A516 Grade 70 + Alloy 625 clad steel plate bonds a nickel-chromium-molybdenum-niobium alloy (UNS N06625) to a carbon steel pressure backing. Gangsteel supplies it to ASTM A265 for sour-gas, flue-gas and severe chemical service.

A516 Grade 70 + Alloy 625 N06625 Clad Steel Plate - generated product illustration

Material Pair and Engineering Use

Alloy 625 has about 20–23% chromium, 8–10% molybdenum and 3.15–4.15% niobium plus tantalum in a nickel matrix. It resists pitting, crevice corrosion and chloride stress-corrosion cracking far better than stainless steels. Clad plate is used for separators, absorbers and scrubbers where a solid nickel-alloy wall would be very costly.

Material identity and specification basis
Part Designation Role
Backing ASTM A516/A516M-25 Grade 70 (Grade 60 by order) Carries pressure and structural load
Cladding ASTM B443 UNS N06625, Grade 1 (annealed) or Grade 2 (solution annealed) Nickel-alloy corrosion face
Clad product ASTM A265 (A265-12(2026) scope; clauses from 12(2019)) Bond, tests and tolerances

Backing Steel Chemical Composition

A516/A516M-25 Grade 70 [485] backing steel: selected heat-analysis requirements, mass %
Backing thickness C max Mn Si P max S max
≤12.5 mm 0.27 0.85–1.20 0.15–0.40 0.025 0.025
>12.5–50 mm 0.28 0.85–1.20 0.15–0.40 0.025 0.025
>50–100 mm 0.30 0.85–1.20 0.15–0.40 0.025 0.025
>100 mm 0.31 0.85–1.20 0.15–0.40 0.025 0.025

The thickness column refers to the steel backing alone. A516/A516M-25 allows 0.06 percentage point more manganese for each 0.01 point of carbon below the maximum, capped at 1.50% (heat) and 1.60% (product). Where Grade 60 backing is ordered instead, its lower carbon maxima and its own 415–550 MPa tensile range apply; the two grades must not be mixed on one certificate.

Cladding Chemical Composition

ASTM B443-19 UNS N06625 cladding chemistry
Element Requirement, mass %
Ni ≥58.0 (by difference)
Cr 20.0–23.0
Mo 8.0–10.0
Nb+Ta 3.15–4.15
Fe ≤5.0
C ≤0.10
Mn ≤0.50
Si ≤0.50
P ≤0.015
S ≤0.015
Al ≤0.40
Ti ≤0.40
Co (if determined) ≤1.0

B443 furnishes N06625 as Grade 1, annealed, normally for service up to 1100°F (593°C), or Grade 2, solution annealed, for higher-temperature creep service. The ordered grade must appear on the facing certificate.

Mechanical Properties of the Layers and the Bond

Constituent room-temperature reference values (separate layers, not a composite guarantee)
Layer / reference Condition Yield / Rp0.2 min, MPa Tensile, MPa Elongation min
A516/A516M-25 Grade 70 [485] backing Plate as ordered; normalized above 1.5 in. [40 mm] 260 485–620 21% in 50 mm; 17% in 200 mm
N06625 Grade 1, B443-19 Annealed hot-rolled plate to 2.75 in. (70 mm) 379 758 min 30%
N06625 Grade 2, B443-19 Solution annealed plate 276 690 min 30%

The facing row is the annealed flat-product reference of its own specification. It is not added to the backing strength, and bond shear is not a substitute for backing tensile strength. Cladding strength counts in design only where the construction code allows it.

Finished-plate acceptance under ASTM A265-12(2019) clauses
Item Requirement or condition Order meaning
Tensile section Grade 70 backing minima (485 MPa tensile, 260 MPa yield) fall within the 70 ksi / 40 ksi limits; total gage then decides Up to 1.5 in. (about 38 mm) total gage, test the composite section unless the facing is declared corrosion allowance only; above that gage, test the backing alone.
Composite tensile ceiling Up to 5 ksi (35 MPa) above the backing maximum Applies only to the composite-section route; it is not a design strength.
Interface shear (when specified) 20 ksi (140 MPa) minimum Bond property only. Below or at 0.075 in. (1.9 mm) facing, shear testing needs agreement; three bond bend tests are the alternative route.
Bond area Ultrasonic method, coverage and acceptance class agreed on the order One shear coupon does not show that the whole Alloy 625 face is bonded.

Inch-pound values govern in the ASTM clad specifications; metric figures are conversions. The scope of A265 is confirmed against the A265-12(2026) listing, while the clause wording above was read from the 12(2019) text, so the purchase order should name the edition it invokes.

Fabrication Points for This Pair

Seams are restored with a qualified nickel-base filler such as an ERNiCrMo-3 type over the carbon steel, with dilution controlled so that iron does not weaken the corrosion-resistant cap.

Nickel alloys are sensitive to sulfur and lead contamination before heating; clean the face before any thermal operation and keep marking materials off it.

Bonding Process, Delivery and Heat Treatment

A265-12(2019) calls for a condition appropriate to the cladding alloy, the backing or both unless the component specifications or the order require a specific treatment. For 625 this means agreeing whether the face is supplied in the Grade 1 or Grade 2 condition and confirming that the backing still meets A516 after any cycle.

Manufacturing and delivery parameters for the enquiry
Parameter Order definition Engineering note
Bonding route Explosion bonded or hot-roll bonded Explosion bonding is common for thick 625 faces
Layer thickness Backing gage plus minimum facing gage in mm; single- or double-sided Allow facing margin for grinding, forming and weld restoration; total gage alone does not define the plate.
Final thermal condition Named final condition, plus any simulated PWHT Represent vessel PWHT on coupons
Surface and edges Pickled or as agreed Face kept free of sulfur- or lead-bearing contaminants
Lead time Confirmed against the enquiry Depends on plate area, layer gages, quantity, thermal condition and witnessed inspection.

Inspection and Certification

For Alloy 625 clad plate the plan confirms the B443 grade and chemistry of the face, the A265 tensile and bond tests and any sour-service tests the project names.

Inspection and test documents for the finished plate
Check What to specify Why it matters
Layer identity Separate backing and facing certificates with heat numbers No blended composite analysis
B443 grade Grade 1 or Grade 2 stated on certificate Different heat-treated conditions
Sour-service tests HIC or SSC testing of the backing, only if specified Not implied by the 625 face
Bond tests Shear or bond bend; ultrasonic acceptance level Interface and area
Tensile Composite or backing-only per A265 Section declared on report

Frequently Asked Questions

Why is Alloy 625 used for clad sour-gas vessels?

Its high chromium, molybdenum and niobium content gives strong resistance to pitting, crevice corrosion and chloride stress-corrosion cracking in wet sour and chloride service.

Should the 625 face be Grade 1 or Grade 2?

B443 Grade 1 (annealed) is normally used up to 1100°F (593°C). Grade 2 (solution annealed) is for higher temperatures where creep resistance is needed. Most corrosion-service clad plate uses Grade 1.

Does 625 cladding make the backing sour-service qualified?

No. HIC and other backing tests must be ordered for the A516 plate separately.

Is Alloy 625 cladding made by weld overlay or bonding?

Both exist. This product is a bonded plate under A265; weld overlay is a different fabrication route.

What filler is used at the seams?

The welding procedure selects a nickel-base filler compatible with 625, with dilution controlled at the cap.

How is nickel reported on the 625 certificate?

B443 determines nickel arithmetically by difference, with a minimum of 58.0%.

Is the composite tensile test used for A516-70 + 625?

At total gage up to 1.5 in. (about 38 mm) A265 uses the composite section for this backing, unless the facing is corrosion allowance only.

What should an Alloy 625 clad enquiry include?

A265 edition, B443 grade, backing grade and thickness, minimum 625 thickness, size, quantity, final condition, PWHT, bond, ultrasonic and sour-service tests. Lead time is confirmed against the enquiry.

Related Materials

ASTM A265 nickel-alloy clad plate; A516 Grade 70 + Alloy C276 clad plate; all clad steel plate combinations.