A516 Grade 70 + Alloy 825 clad steel plate bonds a nickel-iron-chromium alloy with molybdenum, copper and titanium (UNS N08825) to a carbon steel pressure backing. Gangsteel supplies it to ASTM A265 for sour oil and gas and acid process equipment.

A516 Grade 70 + Alloy 825 N08825 Clad Steel Plate - generated product illustration

Material Pair and Engineering Use

Alloy 825 contains 38–46% nickel, 19.5–23.5% chromium, 2.5–3.5% molybdenum and 1.5–3% copper. The nickel gives resistance to chloride stress-corrosion cracking, and the copper and molybdenum help in sulfuric and phosphoric acids. Clad plate is common for separators and pressure vessels in sour service.

Material identity and specification basis
Part Designation Role
Backing ASTM A516/A516M-25 Grade 70 (Grade 60 by order) Carries pressure and structural load
Cladding ASTM B424 UNS N08825 Nickel-iron-chromium face
Clad product ASTM A265 (A265-12(2026) scope; clauses from 12(2019)) Bond, tests and tolerances

Backing Steel Chemical Composition

A516/A516M-25 Grade 70 [485] backing steel: selected heat-analysis requirements, mass %
Backing thickness C max Mn Si P max S max
≤12.5 mm 0.27 0.85–1.20 0.15–0.40 0.025 0.025
>12.5–50 mm 0.28 0.85–1.20 0.15–0.40 0.025 0.025
>50–100 mm 0.30 0.85–1.20 0.15–0.40 0.025 0.025
>100 mm 0.31 0.85–1.20 0.15–0.40 0.025 0.025

The thickness column refers to the steel backing alone. A516/A516M-25 allows 0.06 percentage point more manganese for each 0.01 point of carbon below the maximum, capped at 1.50% (heat) and 1.60% (product). Where Grade 60 backing is ordered instead, its lower carbon maxima and its own 415–550 MPa tensile range apply; the two grades must not be mixed on one certificate.

Cladding Chemical Composition

ASTM B424 UNS N08825 cladding chemistry (values read from the B424-11 text)
Element Requirement, mass %
Ni 38.0–46.0
Cr 19.5–23.5
Fe ≥22.0 (by difference)
Mo 2.5–3.5
Cu 1.5–3.0
Ti 0.6–1.2
C ≤0.05
Mn ≤1.0
Si ≤0.5
S ≤0.03
Al ≤0.2

B424-19 still covers N08825; the table values were read from the B424-11 text. The purchase order should name the B424 edition that applies.

Mechanical Properties of the Layers and the Bond

Constituent room-temperature reference values (separate layers, not a composite guarantee)
Layer / reference Condition Yield / Rp0.2 min, MPa Tensile, MPa Elongation min
A516/A516M-25 Grade 70 [485] backing Plate as ordered; normalized above 1.5 in. [40 mm] 260 485–620 21% in 50 mm; 17% in 200 mm
N08825 facing, B424 (B424-11 text) Annealed hot-rolled plate 241 586 min 30%

The facing row is the annealed flat-product reference of its own specification. It is not added to the backing strength, and bond shear is not a substitute for backing tensile strength. Cladding strength counts in design only where the construction code allows it.

Finished-plate acceptance under ASTM A265-12(2019) clauses
Item Requirement or condition Order meaning
Tensile section Grade 70 backing minima (485 MPa tensile, 260 MPa yield) fall within the 70 ksi / 40 ksi limits; total gage then decides Up to 1.5 in. (about 38 mm) total gage, test the composite section unless the facing is declared corrosion allowance only; above that gage, test the backing alone.
Composite tensile ceiling Up to 5 ksi (35 MPa) above the backing maximum Applies only to the composite-section route; it is not a design strength.
Interface shear (when specified) 20 ksi (140 MPa) minimum Bond property only. Below or at 0.075 in. (1.9 mm) facing, shear testing needs agreement; three bond bend tests are the alternative route.
Bond area Ultrasonic method, coverage and acceptance class agreed on the order One shear coupon does not show that the whole Alloy 825 face is bonded.

Inch-pound values govern in the ASTM clad specifications; metric figures are conversions. The scope of A265 is confirmed against the A265-12(2026) listing, while the clause wording above was read from the 12(2019) text, so the purchase order should name the edition it invokes.

Fabrication Points for This Pair

Restore the corrosion face at seams with a qualified nickel-base filler; a higher-alloy filler is often used for the cap to compensate for dilution.

Keep the face free of sulfur and iron contamination and protect it during forming and transport.

Bonding Process, Delivery and Heat Treatment

A265-12(2019) calls for a condition suited to the cladding and/or backing. Alloy 825 is supplied annealed; titanium in the alloy stabilizes it against sensitization. Any furnace cycle after bonding is agreed so that the A516 backing and the bond remain within requirements.

Manufacturing and delivery parameters for the enquiry
Parameter Order definition Engineering note
Bonding route Explosion bonded or hot-roll bonded Both are used for 825 on pressure-vessel steel
Layer thickness Backing gage plus minimum facing gage in mm; single- or double-sided Allow facing margin for grinding, forming and weld restoration; total gage alone does not define the plate.
Final thermal condition Named final condition and any simulated PWHT Represent vessel PWHT on coupons
Surface and edges Pickled or as agreed Face protected
Lead time Confirmed against the enquiry Depends on plate area, layer gages, quantity, thermal condition and witnessed inspection.

Inspection and Certification

The 825 clad plan confirms the face chemistry, the A265 bond and tensile tests and any sour-service backing tests ordered.

Inspection and test documents for the finished plate
Check What to specify Why it matters
Layer identity Separate backing and facing certificates with heat numbers No blended composite analysis
Ti and Cu check Facing heat analysis against B424 ranges Stabilization and acid resistance
Sour-service tests HIC or SSC tests of the backing, if specified Not implied by the face
Bond tests Shear or bond bend; ultrasonic acceptance level Interface and area
Tensile Composite or backing-only per A265 Section declared on report

Frequently Asked Questions

Why is Alloy 825 used instead of 316L for clad separators?

The much higher nickel content gives resistance to chloride stress-corrosion cracking, and molybdenum and copper improve acid resistance.

How does Alloy 825 differ from Alloy 625?

825 is a nickel-iron-chromium alloy with lower molybdenum and added copper; 625 is a nickel-base alloy with high molybdenum and niobium. 625 handles more severe pitting conditions.

Is iron reported directly on the 825 certificate?

B424 determines iron arithmetically by difference, with a minimum of 22.0%.

Does the 825 face need solution treatment after bonding?

A265 requires a condition suitable for the alloy and backing. The actual cycle is agreed and confirmed by tests in the final condition.

Is 825 clad plate suitable for sour service?

It is widely used in sour oil and gas service, but the backing needs its own HIC or SSC testing and the design must meet the project sour-service standard.

What is the minimum tensile strength of the 825 face?

The B424-11 text gives 586 MPa tensile, 241 MPa yield and 30% elongation for annealed hot-rolled plate. This is the alloy reference, not the design value of the clad plate.

Can the backing be Grade 60 instead of Grade 70?

Yes, if ordered. Grade 60 has a 415–550 MPa tensile range and its own carbon limits.

What information is needed to quote 825 clad plate?

A265 edition, B424 edition, backing grade and thickness, minimum 825 thickness, size, quantity, final condition, PWHT, bond, ultrasonic and sour-service tests. Lead time is confirmed against the enquiry.

Related Materials

ASTM A265 nickel-alloy clad plate; A516 Grade 70 + 904L clad plate; all clad steel plate combinations.

Other Products