A131 steel plate
ASTM A131 FH32 Steel Plate | FH32 Shipbuilding Steel Plate
ASTM A131 FH32 steel plate, also written as A131/A131M Grade FH32, A131 FH32, ASTM A131 FH 32, A131 Gr FH32 or simply FH32 ship steel plate, is a higher-strength hull structural steel of the A131 steel plate specification with a specified minimum yield point of 315 MPa [46 ksi] and guaranteed Charpy V-notch toughness at -60°C [-76°F]. Gangsteel, a steel plate exporter, supplies A131 FH32 plates cut to size for shipbuilding, offshore structures and other marine applications.
In the grade name, "F" is the toughness class (Charpy V-notch test at -60°C), "H" means higher strength and "32" refers to the strength level, with a minimum yield point of 315 MPa [46 ksi]. Data source: Per ASTM A131/A131M-04 (Tables 2, 4, 5, 6 and 7). The current edition is A131/A131M-19; verify against it before ordering.
A131 FH32 Chemical Composition (Heat Analysis)
| Element | C | Mn | Si | P | S | Al (acid sol.) |
|---|---|---|---|---|---|---|
| FH32, % | 0.16 max | 0.90-1.60 | 0.10-0.50 | 0.025 max | 0.025 max | 0.015 min |
| Element | Nb | V | Ti | Cu | Cr | Ni / Mo |
| FH32, % | 0.02-0.05 | 0.05-0.10 | 0.02 max | 0.35 max | 0.20 max | 0.40 max / 0.08 max |
| Element | N | - | - | - | - | - |
| FH32, % | 0.009 max (0.012 if Al present) | - | - | - | - | - |
Per ASTM A131/A131M-04, Table 4. The steel is killed and made to fine grain practice; Al, Nb and V grain-refining elements may be used singly or in combination, and when used in combination the minimum contents of 7.2.2 and 7.2.3 apply instead. Where soluble aluminum is not less than 0.015%, the minimum silicon content does not apply. Cu, Cr, Ni and Mo may be reported as ≤0.02% when not exceeding 0.02%. Carbon equivalent: Ceq = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15 (%), for TMCP plate limited to 0.36% max per Table 5.
Product Analysis (Check Analysis)
Per ASTM A131/A131M-04 (6.1.1 and Supplementary Requirement S85), when product analysis is specified, the finished plate shall conform to the Table 4 limits below, subject to the product analysis tolerances in ASTM A6/A6M.
| Element | Limit applied to product analysis | Tolerance |
|---|---|---|
| C | 0.16 max | per ASTM A6/A6M |
| Mn | 0.90-1.60 | per ASTM A6/A6M |
| Si | 0.10-0.50 | per ASTM A6/A6M |
| P / S | 0.025 max | per ASTM A6/A6M |
| Al (acid sol.) | 0.015 min | per ASTM A6/A6M |
| Nb / V | 0.02-0.05 / 0.05-0.10 | per ASTM A6/A6M |
| Ti | 0.02 max | per ASTM A6/A6M |
| Cu / Cr / Ni / Mo | 0.35 / 0.20 / 0.40 / 0.08 max | per ASTM A6/A6M |
| N | 0.009 max (0.012 if Al present) | per ASTM A6/A6M |
A131 FH32 Mechanical Properties
| Grade | Yield point, min | Tensile strength | Elongation in 200 mm, min | Elongation in 50 mm, min |
|---|---|---|---|---|
| A131 FH32 | 315 MPa [46 ksi] | 440-590 MPa [64-85 ksi] | 19% | 22% |
Per ASTM A131/A131M-04, Table 6. For thickness under 8 mm a deduction from the 200 mm elongation applies, and over 90 mm a deduction from the 50 mm elongation applies, per ASTM A6/A6M.
Charpy V-Notch Impact Requirements (-60°C)
| Thickness | Test temperature | Longitudinal, avg min | Transverse, avg min |
|---|---|---|---|
| t ≤ 50 mm | -60°C [-76°F] | 34 J [25 ft-lbf] | 24 J [17 ft-lbf] |
| 50 < t ≤ 100 mm | -60°C [-76°F] | not specified in Table 7 | not specified in Table 7 |
Per ASTM A131/A131M-04, Table 7; average of three full-size specimens, not more than one value below the average and none below 70% of it. Either orientation is acceptable unless specified (S86). Per 8.2.2, FH32 plate is impact tested with one set of three specimens from each plate-as-rolled.
Thickness Range and Delivery Condition
ASTM A131/A131M covers plates up to 100 mm [4 in.] thick in Tables 1, 2 and 7. FH32 plates in all thicknesses shall be normalized, thermo-mechanically controlled processed or quenched and tempered (5.5); quenched and tempered plate gets one tension test per plate (8.1.4). Plates are marked N, CR, TM or QT to show the condition of supply (Section 12). Optional requirements by agreement include product analysis (S85), impact specimen orientation (S86), additional tension tests (S88), ultrasonic testing and third-party inspection.
Boiler steel plates | Alloy steel plates | Low alloy high strength steel plate | Carbon steel plate
Equivalent Steel Grade of A131 FH32
| DNV steel plate | GL steel plate | LR steel plate | BV steel plate | CCS steel plate | NK steel plate | KR steel plate | RINA steel plate |
|---|---|---|---|---|---|---|---|
| NV F32 | GL-F32 | LR/FH32 | BV/FH32 | CCS/F32 | K F32 | R F32 | RI/F32 |
If you need more stock steel plates in shipbuilding steel plate, please click stock steel plates.
Related grades: A131 AH32 | ASTM A131 AH40 steel plate | A131 EH32
FAQ about ASTM A131 FH32 Steel Plate
What is ASTM A131 FH32 steel?
It is a higher-strength hull structural steel in ASTM A131/A131M with 315 MPa [46 ksi] minimum yield point and Charpy impact toughness at -60°C, used for ship hulls and marine structures.
What is the yield strength of A131 FH32?
Minimum 315 MPa [46 ksi], with tensile strength 440-590 MPa [64-85 ksi] (Table 6).
What is the impact test temperature for A131 FH32?
-60°C [-76°F]. Minimum average energy for t ≤ 50 mm is 34 J [25 ft-lbf] longitudinal and 24 J [17 ft-lbf] transverse.
Is A131 FH32 the same as ABS FH32?
The requirements are essentially harmonized; the ABS grade additionally carries ABS class certification and survey. Plates can be dual-certified.
What does FH32 stand for?
F = toughness class (Charpy test at -60°C), H = higher strength, 32 = strength level with 315 MPa [46 ksi] minimum yield point.
What is the carbon equivalent limit for TMCP FH32?
Per Table 5, 0.36% max, using Ceq = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15.
What delivery condition is required for A131 FH32?
Normalized, TMCP or quenched and tempered in all thicknesses.
Is A131 FH32 weldable?
Yes. Its controlled carbon and carbon equivalent give good weldability with standard shipyard procedures; preheat may be needed for thick or highly restrained joints.
What is the maximum thickness of A131 FH32 plate?
ASTM A131/A131M-04 covers plates up to 100 mm [4 in.]; Table 7 gives impact values only up to 50 mm for this grade, so heavier plate needs agreement.
Other ASTM A131 Grades
ASTM A131 Grade A steel plate | ASTM A131 Grade B steel plate | ASTM A131 Grade D steel plate | ASTM A131 Grade E steel plate | ASTM A131 AH32 steel plate | ASTM A131 AH36 steel plate | ASTM A131 AH40 steel plate | ASTM A131 DH32 steel plate | ASTM A131 DH36 steel plate | ASTM A131 DH40 steel plate | ASTM A131 EH32 steel plate | ASTM A131 EH36 steel plate | ASTM A131 EH40 steel plate | ASTM A131 FH36 steel plate | ASTM A131 FH40 steel plate
Equivalent Class Society Grades
ASTM A131 FH32 corresponds to the same grade under the IACS member classification societies: CCS FH32 steel plate, ABS FH32 steel plate, LR FH32 steel plate.
-
ASTM A131 AH36 Steel Plate | AH
Gangsteelis specialized in supplying A131high strength steel plate in A131 Grade AH36,A131 AH36,A131 Grade AH36
-
ASTM A131 FH36 Steel Plate | FH
Gangsteelis specialized in supplying A131 high strength steel plate in A131 Grade FH36 A131 FH36,A131 Grade FH3
-
ASTM A131 FH32 Steel Plate | FH
Gangsteelis specialized in supplying A131high strength steel plate in A131 Grade DH32,A131 grade FH32. A131 FH3
-
ASTM A131 DH36 Steel Plate | DH
Gangsteelis specialized in supplying A131 high strength steel plate in A131 Grade DH36 A131 DH36,ASTM A131 Grad