BV E620 steel plate, also written as BV/E620, BV Grade E620 or market names such as EH62 / EQ63, is the extra-high-strength hull structural steel of Bureau Veritas Rules for the Classification of Steel Ships (IACS UR W16 extra-high-strength family) with 620 MPa minimum yield, 720-890 MPa tensile strength and Charpy V-notch toughness at -40°C [-40°F]. In the grade name, "E" is the toughness class, and "620" is the yield-strength level in MPa (not AH620). Gangsteel, a steel plate exporter, supplies BV E620 plates cut to size for shipbuilding, offshore platforms and marine structures.

Data source: Per IACS UR W16 (extra-high-strength hull structural steel) as adopted in Bureau Veritas hull structural steel rules, cross-checked with LR EH62 / ABS EQ63 sibling pages on gangsteel.net. Official mill/certificate grade is BV E620. Verify the current BV edition before ordering.

BV E620 Chemical Composition (Heat Analysis)

 

ElementCMnSiPSAl (acid sol.)
BV E620, %0.20 max1.70 max0.10-0.550.030 max0.030 max0.015 min
ElementNNbVTiBNotes
BV E620, %0.020 max0.02-0.050.04-0.100.02 max0.005 maxNi/Cu/Cr/Mo per delivery condition (N/TM/QT) in UR W16

Per IACS UR W16 / Bureau Veritas extra-high-strength rules. Exact maxima for Ni, Cu, Cr and Mo depend on delivery condition (N/NR, TM or QT). Carbon equivalent / CET / Pcm limits apply by thickness and condition; confirm on the mill certificate and current rule edition.

Product Analysis (Check Analysis)

 

When product analysis is required, apply ASTM A6/A6M Table A permitted variations to the heat limits unless the element is min-only or not listed in Table A.

ElementHeat analysis limitProduct analysis (heat ± A6)
C0.20 max0.24 max
Mn1.70 maxsee A6 Table A vs heat upper limit
Si0.10-0.550.05–0.61 (approx. A6)
P0.030 max0.040 max
S0.030 max0.040 max
Al (acid sol.)0.015 minno A6 Table A tolerance; product value not tabulated
N0.020 max0.025 max (typical A6 +0.005)
Nb0.02-0.050.010–0.060
V0.04-0.100.030–0.110
Ti0.02 max0.03 max
B0.005 maxproduct analysis often not applicable

Product analysis applies only when specified; for a range, results may not vary both above and below it.

BV E620 Mechanical Properties

 

GradeYield strength, minTensile strengthElongation, min
BV E620620 MPa [90 ksi]720-890 MPa [104-129 ksi]15%

Per IACS UR W16 / Bureau Veritas rules (common t≤50 mm values). Yield may step down for thicker plates per UR W16; confirm thickness-dependent values on the order.

Charpy V-Notch Impact Requirements (-40°C [-40°F])

 

ThicknessTest temperatureLongitudinal, avg minTransverse, avg min
t≤50 mm-40°C [-40°F]62 J41 J
50<t≤70 mm-40°C [-40°F]62 J41 J
70<t≤100 mm-40°C [-40°F]62 J41 J

Per IACS UR W16 / Bureau Veritas extra-high-strength practice. Average of three full-size specimens; transverse values apply when required. Thicker plates by agreement.

Delivery Condition and Deoxidation

Deoxidation: Killed, fine-grain practice. Delivery condition: typically TMCP or QT for extra-high-strength plates; N/NR may apply at lower extra-high levels per rules. E-class (E620) grades are supplied normalized or TMCP; as-rolled delivery is not permitted for the E toughness class. Optional extras: UT, Z15/Z25/Z35, BV survey.

Thickness Coverage

Extra-high-strength BV A/D/E/F 420-690 plates are commonly supplied from about 6 mm to 100 mm thick (thicker by agreement under UR W16). Width 1500-4000 mm and length 6000-18000 mm are typical.

Equivalent Steel Grades of BV E620

 

Society / StandardEquivalent grade
BV (Bureau Veritas)BV E620 steel plate (LR EH62 / ABS EQ63)
LR (Lloyd's Register)LR EH62 steel plate
ABSABS EQ63 steel plate
CCSCCS E620 steel plate
GLGL E620 steel plate
DNVDNV E620 steel plate
NKNK E63 steel plate
KRKR E63 steel plate
RINARINA E620 steel plate

IACS societies align extra-high-strength hull grades under UR W16; naming differs (BV E620, LR EH62, ABS EQ63). Dual certification is common when ordered that way.

FAQ about BV E620 Steel Plate

What is BV E620 steel plate?

It is an extra-high-strength hull structural steel under Bureau Veritas Rules (IACS UR W16 extra-high-strength family), with 620 MPa minimum yield, 720-890 MPa tensile strength and Charpy toughness at -40°C [-40°F].

What does BV E620 stand for?

BV is Bureau Veritas. The letter E is the toughness class (Charpy at -40°C [-40°F]), and 620 is the yield-strength level in MPa. Market/LR naming often uses EH62; ABS often uses EQ63. Note: BV does not use AH620 — the grade is E620, not AH620.

What is the yield strength of BV E620?

Minimum 620 MPa (90 ksi), tensile 720-890 MPa (104-129 ksi), elongation about 15% min (for the common thickness range).

What is the impact test temperature for BV E620?

Charpy V-notch at -40°C [-40°F]. Typical longitudinal average minimum is 62 J (transverse 41 J) for the tabulated thickness range on this grade page.

What is the difference between BV A620, D620, E620 and F620?

Same 620 MPa strength class. Toughness class differs: A at 0°C, D at -20°C, E at -40°C, F at -60°C. Chemistry (C, P, S, Mn) is tightened for colder classes.

How does BV E620 differ from higher-strength BV AH40?

BV AH40 is UR W11 higher-strength (390 MPa). BV E620 is UR W16 extra-high-strength (620 MPa) with different chemistry and delivery practice (often TM/QT).

Is BV E620 the same as LR EH62 or ABS EQ63?

They are IACS counterparts in the extra-high-strength family; exact chemistry/delivery options differ by society edition. Dual certification is available when surveys are arranged.

Is BV E620 weldable?

Weldable with approved procedures for extra-high-strength ship steel. Preheat, heat input and consumable matching are critical; follow the mill WPS and BV welding requirements.

What heat treatment is required for BV E620?

Extra-high-strength grades are typically delivered TMCP or quenched and tempered (QT), sometimes normalized/normalized-rolled depending on strength level and thickness. E-class (E620) grades are supplied normalized or TMCP; as-rolled delivery is not permitted for the E toughness class. Optional extras: UT, Z15/Z25/Z35, BV survey.

What thickness is available for BV E620?

Common supply is about 6-100 mm (thicker by agreement under UR W16 / BV rules), 1500-4000 mm wide and 6000-18000 mm long.

Other BV Steel Plate Grades

BV Grade A steel plate | BV Grade B steel plate | BV Grade D steel plate | BV Grade E steel plate | BV AH32 steel plate | BV AH36 steel plate | BV AH40 steel plate | BV DH32 steel plate | BV DH36 steel plate | BV DH40 steel plate | BV EH32 steel plate | BV EH36 steel plate | BV EH40 steel plate | BV FH32 steel plate | BV FH36 steel plate | BV FH40 steel plate | BV A420 steel plate | BV A460 steel plate | BV A500 steel plate | BV A550 steel plate | BV A620 steel plate | BV A690 steel plate | BV D420 steel plate | BV D460 steel plate | BV D500 steel plate | BV D550 steel plate | BV D620 steel plate | BV D690 steel plate | BV E420 steel plate | BV E460 steel plate | BV E500 steel plate | BV E550 steel plate | BV E690 steel plate | BV F420 steel plate | BV F460 steel plate | BV F500 steel plate | BV F550 steel plate | BV F620 steel plate | BV F690 steel plate

Equivalent Class Society Grades

BV E620 corresponds to extra-high-strength counterparts under other IACS societies (LR EH62, ABS EQ63, etc.): LR EH62 steel plate, ABS EQ63 steel plate, CCS E620 steel plate, GL E620 steel plate, DNV E620 steel plate, NK E63 steel plate, KR E63 steel plate, RINA E620 steel plate.

Other Products