RINA steel plate
RINA E460 Steel Plate | E460 Shipbuilding Steel Plate
RINA E460 steel plate, also written as RI/E460, RINA Grade E460, Registro Italiano Navale E460 or market names such as EH46 / EQ47, is the extra-high-strength hull structural steel of RINA Rules for the Classification of Ships (IACS UR W16 extra-high-strength family) with 460 MPa minimum yield, 570-720 MPa tensile strength and Charpy V-notch toughness at -40°C [-40°F]. In the grade name, "E" is the toughness class, and "460" is the yield-strength level in MPa (not AH460). Gangsteel, a steel plate exporter, supplies RINA E460 / RI/E460 plates cut to size for shipbuilding, offshore platforms and marine structures.
Data source: Per IACS UR W16 (extra-high-strength hull structural steel) as adopted in RINA (Registro Italiano Navale) hull structural steel rules, cross-checked with LR EH46 / ABS EQ47 sibling pages on gangsteel.net. Official mill/certificate grade is RINA E460 (RI/E460). Verify the current RINA edition before ordering.
RINA E460 Chemical Composition (Heat Analysis)
| Element | C | Mn | Si | P | S | Al (acid sol.) |
|---|---|---|---|---|---|---|
| RINA E460, % | 0.20 max | 1.70 max | 0.10-0.55 | 0.030 max | 0.030 max | 0.015 min |
| Element | N | Nb | V | Ti | B | Notes |
| RINA E460, % | 0.020 max | 0.02-0.05 | 0.04-0.10 | 0.02 max | 0.005 max | Ni/Cu/Cr/Mo per delivery condition (N/TM/QT) in UR W16 |
Per IACS UR W16 / RINA extra-high-strength rules. Exact maxima for Ni, Cu, Cr and Mo depend on delivery condition (N/NR, TM or QT). Carbon equivalent / CET / Pcm limits apply by thickness and condition; confirm on the mill certificate and current rule edition.
Product Analysis (Check Analysis)
When product analysis is required, apply ASTM A6/A6M Table A permitted variations to the heat limits unless the element is min-only or not listed in Table A.
| Element | Heat analysis limit | Product analysis (heat ± A6) |
|---|---|---|
| C | 0.20 max | 0.24 max |
| Mn | 1.70 max | see A6 Table A vs heat upper limit |
| Si | 0.10-0.55 | 0.05–0.61 (approx. A6) |
| P | 0.030 max | 0.040 max |
| S | 0.030 max | 0.040 max |
| Al (acid sol.) | 0.015 min | no A6 Table A tolerance; product value not tabulated |
| N | 0.020 max | 0.025 max (typical A6 +0.005) |
| Nb | 0.02-0.05 | 0.010–0.060 |
| V | 0.04-0.10 | 0.030–0.110 |
| Ti | 0.02 max | 0.03 max |
| B | 0.005 max | product analysis often not applicable |
Product analysis applies only when specified; for a range, results may not vary both above and below it.
RINA E460 Mechanical Properties
| Grade | Yield strength, min | Tensile strength | Elongation, min |
|---|---|---|---|
| RINA E460 | 460 MPa [67 ksi] | 570-720 MPa [83-104 ksi] | 17% |
Per IACS UR W16 / RINA rules (common t≤50 mm values). Yield may step down for thicker plates per UR W16; confirm thickness-dependent values on the order.
Charpy V-Notch Impact Requirements (-40°C [-40°F])
| Thickness | Test temperature | Longitudinal, avg min | Transverse, avg min |
|---|---|---|---|
| t≤50 mm | -40°C [-40°F] | 46 J | 31 J |
| 50<t≤70 mm | -40°C [-40°F] | 46 J | 31 J |
| 70<t≤100 mm | -40°C [-40°F] | 46 J | 31 J |
Per IACS UR W16 / RINA extra-high-strength practice. Average of three full-size specimens; transverse values apply when required. Thicker plates by agreement.
Delivery Condition and Deoxidation
Deoxidation: Killed, fine-grain practice. Delivery condition: typically TMCP or QT for extra-high-strength plates; N/NR may apply at lower extra-high levels per rules. E-class (E460) grades are supplied normalized or TMCP; as-rolled delivery is not permitted for the E toughness class. Optional extras: UT, Z15/Z25/Z35, RINA survey.
Thickness Coverage
Extra-high-strength RINA A/D/E/F 420-690 plates are commonly supplied from about 6 mm to 100 mm thick (thicker by agreement under UR W16). Width 1500-4000 mm and length 6000-18000 mm are typical.
Equivalent Steel Grades of RINA E460
| Society / Standard | Equivalent grade |
|---|---|
| RINA (Registro Italiano Navale) | RINA E460 steel plate (RI/E460; LR EH46 / ABS EQ47) |
| LR (Lloyd's Register) | LR EH46 steel plate |
| ABS | ABS EQ47 steel plate |
| CCS | CCS E460 steel plate |
| GL | GL E460 steel plate |
| DNV | DNV E460 steel plate |
| NK | NK E47 steel plate |
| KR | KR E47 steel plate |
| BV | BV E460 steel plate |
IACS societies align extra-high-strength hull grades under UR W16; naming differs (RINA E460, LR EH46, ABS EQ47). Dual certification is common when ordered that way.
FAQ about RINA E460 Steel Plate
What is RINA E460 steel plate?
It is an extra-high-strength hull structural steel under RINA Rules (IACS UR W16 extra-high-strength family), with 460 MPa minimum yield, 570-720 MPa tensile strength and Charpy toughness at -40°C [-40°F]. The mill certificate grade is RINA E460 (RI/E460).
What does RINA E460 / RI/E460 stand for?
RINA is Registro Italiano Navale (RI on certificates). The letter E is the toughness class (Charpy at -40°C [-40°F]), and 460 is the yield-strength level in MPa. Market/LR naming often uses EH46; ABS often uses EQ47. Note: RINA does not use AH460 — the grade is E460, not AH460.
What is the yield strength of RINA E460?
Minimum 460 MPa (67 ksi), tensile 570-720 MPa (83-104 ksi), elongation about 17% min (for the common thickness range).
What is the impact test temperature for RINA E460?
Charpy V-notch at -40°C [-40°F]. Typical longitudinal average minimum is 46 J (transverse 31 J) for the tabulated thickness range on this grade page.
What is the difference between RINA A460, D460, E460 and F460?
Same 460 MPa strength class. Toughness class differs: A at 0°C, D at -20°C, E at -40°C, F at -60°C. Chemistry (C, P, S, Mn) is tightened for colder classes.
How does RINA E460 differ from higher-strength RINA AH40?
RINA AH40 is UR W11 higher-strength (390 MPa). RINA E460 is UR W16 extra-high-strength (460 MPa) with different chemistry and delivery practice (often TM/QT).
Is RINA E460 the same as LR EH46 or ABS EQ47?
They are IACS counterparts in the extra-high-strength family; exact chemistry/delivery options differ by society edition. Dual certification is available when surveys are arranged.
Is RINA E460 weldable?
Weldable with approved procedures for extra-high-strength ship steel. Preheat, heat input and consumable matching are critical; follow the mill WPS and RINA welding requirements.
What heat treatment is required for RINA E460?
Extra-high-strength grades are typically delivered TMCP or quenched and tempered (QT), sometimes normalized/normalized-rolled depending on strength level and thickness. E-class (E460) grades are supplied normalized or TMCP; as-rolled delivery is not permitted for the E toughness class. Optional extras: UT, Z15/Z25/Z35, RINA survey.
What thickness is available for RINA E460?
Common supply is about 6-100 mm (thicker by agreement under UR W16 / RINA rules), 1500-4000 mm wide and 6000-18000 mm long.
Other RINA Steel Plate Grades
RINA Grade A steel plate | RINA Grade B steel plate | RINA Grade D steel plate | RINA Grade E steel plate | RINA AH32 steel plate | RINA AH36 steel plate | RINA AH40 steel plate | RINA DH32 steel plate | RINA DH36 steel plate | RINA DH40 steel plate | RINA EH32 steel plate | RINA EH36 steel plate | RINA EH40 steel plate | RINA FH32 steel plate | RINA FH36 steel plate | RINA FH40 steel plate | RINA A420 steel plate | RINA A460 steel plate | RINA A500 steel plate | RINA A550 steel plate | RINA A620 steel plate | RINA A690 steel plate | RINA D420 steel plate | RINA D460 steel plate | RINA D500 steel plate | RINA D550 steel plate | RINA D620 steel plate | RINA D690 steel plate | RINA E420 steel plate | RINA E500 steel plate | RINA E550 steel plate | RINA E620 steel plate | RINA E690 steel plate | RINA F420 steel plate | RINA F460 steel plate | RINA F500 steel plate | RINA F550 steel plate | RINA F620 steel plate | RINA F690 steel plate
Equivalent Class Society Grades
RINA E460 corresponds to extra-high-strength counterparts under other IACS societies (LR EH46, ABS EQ47, etc.): LR EH46 steel plate, ABS EQ47 steel plate, CCS E460 steel plate, GL E460 steel plate, DNV E460 steel plate, NK E47 steel plate, KR E47 steel plate, BV E460 steel plate, RINA E460 steel plate.
-
RINA DH36 Steel Plate | DH36 Sh
RINA DH36 (RI/DH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at -20C, chemistry and
-
RINA AH36 Steel Plate | AH36 Sh
RINA AH36 (RI/AH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at 0C, chemistry and e
-
RINA FH32 Steel Plate | FH32 Sh
RINA FH32 (RI/FH32) shipbuilding steel plate: 315 MPa yield, 440-590 MPa tensile, Charpy at -60C, chemistry and
-
RINA Grade A Steel Plate | Grad
RINA Grade A (RI/A) shipbuilding steel plate: 235 MPa yield, 400-520 MPa tensile, Charpy at +20C, chemistry and