ASTM A1011 Sheet & Strip
ASTM A1011 HSLAS Grade 55 Class 2 HSLA Hot Rolled Steel Sheet

ASTM A1011 HSLAS Grade 55 Class 2 — also written ASTM A1011 HSLAS Grade 55 Class 2, A1011M HSLAS Grade 55 [380] Class 2, A1011 high-strength low-alloy steel Grade 55 Class 2, SA-1011 HSLAS 55 Class 2 — is a high-strength low-alloy designation of ASTM A1011/A1011M for hot-rolled sheet and strip, with a minimum yield strength of 55 ksi [380 MPa] and a minimum tensile strength of 65 ksi [450 MPa]. Gangsteel supplies HSLAS Grade 55 Class 2 as black coil, pickled and oiled coil, slit strip and cut sheets for structural and formed parts.
What is ASTM A1011 HSLAS Grade 55 Class 2?
HSLAS steels in A1011 contain columbium (niobium), vanadium, titanium or molybdenum, added singly or in combination, which refine the grain and give strength at a lower carbon content than SS grades. Each HSLAS grade comes in two classes. Class 1 is the default; Class 2 limits carbon to 0.15% maximum for better weldability and formability and therefore has a minimum tensile strength 5 ksi lower than Class 1. HSLAS Grade 55 Class 2 is the Class 2 (low-carbon) version: carbon 0.15% max, minimum tensile 65 ksi [450 MPa].
ASTM A1011 HSLAS Grade 55 Class 2 Chemical Composition (Heat Analysis, %)
| Designation | C | Mn | P | S | Cu | Ni | Cr | Mo | V | Cb (Nb) | Ti | N |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| HSLAS Grade 55 Class 2 | 0.15 | 1.35 | 0.04 | 0.04 | 0.20 | 0.20 | 0.15 | 0.06 | 0.005 min | 0.005 min | 0.005 min | report |
| HSLAS Grade 55 Class 1 | 0.25 | 1.35 | 0.04 | 0.04 | 0.20 | 0.20 | 0.15 | 0.06 | 0.005 min | 0.005 min | 0.005 min | report |
The microalloying minimum of 0.005% applies only to the element or elements the producer chooses to add; not all three are required. Aluminium and silicon are reported. When copper-bearing steel is specified, copper is 0.20% minimum. Product (check) analysis tolerances follow ASTM A568/A568M.
ASTM A1011 HSLAS Grade 55 Class 2 Mechanical Properties
| Property | Requirement |
|---|---|
| Yield strength | 55 ksi [380 MPa] min |
| Tensile strength | 65 ksi [450 MPa] min |
| Elongation in 2 in [50 mm], over 0.097 in [2.5 mm] | ≥20% |
| Elongation in 2 in [50 mm], 0.097 in [2.5 mm] and under | ≥18% |
| Suggested min. inside radius, 90° cold bend | 2t |
The tension test is made on longitudinal, full-thickness specimens taken about midway between the centre and edge; on coils the producer tests from the coil end. Two tests are made per heat or per 50 tons, with both the thickest and thinnest gauge tested when they differ by 0.050 in [1.3 mm] or more. The bend radius is a non-mandatory guide from Appendix X1 of the standard.
Delivery Condition and Heat Treatment
ASTM A1011 HSLAS Grade 55 Class 2 is delivered in the hot-rolled condition. A1011 does not call for normalizing, quenching or any other post-rolling heat treatment: the strength and ductility are set on the hot strip mill by the chemistry, the finishing temperature, run-out-table cooling and the coiling temperature. The default surface is as rolled with its mill scale, and the purchaser may order the coil pickled (and oiled) or blast cleaned instead. Edges are supplied as mill edge unless cut edge is ordered, and general requirements such as dimensional tolerances, flatness and coil packaging follow ASTM A568/A568M for sheet or ASTM A749/A749M for strip.
| Item | Delivery condition per ASTM A1011/A1011M |
|---|---|
| Condition | Hot rolled (as rolled), coils or cut lengths |
| Surface finish | As rolled with mill scale (default); pickled, or blast cleaned when ordered |
| Oiling | As-rolled material is shipped dry; pickled or blast-cleaned material is oiled unless ordered dry |
| Edges | Mill edge or cut (slit / trimmed) edge |
| Product forms | Sheet (coils, cut-to-length sheets) and strip (narrow coils, slit strip) |
| General requirements | ASTM A568/A568M for sheet; ASTM A749/A749M for strip |
| Heat treatment | None required by A1011; properties come from hot rolling and controlled coiling |
For HSLAS grades the strength depends on the microalloy precipitation achieved during hot rolling and coiling, so the steel should not be normalized or hot formed by the user without checking that the properties are retained; stress relieving after welding is possible but should be qualified.
Ordering Information
| Ordering item | What to state on the enquiry |
|---|---|
| Standard | ASTM A1011 or A1011M with year of issue (we work to the current edition unless a year is stated) |
| Designation | HSLAS Grade 55 Class 2 (Class 1 is assumed if no class is given), e.g. “ASTM A1011M-23, HSLAS Grade 380 Class 2, pickled and oiled, 4.0 x 1500 mm coil” |
| Copper bearing | State when copper-bearing steel is required (Cu 0.20% min) |
| Finish | As rolled, pickled, or blast cleaned |
| Oiling | Oiled or dry (pickled / blasted material is normally oiled) |
| Edge | Mill edge or cut edge |
| Dimensions | Thickness, width, and length for cut lengths; coil ID, maximum OD and maximum coil mass for coils |
| Application | Part name or end use, so forming and surface requirements can be checked |
| Reports | Heat analysis and mechanical test report requirements, third-party inspection if any |
Comparable Grades
Approximate counterparts by minimum yield strength (for comparison only; test direction, thickness bands and chemistry differ): QStE380TM, S355MC. In plate thicknesses the closest ASTM structural grade is ASTM A572 Grade 50 / Grade 55.
Applications
HSLAS Grade 55 Class 2 is used for truck and trailer chassis members, crane booms, agricultural and construction equipment, roll-formed racking, wheels, brackets and structural tubes, where its strength allows thinner gauges than carbon steel. Class 2 is preferred for parts with tight bends, flanging or extensive welding.
Documents, Inspection and Lead Time
Every ASTM A1011 HSLAS Grade 55 Class 2 shipment from Gangsteel is supplied with a mill test certificate to EN 10204 type 3.1 that states the ASTM designation and year, the designation, grade, type or class, the heat number, the heat analysis and, for structural and high-strength designations, the tension test results, together with the purchase order number. Third-party inspection to EN 10204 type 3.2 by SGS, BV, TUV, LR or another agency nominated by the buyer can be arranged before shipment. Each coil or lift carries a tag with the specification, designation, heat number, size and mass.
Lead time is confirmed with each enquiry against the current hot strip mill rolling schedule, the thickness and width mix and any pickling, slitting or cut-to-length processing required, so please send the size list and quantity per item for a firm delivery date.
FAQ
What is the difference between HSLAS Grade 55 Class 2 and Class 1?
Both classes have the same minimum yield strength of 55 ksi [380 MPa]. Class 1 allows carbon up to 0.25% and requires a tensile strength of at least 70 ksi [480 MPa]; Class 2 limits carbon to 0.15% and requires at least 65 ksi [450 MPa]. Lower carbon in Class 2 improves weldability and formability; the suggested 90° bend radius is 2t for Class 1 and 2t for Class 2.
Which class do I get if I order HSLAS Grade 55 without a class?
A1011 assigns Class 1 by default. If your design or forming trials were based on Class 2, the class must be written on the purchase order, otherwise a mill may legitimately ship Class 1 with its higher carbon limit.
Which microalloying elements are used?
The standard lets the producer add columbium (niobium), vanadium, titanium or molybdenum, singly or in combination, with at least 0.005% of each element used. In practice hot strip mills mostly use niobium and titanium for these grades. The elements actually added are reported on the mill certificate.
Is HSLAS Grade 55 Class 2 suitable for welding?
Yes. With carbon 0.15% max, manganese 1.35% max and microalloying instead of high carbon, the steel welds well by MIG/MAG, submerged arc, resistance and laser processes. A1011 does not set a carbon equivalent limit, so if your welding procedure needs one, state the CE or Pcm formula and maximum on the enquiry.
What thicknesses can Gangsteel supply?
A1011 hot-rolled sheet and strip covers thicknesses below 0.230 in [6.0 mm]; the elongation table distinguishes material over and under 0.097 in [2.5 mm]. For heavier coil, ASTM A635/A635M (heavy-thickness coils) applies, and for plate the ASTM A572 series is the usual alternative. Send us the thickness, width and coil weight required and we will confirm the mill and lead time.
Related ASTM A1011 Designations
HSLAS Grade 45 Class 1 | HSLAS Grade 45 Class 2 | HSLAS Grade 50 Class 1 | HSLAS Grade 50 Class 2 | HSLAS Grade 55 Class 1 | HSLAS Grade 60 Class 1 | HSLAS Grade 60 Class 2 | HSLAS Grade 65 Class 1 | HSLAS Grade 65 Class 2 | HSLAS Grade 70 Class 1 | HSLAS Grade 70 Class 2 | ASTM A1011/A1011M standard overview