RINA steel plate
RINA D620 Steel Plate | D620 Shipbuilding Steel Plate
RINA D620 steel plate, also written as RI/D620, RINA Grade D620, Registro Italiano Navale D620 or market names such as DH62 / DQ63, is the extra-high-strength hull structural steel of RINA Rules for the Classification of Ships (IACS UR W16 extra-high-strength family) with 620 MPa minimum yield, 720-890 MPa tensile strength and Charpy V-notch toughness at -20°C [-4°F]. In the grade name, "D" is the toughness class, and "620" is the yield-strength level in MPa (not AH620). Gangsteel, a steel plate exporter, supplies RINA D620 / RI/D620 plates cut to size for shipbuilding, offshore platforms and marine structures.
Data source: Per IACS UR W16 (extra-high-strength hull structural steel) as adopted in RINA (Registro Italiano Navale) hull structural steel rules, cross-checked with LR DH62 / ABS DQ63 sibling pages on gangsteel.net. Official mill/certificate grade is RINA D620 (RI/D620). Verify the current RINA edition before ordering.
RINA D620 Chemical Composition (Heat Analysis)
| Element | C | Mn | Si | P | S | Al (acid sol.) |
|---|---|---|---|---|---|---|
| RINA D620, % | 0.20 max | 1.70 max | 0.10-0.55 | 0.030 max | 0.030 max | 0.015 min |
| Element | N | Nb | V | Ti | B | Notes |
| RINA D620, % | 0.020 max | 0.02-0.05 | 0.04-0.10 | 0.02 max | 0.005 max | Ni/Cu/Cr/Mo per delivery condition (N/TM/QT) in UR W16 |
Per IACS UR W16 / RINA extra-high-strength rules. Exact maxima for Ni, Cu, Cr and Mo depend on delivery condition (N/NR, TM or QT). Carbon equivalent / CET / Pcm limits apply by thickness and condition; confirm on the mill certificate and current rule edition.
Product Analysis (Check Analysis)
When product analysis is required, apply ASTM A6/A6M Table A permitted variations to the heat limits unless the element is min-only or not listed in Table A.
| Element | Heat analysis limit | Product analysis (heat ± A6) |
|---|---|---|
| C | 0.20 max | 0.24 max |
| Mn | 1.70 max | see A6 Table A vs heat upper limit |
| Si | 0.10-0.55 | 0.05–0.61 (approx. A6) |
| P | 0.030 max | 0.040 max |
| S | 0.030 max | 0.040 max |
| Al (acid sol.) | 0.015 min | no A6 Table A tolerance; product value not tabulated |
| N | 0.020 max | 0.025 max (typical A6 +0.005) |
| Nb | 0.02-0.05 | 0.010–0.060 |
| V | 0.04-0.10 | 0.030–0.110 |
| Ti | 0.02 max | 0.03 max |
| B | 0.005 max | product analysis often not applicable |
Product analysis applies only when specified; for a range, results may not vary both above and below it.
RINA D620 Mechanical Properties
| Grade | Yield strength, min | Tensile strength | Elongation, min |
|---|---|---|---|
| RINA D620 | 620 MPa [90 ksi] | 720-890 MPa [104-129 ksi] | 15% |
Per IACS UR W16 / RINA rules (common t≤50 mm values). Yield may step down for thicker plates per UR W16; confirm thickness-dependent values on the order.
Charpy V-Notch Impact Requirements (-20°C [-4°F])
| Thickness | Test temperature | Longitudinal, avg min | Transverse, avg min |
|---|---|---|---|
| t≤50 mm | -20°C [-4°F] | 62 J | 41 J |
| 50<t≤70 mm | -20°C [-4°F] | 62 J | 41 J |
| 70<t≤100 mm | -20°C [-4°F] | 62 J | 41 J |
Per IACS UR W16 / RINA extra-high-strength practice. Average of three full-size specimens; transverse values apply when required. Thicker plates by agreement.
Delivery Condition and Deoxidation
Deoxidation: Killed, fine-grain practice. Delivery condition: typically TMCP or QT for extra-high-strength plates; N/NR may apply at lower extra-high levels per rules. D-class (D620) grades are typically normalized or TMCP; controlled-rolled delivery may apply within rule limits. Optional extras: UT, Z15/Z25/Z35, RINA survey.
Thickness Coverage
Extra-high-strength RINA A/D/E/F 420-690 plates are commonly supplied from about 6 mm to 100 mm thick (thicker by agreement under UR W16). Width 1500-4000 mm and length 6000-18000 mm are typical.
Equivalent Steel Grades of RINA D620
| Society / Standard | Equivalent grade |
|---|---|
| RINA (Registro Italiano Navale) | RINA D620 steel plate (RI/D620; LR DH62 / ABS DQ63) |
| LR (Lloyd's Register) | LR DH62 steel plate |
| ABS | ABS DQ63 steel plate |
| CCS | CCS D620 steel plate |
| GL | GL D620 steel plate |
| DNV | DNV D620 steel plate |
| NK | NK D63 steel plate |
| BV | BV D620 steel plate |
IACS societies align extra-high-strength hull grades under UR W16; naming differs (RINA D620, LR DH62, ABS DQ63). Dual certification is common when ordered that way.
FAQ about RINA D620 Steel Plate
What is RINA D620 steel plate?
It is an extra-high-strength hull structural steel under RINA Rules (IACS UR W16 extra-high-strength family), with 620 MPa minimum yield, 720-890 MPa tensile strength and Charpy toughness at -20°C [-4°F]. The mill certificate grade is RINA D620 (RI/D620).
What does RINA D620 / RI/D620 stand for?
RINA is Registro Italiano Navale (RI on certificates). The letter D is the toughness class (Charpy at -20°C [-4°F]), and 620 is the yield-strength level in MPa. Market/LR naming often uses DH62; ABS often uses DQ63. Note: RINA does not use AH620 — the grade is D620, not AH620.
What is the yield strength of RINA D620?
Minimum 620 MPa (90 ksi), tensile 720-890 MPa (104-129 ksi), elongation about 15% min (for the common thickness range).
What is the impact test temperature for RINA D620?
Charpy V-notch at -20°C [-4°F]. Typical longitudinal average minimum is 62 J (transverse 41 J) for the tabulated thickness range on this grade page.
What is the difference between RINA A620, D620, E620 and F620?
Same 620 MPa strength class. Toughness class differs: A at 0°C, D at -20°C, E at -40°C, F at -60°C. Chemistry (C, P, S, Mn) is tightened for colder classes.
How does RINA D620 differ from higher-strength RINA AH40?
RINA AH40 is UR W11 higher-strength (390 MPa). RINA D620 is UR W16 extra-high-strength (620 MPa) with different chemistry and delivery practice (often TM/QT).
Is RINA D620 the same as LR DH62 or ABS DQ63?
They are IACS counterparts in the extra-high-strength family; exact chemistry/delivery options differ by society edition. Dual certification is available when surveys are arranged.
Is RINA D620 weldable?
Weldable with approved procedures for extra-high-strength ship steel. Preheat, heat input and consumable matching are critical; follow the mill WPS and RINA welding requirements.
What heat treatment is required for RINA D620?
Extra-high-strength grades are typically delivered TMCP or quenched and tempered (QT), sometimes normalized/normalized-rolled depending on strength level and thickness. D-class (D620) grades are typically normalized or TMCP; controlled-rolled delivery may apply within rule limits. Optional extras: UT, Z15/Z25/Z35, RINA survey.
What thickness is available for RINA D620?
Common supply is about 6-100 mm (thicker by agreement under UR W16 / RINA rules), 1500-4000 mm wide and 6000-18000 mm long.
Other RINA Steel Plate Grades
RINA Grade A steel plate | RINA Grade B steel plate | RINA Grade D steel plate | RINA Grade E steel plate | RINA AH32 steel plate | RINA AH36 steel plate | RINA AH40 steel plate | RINA DH32 steel plate | RINA DH36 steel plate | RINA DH40 steel plate | RINA EH32 steel plate | RINA EH36 steel plate | RINA EH40 steel plate | RINA FH32 steel plate | RINA FH36 steel plate | RINA FH40 steel plate | RINA A420 steel plate | RINA A460 steel plate | RINA A500 steel plate | RINA A550 steel plate | RINA A620 steel plate | RINA A690 steel plate | RINA D420 steel plate | RINA D460 steel plate | RINA D500 steel plate | RINA D550 steel plate | RINA D690 steel plate | RINA E420 steel plate | RINA E460 steel plate | RINA E500 steel plate | RINA E550 steel plate | RINA E620 steel plate | RINA E690 steel plate | RINA F420 steel plate | RINA F460 steel plate | RINA F500 steel plate | RINA F550 steel plate | RINA F620 steel plate | RINA F690 steel plate
Equivalent Class Society Grades
RINA D620 corresponds to extra-high-strength counterparts under other IACS societies (LR DH62, ABS DQ63, etc.): LR DH62 steel plate, ABS DQ63 steel plate, CCS D620 steel plate, GL D620 steel plate, DNV D620 steel plate, NK D63 steel plate, BV D620 steel plate, RINA D620 steel plate.
-
RINA DH36 Steel Plate | DH36 Sh
RINA DH36 (RI/DH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at -20C, chemistry and
-
RINA AH36 Steel Plate | AH36 Sh
RINA AH36 (RI/AH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at 0C, chemistry and e
-
RINA FH32 Steel Plate | FH32 Sh
RINA FH32 (RI/FH32) shipbuilding steel plate: 315 MPa yield, 440-590 MPa tensile, Charpy at -60C, chemistry and
-
RINA Grade A Steel Plate | Grad
RINA Grade A (RI/A) shipbuilding steel plate: 235 MPa yield, 400-520 MPa tensile, Charpy at +20C, chemistry and