Q345R + S32168 clad steel plate bonds 06Cr18Ni11Ti titanium-stabilized austenitic stainless to a Q345R pressure-vessel backing under GB/T 8165-2025. Gangsteel supplies it for heat exchangers and process vessels with the GB bond grade stated on the order.

Q345R + S32168 Stainless Clad Steel Plate - generated product illustration

Material Pair and Engineering Use

S32168 (06Cr18Ni11Ti) is the GB titanium-stabilized 18-8 grade, related to ASTM 321. Q345R + S32168 is widely used for petrochemical and chemical vessels and heat exchangers where sensitization during fabrication or warm service is a concern. GB/T 8165-2025 uses S32168 on Q345R in its first marking example.

Material identity and specification basis
Part Designation Role
Backing Q345R, GB/T 713.2-2023 Pressure and structural load
Cladding S32168 (06Cr18Ni11Ti), GB/T 4237-2015 Corrosion-resistant face
Clad product GB/T 8165-2025 (effective 2026-01-01); S32168 is a Table 2 typical cladding grade Bond grade, tests and marking

Backing Steel Requirements

Q345R backing: verified selected requirement
Item Requirement Boundary
Carbon (GB/T 713.2-2023, clause 7.1.2) ≤0.20% up to 60 mm; ≤0.22% above 60 mm Backing thickness, not total clad gage
Strength and impact Per GB/T 713.2-2023 table for the actual backing thickness and delivery condition No single 345 MPa figure applies at every thickness

Q345R is ordered to GB/T 713.2-2023 together with GB/T 713.1. Its strength and impact values depend on backing thickness and delivery condition, so they are taken from the standard table for the actual thickness rather than quoted as one figure.

Cladding Chemical Composition

GB/T 4237-2015 06Cr18Ni11Ti (S32168) cladding chemistry
Element Requirement, mass %
C ≤0.08
Si ≤0.75
Mn ≤2.00
P ≤0.045
S ≤0.030
Ni 9.00–12.00
Cr 17.00–19.00
Ti ≥5×C

Chemistry is from the GB/T 4237-2015 table. The GB titanium rule (≥5×C) differs from the ASTM A240 Type 321 rule (5×(C+N), 0.70 max), which is one reason GB and ASTM certificates are not interchangeable.

Mechanical Properties of the Layers and the Bond

The facing strength is taken from the GB/T 4237-2015 table for the ordered grade and condition, and the Q345R strength from GB/T 713.2-2023 for the actual backing thickness. GB/T 8165-2025 then sets the finished-plate requirements below. Bond shear is an interface value and is never used as the tensile strength of the backing.

GB/T 8165-2025 finished-plate requirements (Tables 3 and 4, clause 7.2)
Item Requirement Note
Interface shear, bond Grades 1 and 2 ≥250 MPa Interface property; not the tensile strength of Q345R or of the composite
Interface shear, bond Grade 3 ≥210 MPa Lower quality grade; state the grade on the order
Composite tensile strength Not below the backing-standard lower limit; not more than 35 MPa above its upper limit, with the Table 4 footnote calculation permitted Record which basis was used
Bonded area, Grade 1 / 2 / 3 100% / ≥99% / ≥95% Single unbonded area limits ≤50 mm and ≤900 mm² / ≤50 mm and ≤2000 mm² / ≤75 mm and ≤4500 mm²; areas less than 20 mm apart are combined
Ultrasonic examination 100% of each plate to GB/T 7734 when the backing exceeds 4 mm For thinner backing, examination and sampling are agreed (GB/T 8651)
Impact Per the backing product standard; no impact test of the facing Specify test temperature only if the backing standard or order requires it

Fabrication Points for This Pair

Restore the face at seams with a qualified stabilized stainless cap over a transition layer; niobium-stabilized filler is common because titanium transfers poorly across the arc.

Keep enough S32168 thickness after grinding at weld preparations and protect the face from iron contamination.

Bonding Process, Delivery and Heat Treatment

GB/T 8165-2025 recognizes explosion bonding, explosion plus rolling and roll bonding. Under clause 5.2 the plate is delivered heat treated, or hot rolled, normalized rolled or thermomechanically rolled. The Q345R condition and the S32168 condition are agreed together as one route.

Manufacturing and delivery parameters for the enquiry
Parameter Order definition Engineering note
Bonding route Explosion (B), explosion plus rolling (BR) or rolling (R) The route code appears in the GB/T 8165 product marking
Layer thickness Backing gage plus minimum facing gage in mm; single- or double-sided Allow facing margin for grinding, forming and weld restoration; total gage alone does not define the plate.
Final thermal condition Heat treated, or as-rolled / normalized-rolled / TMCP per clause 5.2 Agree any simulated PWHT testing
Surface and edges Pickled or as agreed Face protected from iron
Lead time Confirmed against the enquiry Depends on plate area, layer gages, quantity, thermal condition and witnessed inspection.

Inspection and Certification

GB/T 8165 inspection combines the bond-grade ultrasonic examination, the Table 4 mechanical tests and the backing and facing certificates.

Inspection and test documents for the finished plate
Check What to specify Why it matters
Layer identity Separate backing and facing certificates with heat numbers No blended composite analysis
Bond grade Grade 1, 2 or 3 stated in the marking Sets shear and bonded-area limits
Ultrasonic 100% to GB/T 7734 for backing over 4 mm Bond area
Shear and tensile Table 4 requirements Interface and composite strength
Facing grade GB/T 4237 certificate for S32168 Chemistry and condition

Frequently Asked Questions

Is S32168 the same as ASTM 321?

They are closely related titanium-stabilized grades, but the GB titanium requirement is ≥5×C while A240 uses 5×(C+N) with a 0.70% maximum.

Why choose S32168 instead of S30408 facing?

Titanium stabilization helps resist sensitization during welding or warm service. S30408 has no stabilizing element.

Does GB/T 8165 list S32168 as a standard cladding grade?

Yes. S32168 is in Table 2 of typical cladding grades and is used in the standard marking example with Q345R.

What shear strength does a Grade 2 bond need?

At least 250 MPa, the same as Grade 1; Grade 3 needs 210 MPa.

Is intergranular corrosion testing included?

Only if the order specifies it, with the method and acceptance stated.

Does a rolled (R) plate differ from an explosion (B) plate in acceptance?

Both meet the same GB/T 8165 bond-grade and Table 4 requirements; the route code records how the plate was made.

How much can composite tensile exceed the backing range?

Not more than 35 MPa above the backing upper limit, subject to the Table 4 footnote calculation.

What should a Q345R + S32168 enquiry include?

GB/T 8165 edition, bond grade, route, layer thicknesses, size, quantity, delivery condition and any corrosion or PWHT tests. Lead time is confirmed against the enquiry.