ASTM A263 covers carbon steel or low-alloy steel plate integrally and continuously bonded on one or both sides to stainless chromium steel facing, including specified chromium stainless grades such as Type 410. Gangsteel treats the backing, facing and metallurgical bond as three separate parts of a clad-plate enquiry, so that corrosion selection is not confused with pressure-retaining strength.

ASTM A263 Stainless Chromium Clad Steel Plate - generated product illustration

Scope, Grade Structure and Edition Basis

The clad-standard scope follows ASTM's A263-12(2026) listing. The clause-level manufacturing and test discussion uses the accessible A263-12(2019) text; the purchase order must name the contractual edition. Component data below identify their own editions and are not a claim of automatic ASME certification.

The important boundary is the facing family: Type 410 is a chromium stainless grade, so an A516 Grade 70 plus 410 order belongs in the A263 discussion, not the A264 chromium-nickel group. It is also essential to distinguish 410 from low-carbon 410S; one designation must not silently replace the other.

A263 is a clad-product specification, not a fixed list of composite grades
Order element What must be named Example, not a unique standard grade
Backing steel Standard, edition, grade and delivery condition A516/A516M-25 Grade 70 [485]
Corrosion-resistant facing Alloy designation and component product standard 410 / S41000 to ASTM A240/A240M-25a
Bonded product Clad specification, edition and required bond examination ASTM A263 with contractual edition and test plan
Geometry Backing + minimum facing thickness; size and clad face count Specified on the drawing; not inferred from alloy name

Chemical Composition: Keep the Layers Separate

There is no single chemical-composition row for every A263 plate. The following defined material pair is an engineering example, not a new composite grade and not a substitute for the ordered layer certificates.

A516/A516M-25 Grade 70 [485] backing steel: selected heat-analysis requirements, mass %
Backing thickness C max Mn Si P max S max
≤12.5 mm 0.27 0.85–1.20 0.15–0.40 0.025 0.025
>12.5–50 mm 0.28 0.85–1.20 0.15–0.40 0.025 0.025
>50–100 mm 0.30 0.85–1.20 0.15–0.40 0.025 0.025
>100 mm 0.31 0.85–1.20 0.15–0.40 0.025 0.025

Thickness in this table is the backing-steel thickness, not the sum of the layers. For each 0.01 percentage-point reduction below the specified carbon maximum, A516/A516M-25 permits a 0.06 percentage-point increase above the manganese maximum, up to 1.50% on heat analysis and 1.60% on product analysis. Product-analysis manganese and silicon ranges differ from heat analysis; compare the correct certificate column. Special supplementary chemistry provisions must be stated in the order.

ASTM A240/A240M-25a 410 (S41000): cladding chemistry, mass %
Element Requirement
C 0.08–0.15
Mn ≤1.00
Si ≤1.00
P ≤0.040
S ≤0.030
Cr 11.5–13.5
Ni ≤0.75
Fe Balance

Mechanical Properties and the Bond Interface

Separate room-temperature constituent reference values; not a finished-composite guarantee
Layer / reference Applicable reference condition Yield / Rp0.2 min, MPa Tensile, MPa Elongation min
A516/A516M-25 Grade 70 [485] backing All qualified plate thicknesses; no fixed maximum thickness in A516 260 485–620 21% in 50 mm; 17% in 200 mm; A20 adjustments apply
410 S41000 facing; ASTM A240/A240M-25a Annealed flat product 205 450 min 20% in 50 mm

The cladding row describes the separately specified flat-product reference condition. It is not a requirement to extract a tiny tensile coupon from every finished facing. Finished clad-plate tensile acceptance follows the clad specification and the selected test section. Do not add the two tensile strengths or substitute bond shear strength for backing tensile strength. Cladding strength can enter vessel calculations only when the construction code and design permit it.

ASTM A263-12(2019): tensile section and bond-test planning
Item Condition / parameter Meaning for the order
Composite tension section Total gage ≤1.5 in. (about 38 mm), backing specified minimum tensile ≤70 ksi (485 MPa), and backing specified minimum yield ≤40 ksi (275 MPa) All three conditions apply. Composite tensile maximum may be up to 5 ksi (35 MPa) above the backing specification maximum.
Backing-only tension section Any of the three limits is exceeded Backing tensile requirements apply without the composite upper allowance.
Corrosion-only cladding Cladding is for corrosion allowance only The cladding need not be included in the tensile test; backing requirements then govern. State the design basis.
Specified interface shear test 20 ksi (140 MPa) minimum when required by purchaser A bond-interface shear criterion; never the tensile strength of the backing or finished vessel.
Shear coupon feasibility The standard identifies 0.075 in. (1.9 mm) cladding; testing at or below this thickness needs purchaser/manufacturer agreement Specify minimum facing thickness and the test method together.
Alternative bond bend test Use the alternative procedure when specified/agreed under the standard A separate bond assessment, not a calculation from a tensile table.

The inch-pound requirements are controlling in these ASTM clad standards; parenthesized metric figures are conversions. Plate tensile tests, bond tests and ultrasonic bond-integrity examination answer different questions. One successful shear coupon does not prove the entire plate area is bonded.

Bonding Process, Delivery and Heat Treatment

Explosion bonding joins prepared metal surfaces by a controlled high-velocity collision. Hot-roll bonding establishes the metallurgical bond during rolling of a prepared assembly; explosion bonding followed by rolling is a separate combined route. These are integrally bonded plates, not loose liners, adhesive laminates or chromium-carbide weld-overlay wear plates.

For chromium stainless facing, coordinate the heat-treated condition with the backing specification and the hardenability of the facing. The 2019 A263 text provides normalized, tempered, normalized-and-tempered or quenched-and-tempered conditions as permitted by the backing specification unless otherwise agreed. A furnace cycle suitable for one layer cannot simply be copied to the other.

Manufacturing and delivery parameters to put on the enquiry
Parameter Required order definition Technical note
Bonding route Explosion bonded, hot-roll bonded, or combined route Route capability depends on the material pair, area, layer ratio and final condition. No blanket stock range is implied.
Thickness Backing thickness + minimum facing thickness, in mm; identify one or two clad faces Reserve facing allowance for grinding, forming and weld restoration. Total thickness alone is insufficient.
Final thermal condition Named delivery condition and any simulated fabrication/PWHT cycle Test in the representative final condition; agree number and duration of simulated cycles where required.
Heat-treatment temperature / hold Qualified procedure for the selected pair and thickness No single temperature, hold time or cooling rate is specified here for all clad plates.
Surface and cutting As agreed: pickled, ground or specified finish; edge machining and protection Prevent carbon-steel contamination of the corrosion-resistant face.
Lead time Confirmed against the enquiry and agreed inspection plan Not a fixed number of days for every thickness or bonding route.

For an A516 backing, A516/A516M-25 normally requires normalization above 1.5 in. [40 mm]; thinner plate may be normalized when ordered. That backing rule does not authorize a final composite furnace cycle without checking the facing and clad-standard requirements. The two standards use different rounded metric values for 1.5 in.; do not substitute the 40 mm heat-treatment boundary for the clad-standard tensile boundary.

Inspection and Certification

Gangsteel separates incoming-material traceability, finished-plate mechanical qualification and bond-area examination in the inspection plan. Keep the backing heat number, facing heat/lot, plate identity and final thermal history linked through cutting. State the examination stage, coverage and acceptance class before manufacture; a certificate description such as "UT tested" without a method and class is incomplete.

Inspection plan for the finished clad plate
Check What to specify Acceptance concern
Chemistry and identity Backing and facing specifications; heat analysis and product analysis if ordered Do not report an averaged composite chemistry as either layer.
Tensile testing Composite or backing-only section under the governing clad standard State specimen section, direction and final test condition.
Bond examination Ultrasonic method, acceptance class, coverage and edge/cut-zone requirements Map reportable unbonded areas; distinguish scanning coverage from bonded-area percentage.
Bond mechanical test Shear or alternative bend route where applicable Record specimen location and criterion; do not relabel shear as tensile.
Forming / corrosion tests Required bends, intergranular corrosion or project-specific tests by agreement A low-carbon designation does not replace a specified corrosion test.
Additional service tests Backing impact, HIC/SSC and simulated PWHT only when required by specification/code/order No automatic sour-service, low-temperature or hydrogen-service qualification.
Documentation Layer certificates, test reports, UT map, thermal records and agreed inspection release An inspection certificate does not itself approve the vessel design.

Frequently Asked Questions

Does A263 cover 304L or 316L stainless facing?

No. Chromium-nickel stainless facing belongs under the A264 scope. A263 addresses chromium stainless facing; a Type 410 order should not be relabelled A264 simply because the base steel is the same.

Can every chromium stainless face use one heat treatment?

No. Grade hardenability, backing requirements and intended fabrication determine the compatible condition. A Type 410 delivery should not be treated as though it were nonhardenable austenitic stainless.

Does A263 itself define a grade called A516-410?

No. The purchaser selects the backing specification and the chromium stainless facing under the clad standard material provisions. A516 Grade 70 plus 410 is a defined material pair, not a new standalone A263 steel grade.

Does specifying A263 force one particular bonding process?

The standard permits a metallurgical bonding method that produces a conforming product. Explosion bonding, rolling or a combined route must be reviewed against the actual thicknesses and delivery condition; none is an automatic synonym for A263 quality.

What is the purpose of the 20 ksi interface test in an A263 enquiry?

When the purchaser requires the shear route, the cited 2019 minimum is 20 ksi, conventionally shown as 140 MPa. It assesses the chromium stainless/steel interface locally; it is not the backing tensile strength and does not define a vessel pressure rating.

Why do chromium-clad tensile specimen rules use both gage and backing strength?

A263 distinguishes the relatively thin, lower-strength composite test route from conditions requiring backing-only testing. All cited gage and strength conditions must be evaluated together. A corrosion-only facing can be excluded as provided by the standard.

Can one successful bond specimen replace an area examination of the chromium face?

No. A specimen tests one location, while an agreed ultrasonic examination checks the plate area under a stated acceptance class. The two reports provide different evidence; the project should identify any critical forming or cut-edge zones.

What does Gangsteel need to schedule a chromium stainless clad order?

Provide the backing standard and edition, exact chromium stainless grade, A263 edition, layer gages, usable dimensions, final heat treatment, bond requirements and any repair restrictions. Identify fabrication thermal cycles early. Lead time follows the accepted enquiry, not a blanket stock promise.

Related Clad Plate Selection

See the defined A516 Grade 70 + 410 combination; Clad Steel Plate range; pressure-vessel steel plate.

Other Products