Q345R + S31603 clad steel plate bonds 022Cr17Ni12Mo2 low-carbon molybdenum-bearing austenitic stainless to a Q345R pressure-vessel backing under GB/T 8165-2025. Gangsteel supplies the plate with bond grade, route and layer thicknesses stated in the GB product marking.

Q345R + S31603 Stainless Clad Steel Plate - generated product illustration

Material Pair and Engineering Use

S31603 (022Cr17Ni12Mo2) is the GB equivalent family of 316L. Q345R + S31603 is one of the most common Chinese clad combinations for chemical, pharmaceutical, fertilizer and seawater-related vessels, and GB/T 8165-2025 itself uses S31603 on Q345R in its marking examples.

Material identity and specification basis
Part Designation Role
Backing Q345R, GB/T 713.2-2023 Pressure and structural load
Cladding S31603 (022Cr17Ni12Mo2), GB/T 4237-2015 Corrosion-resistant face
Clad product GB/T 8165-2025 (effective 2026-01-01); S31603 is a Table 2 typical cladding grade Bond grade, tests and marking

Backing Steel Requirements

Q345R backing: verified selected requirement
Item Requirement Boundary
Carbon (GB/T 713.2-2023, clause 7.1.2) ≤0.20% up to 60 mm; ≤0.22% above 60 mm Backing thickness, not total clad gage
Strength and impact Per GB/T 713.2-2023 table for the actual backing thickness and delivery condition No single 345 MPa figure applies at every thickness

Q345R is ordered to GB/T 713.2-2023 together with GB/T 713.1. Its strength and impact values depend on backing thickness and delivery condition, so they are taken from the standard table for the actual thickness rather than quoted as one figure.

Cladding Chemical Composition

GB/T 4237-2015 022Cr17Ni12Mo2 (S31603) cladding chemistry
Element Requirement, mass %
C ≤0.030
Si ≤0.75
Mn ≤2.00
P ≤0.045
S ≤0.030
Ni 10.00–14.00
Cr 16.00–18.00
Mo 2.00–3.00
N ≤0.10

Chemistry is from the GB/T 4237-2015 table. Close in composition to ASTM 316L, but a GB certificate and an A240 certificate are not interchangeable without checking each requirement.

Mechanical Properties of the Layers and the Bond

The facing strength is taken from the GB/T 4237-2015 table for the ordered grade and condition, and the Q345R strength from GB/T 713.2-2023 for the actual backing thickness. GB/T 8165-2025 then sets the finished-plate requirements below. Bond shear is an interface value and is never used as the tensile strength of the backing.

GB/T 8165-2025 finished-plate requirements (Tables 3 and 4, clause 7.2)
Item Requirement Note
Interface shear, bond Grades 1 and 2 ≥250 MPa Interface property; not the tensile strength of Q345R or of the composite
Interface shear, bond Grade 3 ≥210 MPa Lower quality grade; state the grade on the order
Composite tensile strength Not below the backing-standard lower limit; not more than 35 MPa above its upper limit, with the Table 4 footnote calculation permitted Record which basis was used
Bonded area, Grade 1 / 2 / 3 100% / ≥99% / ≥95% Single unbonded area limits ≤50 mm and ≤900 mm² / ≤50 mm and ≤2000 mm² / ≤75 mm and ≤4500 mm²; areas less than 20 mm apart are combined
Ultrasonic examination 100% of each plate to GB/T 7734 when the backing exceeds 4 mm For thinner backing, examination and sampling are agreed (GB/T 8651)
Impact Per the backing product standard; no impact test of the facing Specify test temperature only if the backing standard or order requires it

Fabrication Points for This Pair

Restore seams with a qualified 316L-type cap over a transition layer so that no Q345R is left exposed on the process side.

Specify the minimum S31603 thickness after grinding and forming, and keep the face free of carbon steel contamination.

Bonding Process, Delivery and Heat Treatment

GB/T 8165-2025 recognizes explosion bonding, explosion plus rolling and roll bonding. Under clause 5.2 the plate is delivered heat treated, or hot rolled, normalized rolled or thermomechanically rolled. The Q345R condition and the S31603 condition are agreed together as one route.

Manufacturing and delivery parameters for the enquiry
Parameter Order definition Engineering note
Bonding route Explosion (B), explosion plus rolling (BR) or rolling (R) The route code appears in the GB/T 8165 product marking
Layer thickness Backing gage plus minimum facing gage in mm; single- or double-sided Allow facing margin for grinding, forming and weld restoration; total gage alone does not define the plate.
Final thermal condition Heat treated, or as-rolled / normalized-rolled / TMCP per clause 5.2 Agree any simulated PWHT testing
Surface and edges Pickled or as agreed Face protected from iron
Lead time Confirmed against the enquiry Depends on plate area, layer gages, quantity, thermal condition and witnessed inspection.

Inspection and Certification

GB/T 8165 inspection combines the bond-grade ultrasonic examination, the Table 4 mechanical tests and the backing and facing certificates.

Inspection and test documents for the finished plate
Check What to specify Why it matters
Layer identity Separate backing and facing certificates with heat numbers No blended composite analysis
Bond grade Grade 1, 2 or 3 stated in the marking Sets shear and bonded-area limits
Ultrasonic 100% to GB/T 7734 for backing over 4 mm Bond area
Shear and tensile Table 4 requirements Interface and composite strength
Facing grade GB/T 4237 certificate for S31603 Chemistry and condition

Frequently Asked Questions

Is Q345R + S31603 the same as A516-70 + 316L?

The facings are similar in chemistry, but the standards, certificates and acceptance values differ. Order to one system and do not swap certificates.

Which bond grade should I order?

Grade 1 has 100% bonded area under the standard counting rules and Grade 2 at least 99%; both need 250 MPa shear. Grade 3 allows 95% and 210 MPa shear.

How is a Q345R + S31603 plate marked?

GB/T 8165-2025 marks the cladding grade, base grade, layer thicknesses, width × length, route code (B, BR or R), bond grade and standard number in that order. Its own examples include double-sided S31603 + Q345R + S30408 plate.

Can S31603 be clad on both sides?

Yes. GB/T 8165 covers double-sided plate, and shear testing is done for each bonded face.

Is ultrasonic examination of every plate required?

Yes, 100% under GB/T 7734 when the backing is over 4 mm thick.

What tensile requirement applies to the finished plate?

The composite tensile is at least the backing lower limit and no more than 35 MPa above its upper limit, with the Table 4 calculation allowed.

Does the molybdenum in S31603 guarantee chloride resistance?

No. It improves pitting resistance compared with S30403, but the medium, temperature and crevices decide suitability.

What should an enquiry for Q345R + S31603 include?

GB/T 8165 edition, bond grade, route, Q345R and S31603 thicknesses, size, quantity, delivery condition and test requirements. Lead time is confirmed against the enquiry.