A516 Grade 70 + 904L clad steel plate bonds high-alloy austenitic stainless (UNS N08904) to a carbon steel pressure backing. Gangsteel supplies it to ASTM A264 for sulfuric and phosphoric acid equipment and other aggressive process duty.

A516 Grade 70 + 904L Stainless Clad Steel Plate - generated product illustration

Material Pair and Engineering Use

904L carries 23–28% nickel, 4–5% molybdenum and 1–2% copper. The copper addition helps in sulfuric acid, and the high nickel and molybdenum improve resistance to pitting and stress-corrosion cracking compared with 316L. Clad plate lets the vessel wall use carbon steel for strength.

Material identity and specification basis
Part Designation Role
Backing ASTM A516/A516M-25 Grade 70 (Grade 60 by order) Carries pressure and structural load
Cladding ASTM A240/A240M-25a 904L (UNS N08904) High-alloy austenitic face
Clad product ASTM A264 (A264-12(2026) scope; clauses from 12(2019)) Bond, tests and tolerances

Backing Steel Chemical Composition

A516/A516M-25 Grade 70 [485] backing steel: selected heat-analysis requirements, mass %
Backing thickness C max Mn Si P max S max
≤12.5 mm 0.27 0.85–1.20 0.15–0.40 0.025 0.025
>12.5–50 mm 0.28 0.85–1.20 0.15–0.40 0.025 0.025
>50–100 mm 0.30 0.85–1.20 0.15–0.40 0.025 0.025
>100 mm 0.31 0.85–1.20 0.15–0.40 0.025 0.025

The thickness column refers to the steel backing alone. A516/A516M-25 allows 0.06 percentage point more manganese for each 0.01 point of carbon below the maximum, capped at 1.50% (heat) and 1.60% (product). Where Grade 60 backing is ordered instead, its lower carbon maxima and its own 415–550 MPa tensile range apply; the two grades must not be mixed on one certificate.

Cladding Chemical Composition

ASTM A240/A240M-25a 904L (N08904) cladding chemistry
Element Requirement, mass %
C ≤0.020
Mn ≤2.00
P ≤0.045
S ≤0.035
Si ≤1.00
Cr 19.0–23.0
Ni 23.0–28.0
Mo 4.00–5.00
N ≤0.10
Cu 1.00–2.00

904L carries a UNS N-number but is specified in A240 as a stainless steel plate grade, so it is handled as an A264 facing rather than an A265 nickel-alloy facing.

Mechanical Properties of the Layers and the Bond

Constituent room-temperature reference values (separate layers, not a composite guarantee)
Layer / reference Condition Yield / Rp0.2 min, MPa Tensile, MPa Elongation min
A516/A516M-25 Grade 70 [485] backing Plate as ordered; normalized above 1.5 in. [40 mm] 260 485–620 21% in 50 mm; 17% in 200 mm
904L facing, A240/A240M-25a Annealed plate 220 490 min 35% in 50 mm

The facing row is the annealed flat-product reference of its own specification. It is not added to the backing strength, and bond shear is not a substitute for backing tensile strength. Cladding strength counts in design only where the construction code allows it. A240 gives 90 HRBW maximum hardness for 904L.

Finished-plate acceptance under ASTM A264-12(2019) clauses
Item Requirement or condition Order meaning
Tensile section Grade 70 backing minima (485 MPa tensile, 260 MPa yield) fall within the 70 ksi / 40 ksi limits; total gage then decides Up to 1.5 in. (about 38 mm) total gage, test the composite section unless the facing is declared corrosion allowance only; above that gage, test the backing alone.
Composite tensile ceiling Up to 5 ksi (35 MPa) above the backing maximum Applies only to the composite-section route; it is not a design strength.
Interface shear (when specified) 20 ksi (140 MPa) minimum Bond property only. Below or at 0.075 in. (1.9 mm) facing, shear testing needs agreement; three bond bend tests are the alternative route.
Bond area Ultrasonic method, coverage and acceptance class agreed on the order One shear coupon does not show that the whole 904L face is bonded.

Inch-pound values govern in the ASTM clad specifications; metric figures are conversions. The scope of A264 is confirmed against the A264-12(2026) listing, while the clause wording above was read from the 12(2019) text, so the purchase order should name the edition it invokes.

Fabrication Points for This Pair

Fully austenitic 904L is prone to hot cracking, so restoration welds use low heat input and a qualified over-alloyed nickel-base or matching filler over a transition layer.

Because the face is expensive, specify cutting allowances and the minimum remaining 904L thickness after weld preparation and grinding.

Bonding Process, Delivery and Heat Treatment

Under A264-12(2019) the austenitic face is solution treated and individually air cooled unless otherwise agreed. Any combined furnace cycle has to suit both the 904L face and the A516 backing, which needs normalizing above 1.5 in. [40 mm].

Manufacturing and delivery parameters for the enquiry
Parameter Order definition Engineering note
Bonding route Explosion bonded or hot-roll bonded Explosion bonding is common for thick, high-alloy faces
Layer thickness Backing gage plus minimum facing gage in mm; single- or double-sided Allow facing margin for grinding, forming and weld restoration; total gage alone does not define the plate.
Final thermal condition Named final condition and any simulated PWHT Represent fabrication cycles on test coupons
Surface and edges Pickled or as agreed Protect the face from iron pickup
Lead time Confirmed against the enquiry Depends on plate area, layer gages, quantity, thermal condition and witnessed inspection.

Inspection and Certification

904L clad plate inspection follows the A264 test plan; corrosion testing is added only when the project specifies it.

Inspection and test documents for the finished plate
Check What to specify Why it matters
Layer identity Separate backing and facing certificates with heat numbers No blended composite analysis
Cu and Mo check Facing heat analysis against A240 ranges Confirms the acid-service alloy
Corrosion test Method and acceptance, if ordered Not automatic
Bond tests Shear or bond bend; ultrasonic acceptance level Interface and area
Tensile Composite or backing-only per A264 Section declared on report

Frequently Asked Questions

Why is 904L clad plate used in sulfuric acid service?

Its copper addition and high nickel content improve resistance to sulfuric acid compared with standard austenitic grades. Suitability depends on concentration, temperature and impurities.

Is 904L clad plate made to A264 or A265?

It is generally ordered under A264, because 904L is an A240 stainless grade. A265 is for nickel and nickel-base alloy faces.

How does 904L compare with Alloy 625 cladding?

Alloy 625 is a nickel-base alloy with far higher molybdenum and niobium and is used for more severe duties. 904L is a cheaper option where its resistance is enough.

What carbon limit applies to the 904L face?

A240/A240M-25a sets 0.020% maximum carbon for N08904.

Are 904L welds prone to cracking?

The fully austenitic weld metal is susceptible to hot cracking, so heat input and filler selection are controlled in the welding procedure.

Does the 904L face add to the plate tensile rating?

Within the A264 composite tensile section the face is part of the specimen, but design strength comes from the construction code and the backing.

Can 904L be supplied on Grade 60 backing?

Yes, if ordered. Grade 60 has its own chemistry and a lower 415–550 MPa tensile range.

What information is needed for a 904L clad quotation?

A264 edition, backing grade and thickness, minimum 904L thickness, size, quantity, final condition, bond and ultrasonic requirements and any corrosion test. Lead time is confirmed against the enquiry.