Q345R + S30403 stainless clad steel plate combines a Chinese pressure-equipment backing with low-carbon 022Cr19Ni10 stainless facing. Gangsteel specifies the Q345R backing, the facing product standard and the finished clad-product requirements separately; a low-carbon stainless name alone does not establish the qualification of a bonded pressure-vessel plate.

Q345R + S30403 Stainless Clad Steel Plate - generated product illustration

Specification and Application

The example order basis here is Q345R to GB/T 713.2-2023 with GB/T 713.1, and 022Cr19Ni10/S30403 facing to GB/T 4237-2015, bonded to GB/T 8165-2025. The GB/T 8165 edition became effective in 2026. S30403 is not explicitly among its Table 2 typical facing codes, so the contract should invoke clause 7.1 for the purchaser-requested grade and state its product standard. Pressure-equipment projects may require a different approved facing specification; this must be resolved in the order rather than inferred from the code S30403.

This pairing is considered for fabricated vessels, storage and process equipment when the low-carbon austenitic face suits the medium and the Q345R backing is accepted by the governing design code. It is not automatically interchangeable with A516 Grade 70 plus ASTM 304L, and is not an automatic sour-service or low-temperature qualification.

Backing and Facing Chemical Composition

GB layers: selected chemistry, not an averaged composite analysis
Layer / source Element Limit, mass % Boundary
Q345R; GB/T 713.2-2023 clause 7.1.2 C ≤0.20 through 60 mm; ≤0.22 above 60 mm Backing thickness; other elements follow the ordered standard
022Cr19Ni10 / S30403; GB/T 4237-2015 C ≤0.030 Facing chemistry
022Cr19Ni10 / S30403; GB/T 4237-2015 Cr 17.50–19.50 GB chemistry limits, not the A240 304L range
022Cr19Ni10 / S30403; GB/T 4237-2015 Ni 8.00–12.00 Facing chemistry

This is a deliberately selected chemistry table. The backing and facing still require their complete material certificates. A matching S30403 code does not make the GB product specification identical to ASTM A240 Type 304L.

GB/T 4237-2015 022Cr19Ni10 (S30403 (GB unified code)): cladding chemistry, mass %
Element Requirement
C ≤0.030
Mn ≤2.00
Si ≤0.75
P ≤0.045
S ≤0.030
Cr 17.50–19.50
Ni 8.00–12.00
N ≤0.10

Mechanical Properties of the Layers

Constituent properties: distinguish the GB facing from the backing
Layer Reference and condition Yield / proof strength Tensile strength Elongation
Q345R backing GB/T 713.2-2023, ordered thickness and delivery condition Use the Table 2 value for the actual backing thickness Use the Table 2 range for actual backing thickness Use applicable backing-standard specimen requirement
022Cr19Ni10 / S30403 facing GB/T 4237-2015 Table 20, solution-treated flat product Rp0.2 ≥180 MPa Rm ≥485 MPa A ≥40%

The Q345R designation is not a constant yield guarantee at every thickness. Its product-standard strength and impact requirements must be matched to the actual backing thickness and condition. The facing row is a constituent reference, not an isolated thin-layer test promise for every finished clad plate. Do not substitute the ASTM 304L proof-strength value for the GB facing requirement.

Finished Bond and Composite Acceptance

GB/T 8165-2025 Table 4: finished-composite mechanical requirements
Property Requirement / scope Important distinction
Interface shear, Grades 1 and 2 ≥250 MPa Interface property; not backing or composite tensile strength
Interface shear, Grade 3 ≥210 MPa Different quality grade; do not substitute ASTM's 140 MPa criterion
Yield / proof strength Reference the applicable backing product-standard thickness requirement and the permitted Table 4 footnote calculation Record the selected acceptance basis; do not use a universal 345 MPa for every thickness
Tensile strength Backing-product thickness lower limit and no more than 35 MPa above its upper limit, subject to Table 4 footnote provisions The standard also provides a constituent-thickness calculation for the lower limit; design allowables are separate
Elongation Not less than the relevant backing product-standard requirement Specimen basis must be stated
Impact Relevant backing product specification; no facing impact test Where backing standard has no impact requirement, Table 4 allows omission
Double-sided plate Test interface shear for both bonded faces A result from one face does not certify the other

The permitted strength calculations in Table 4 use each layer's minimum strength and thickness; they are not permission to average a delivered heat analysis or invent a code design allowable. The test report should identify whether a backing-based limit or the permitted constituent calculation was used.

GB/T 8165-2025 Table 3: bonded-area quality grades
Grade Bonded-area rate Reportable individual unbonded area limit
1 100% under the standard's indication-counting rules Individual unbonded regions within the Table 3 exclusion (length ≤50 mm and area ≤900 mm²) are not counted; larger reportable regions do not satisfy Grade 1
2 ≥99% Length ≤50 mm and area ≤2000 mm²
3 ≥95% Length ≤75 mm and area ≤4500 mm²

The standard groups adjacent unbonded areas when their minimum separation is not more than 20 mm, using the combined area. Unbonded areas below 900 mm² need not be recorded. Therefore Grade 1 terminology is not a claim that every microscopic point has been demonstrated bonded. For backing thickness above 4 mm, clause 7.2.1 requires 100% ultrasonic examination of each plate under GB/T 7734. For backing at or below 4 mm, ultrasonic examination and sampling are agreed as specified using GB/T 8651.

Fabrication and Corrosion-Side Control

Specify the remaining facing thickness after any grinding, forming or weld restoration. Low carbon helps when assessing sensitization risk but does not prove resistance to the actual process chemistry. Protect the stainless face from carbon-steel grinding contamination, and use a qualified transition and weld-restoration procedure so that the exposed weld surface retains the required corrosion performance. Bond testing does not qualify the weld procedure.

Bonding Process, Delivery and Heat Treatment

Explosion bonding joins prepared metal surfaces by a controlled high-velocity collision. Hot-roll bonding establishes the metallurgical bond during rolling of a prepared assembly; explosion bonding followed by rolling is a separate combined route. These are integrally bonded plates, not loose liners, adhesive laminates or chromium-carbide weld-overlay wear plates.

GB/T 8165-2025 distinguishes explosive bonding, explosion-plus-rolling and roll bonding, and specifies heat-treated delivery, with hot-rolled, normalized-rolled or thermomechanically rolled delivery also permitted. The selected Q345R condition and stainless condition must be agreed as part of one manufacturing route.

Manufacturing and delivery parameters to put on the enquiry
Parameter Required order definition Technical note
Bonding route Explosion bonded, hot-roll bonded, or combined route Route capability depends on the material pair, area, layer ratio and final condition. No blanket stock range is implied.
Thickness Backing thickness + minimum facing thickness, in mm; identify one or two clad faces Reserve facing allowance for grinding, forming and weld restoration. Total thickness alone is insufficient.
Final thermal condition Named delivery condition and any simulated fabrication/PWHT cycle Test in the representative final condition; agree number and duration of simulated cycles where required.
Heat-treatment temperature / hold Qualified procedure for the selected pair and thickness No single temperature, hold time or cooling rate is specified here for all clad plates.
Surface and cutting As agreed: pickled, ground or specified finish; edge machining and protection Prevent carbon-steel contamination of the corrosion-resistant face.
Lead time Confirmed against the enquiry and agreed inspection plan Not a fixed number of days for every thickness or bonding route.

An order for Q345R plus S30403 must identify whether the facing product standard is GB/T 4237, GB/T 713.7 or another agreed specification. The code S30403 alone does not define a pressure-equipment plate certificate or a finished-composite delivery condition.

Inspection Documents to Request

Request backing and facing material certificates, finished tensile and bond test results, a bond-area ultrasonic report to the ordered grade, dimensional/facing-thickness checks, final heat-treatment records and any repair documentation. Specify corrosion tests and extra backing impact, HIC or simulated fabrication-cycle testing when required. A plate certificate must report what was actually ordered and tested rather than simply repeating "Q345R + 304L".

Frequently Asked Questions

Is GB S30403 exactly the same order as ASTM Type 304L?

No. They are closely related low-carbon austenitic designations but the product-standard requirements are not identical. This page uses GB/T 4237-2015 chemistry and its 180 MPa proof-strength minimum; an ASTM order must identify its own A240 edition and acceptance values.

Why must S30403 be specially written into the GB/T 8165-2025 order?

It is not explicitly in the typical-facing list in Table 2. Clause 7.1 permits purchaser-requested grades outside that list, so specify 022Cr19Ni10/S30403 and its component product standard. Do not silently substitute the listed S30408 grade.

Can I use 345 MPa for the entire clad plate at every thickness?

No. Q345R backing strength depends on its product-standard thickness range, and the finished-composite requirements follow GB/T 8165 Table 4 including its notes. Pressure-design allowable stress is a separate construction-code matter.

What is the difference between 250 MPa and 210 MPa on a GB clad plate enquiry?

They are the Table 4 minimum interface shear values for quality Grades 1/2 and Grade 3 respectively. They are not alternative Q345R tensile grades. The order must define the quality grade and the corresponding bond-area requirements together.

Does a Grade 1 order prove an absolutely perfect bond at every point?

It is evaluated under the standard's ultrasonic indication and counting rules, including its small-area provisions. Scanning coverage and the standard-defined bonded-area rate are different concepts; request the examination report rather than relying on a bare "100% bonded" sales statement.

Can a 20 + 3 mm notation be used on the drawing?

Yes, if it explicitly states which number is the backing and which is the minimum facing thickness and defines tolerances. It is only a notation example here, not an advertised stock size. Identify whether minimum facing thickness applies before or after finishing and forming.

Is post-weld heat treatment automatically suitable for both layers?

No. The Q345R condition, stainless corrosion behavior, bond and fabrication-code requirements must be evaluated together. State the proposed cycle, number of cycles and any required simulated-cycle testing before manufacture; do not apply a generic furnace recipe.

How should I obtain a price and reliable delivery date?

Send the full GB constituent and clad specifications with editions, quality grade, size, backing and minimum facing thicknesses, quantity, route restrictions, final condition and inspection requirements. Gangsteel confirms lead time against that enquiry; no universal delivery interval is implied.

Related Specifications

GB/T 8165-2025 standard overview; A516 Grade 70 + ASTM 304L alternative specification route; pressure-vessel backing steels.

Other Products