | 0.28 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >50–100 mm | 0.30 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
| >100 mm | 0.31 | 0.85–1.20 | 0.15–0.40 | 0.025 | 0.025 |
Thickness in this table is the backing-steel thickness, not the sum of the layers. For each 0.01 percentage-point reduction below the specified carbon maximum, A516/A516M-25 permits a 0.06 percentage-point increase above the manganese maximum, up to 1.50% on heat analysis and 1.60% on product analysis. Product-analysis manganese and silicon ranges differ from heat analysis; compare the correct certificate column. Special supplementary chemistry provisions must be stated in the order.
Corrosion-Resistant Facing Chemical Composition
| Element | Requirement |
|---|---|
| C | 0.08–0.15 |
| Mn | ≤1.00 |
| Si | ≤1.00 |
| P | ≤0.040 |
| S | ≤0.030 |
| Cr | 11.5–13.5 |
| Ni | ≤0.75 |
| Fe | Balance |
Mechanical Properties: Backing, Facing and Bond
| Layer / reference | Applicable reference condition | Yield / Rp0.2 min, MPa | Tensile, MPa | Elongation min |
|---|---|---|---|---|
| A516/A516M-25 Grade 70 [485] backing | All qualified plate thicknesses; no fixed maximum thickness in A516 | 260 | 485–620 | 21% in 50 mm; 17% in 200 mm; A20 adjustments apply |
| 410 S41000 facing; ASTM A240/A240M-25a | Annealed flat product | 205 | 450 min | 20% in 50 mm |
The cladding row describes the separately specified flat-product reference condition. It is not a requirement to extract a tiny tensile coupon from every finished facing. Finished clad-plate tensile acceptance follows the clad specification and the selected test section. Do not add the two tensile strengths or substitute bond shear strength for backing tensile strength. Cladding strength can enter vessel calculations only when the construction code and design permit it.
| Test decision | Application to this material pair | Order action |
|---|---|---|
| Tensile section | The Grade 70 [485] backing minima, 485 MPa tensile and 260 MPa yield, satisfy the cited 485/275 MPa strength thresholds. Total gage still determines the applicable section. | At total gage up to 1.5 in. (about 38 mm), the composite section is the general route unless the corrosion-only provision is used. Above that gage use backing-only testing. |
| Backing-only option | When the facing is for corrosion allowance only, it need not be included in the tensile specimen. | Identify this basis and retain the backing tensile limits; a face-excluded test is not a test of the facing. |
| Required bond test | Where the purchaser specifies the interface shear route, the minimum is 20 ksi (140 MPa). | Specify the coupon requirement, facing thickness and any agreed thin-facing procedure; this is not 140 MPa plate tensile strength. |
| Area integrity | One mechanical bond specimen does not sample all of the 410 face. | Agree ultrasonic method, coverage, acceptance class and the treatment of areas that will become formed or welded edges. |
The ASTM clad specification uses inch-pound values as controlling requirements. The 0.075 in. (1.9 mm) shear-coupon facing provision and any agreed testing at or below that thickness must be considered before choosing a thin corrosion layer. The standard overview explains the general test hierarchy in more detail.
Fabrication Considerations for This Pair
Type 410 is hardenable. Bonding, forming, backing welds and any post-weld thermal cycle can change facing hardness and toughness. Agree the final condition, repair procedure and any required hardness checks; do not apply an austenitic-stainless solution cycle by habit.
Order the base and minimum finished facing thicknesses separately. There is no universal standard layer ratio for this pair. A drawing notation such as 20 + 3 mm means 20 mm backing plus 3 mm facing only if that order is explicitly stated; it is an illustration of notation, not a stock-size or capacity claim. Assess forming strain, cut-edge restoration and any local thinning before fixing the purchase allowance.
Bonding Process, Delivery and Heat Treatment
Explosion bonding joins prepared metal surfaces by a controlled high-velocity collision. Hot-roll bonding establishes the metallurgical bond during rolling of a prepared assembly; explosion bonding followed by rolling is a separate combined route. These are integrally bonded plates, not loose liners, adhesive laminates or chromium-carbide weld-overlay wear plates.
For chromium stainless facing, coordinate the heat-treated condition with the backing specification and the hardenability of the facing. The 2019 A263 text provides normalized, tempered, normalized-and-tempered or quenched-and-tempered conditions as permitted by the backing specification unless otherwise agreed. A furnace cycle suitable for one layer cannot simply be copied to the other.
| Parameter | Required order definition | Technical note |
|---|---|---|
| Bonding route | Explosion bonded, hot-roll bonded, or combined route | Route capability depends on the material pair, area, layer ratio and final condition. No blanket stock range is implied. |
| Thickness | Backing thickness + minimum facing thickness, in mm; identify one or two clad faces | Reserve facing allowance for grinding, forming and weld restoration. Total thickness alone is insufficient. |
| Final thermal condition | Named delivery condition and any simulated fabrication/PWHT cycle | Test in the representative final condition; agree number and duration of simulated cycles where required. |
| Heat-treatment temperature / hold | Qualified procedure for the selected pair and thickness | No single temperature, hold time or cooling rate is specified here for all clad plates. |
| Surface and cutting | As agreed: pickled, ground or specified finish; edge machining and protection | Prevent carbon-steel contamination of the corrosion-resistant face. |
| Lead time | Confirmed against the enquiry and agreed inspection plan | Not a fixed number of days for every thickness or bonding route. |
For an A516 backing, A516/A516M-25 normally requires normalization above 1.5 in. [40 mm]; thinner plate may be normalized when ordered. That backing rule does not authorize a final composite furnace cycle without checking the facing and clad-standard requirements. The two standards use different rounded metric values for 1.5 in.; do not substitute the 40 mm heat-treatment boundary for the clad-standard tensile boundary.
Inspection and Certification
Gangsteel separates incoming-material traceability, finished-plate mechanical qualification and bond-area examination in the inspection plan. Keep the backing heat number, facing heat/lot, plate identity and final thermal history linked through cutting. State the examination stage, coverage and acceptance class before manufacture; a certificate description such as "UT tested" without a method and class is incomplete.
| Check | What to specify | Acceptance concern |
|---|---|---|
| Chemistry and identity | Backing and facing specifications; heat analysis and product analysis if ordered | Do not report an averaged composite chemistry as either layer. |
| Tensile testing | Composite or backing-only section under the governing clad standard | State specimen section, direction and final test condition. |
| Bond examination | Ultrasonic method, acceptance class, coverage and edge/cut-zone requirements | Map reportable unbonded areas; distinguish scanning coverage from bonded-area percentage. |
| Bond mechanical test | Shear or alternative bend route where applicable | Record specimen location and criterion; do not relabel shear as tensile. |
| Forming / corrosion tests | Required bends, intergranular corrosion or project-specific tests by agreement | A low-carbon designation does not replace a specified corrosion test. |
| Additional service tests | Backing impact, HIC/SSC and simulated PWHT only when required by specification/code/order | No automatic sour-service, low-temperature or hydrogen-service qualification. |
| Documentation | Layer certificates, test reports, UT map, thermal records and agreed inspection release | An inspection certificate does not itself approve the vessel design. |
Frequently Asked Questions
Can 410S be supplied instead of 410 without changing the order?
No. Type 410S is a different lower-carbon chromium stainless grade with different metallurgical behavior. It may be useful for a clad application, but substitution requires explicit design and purchasing approval and the correct certificate designation.
Will the 410 surface be delivered in a hardened condition?
Not automatically. The flat-product reference figures shown here describe the annealed condition. The composite delivery condition must be compatible with the backing specification, the specified facing and the fabrication route; a hardening treatment must not be inferred from the alloy name.
Why is this combination discussed under A263 rather than A264?
The distinction is the facing: Type 410 is chromium stainless, whereas A264 addresses chromium-nickel stainless facing. A common A516 backing does not make the finished clad specifications interchangeable.
Can the facing be treated like a nonhardenable 304L sheet during fabrication?
No. Type 410 hardenability makes welding and thermal history important to local hardness and ductility. The engineer should define the final facing condition and any hardness or cracking-control requirements for the actual fabrication procedure.
Does the 450 MPa reference number describe the A516 backing?
No. It is the A240 Type 410 annealed flat-product tensile minimum. The Grade 70 backing has its own 485–620 MPa reference range, and the finished-clad test uses the specimen rules of the ordered A263 edition.
Does magnetic response prove that the correct 410 facing was supplied?
No. Magnetic response is not sufficient material identification or evidence of a conforming heat. Retain the facing certificate and any ordered positive material identification; also distinguish the specified 410 grade from another chromium stainless grade.
May a fabricator use an austenitic-stainless PWHT recipe on this plate?
Not simply because it is stainless clad. The backing specification, 410 condition, bond integrity and construction-code obligations must be considered together. Any simulated thermal testing should represent the agreed fabrication cycle, not a generic stainless recipe.
How should I request a firm offer for 410 clad plate?
Name A263 and its edition, the precise facing designation, backing grade, layer thicknesses, final condition, dimensions and examination plan. Identify any 410S substitution proposal as a separate technical decision. Delivery is confirmed against the accepted enquiry.
Related Materials
ASTM A263 standard overview; Clad Steel Plate combinations; pressure-vessel backing steels.