BV steel plate
BV/A420|BV Grade A420 STEEL PLATE
BV A420 steel plate, also written as BV/A420, BV Grade A420 or market names such as AH42 / AQ43, is the extra-high-strength hull structural steel of Bureau Veritas Rules for the Classification of Steel Ships (IACS UR W16 extra-high-strength family) with 420 MPa minimum yield, 530-680 MPa tensile strength and Charpy V-notch toughness at 0°C [32°F]. In the grade name, "A" is the toughness class, and "420" is the yield-strength level in MPa (not AH420). Gangsteel, a steel plate exporter, supplies BV A420 plates cut to size for shipbuilding, offshore platforms and marine structures.
Data source: Per IACS UR W16 (extra-high-strength hull structural steel) as adopted in Bureau Veritas hull structural steel rules, cross-checked with LR AH42 / ABS AQ43 sibling pages on gangsteel.net. Official mill/certificate grade is BV A420. Verify the current BV edition before ordering.
BV A420 Chemical Composition (Heat Analysis)
| Element | C | Mn | Si | P | S | Al (acid sol.) |
|---|---|---|---|---|---|---|
| BV A420, % | 0.21 max | 1.70 max | 0.10-0.55 | 0.035 max | 0.035 max | 0.015 min |
| Element | N | Nb | V | Ti | B | Notes |
| BV A420, % | 0.020 max | 0.02-0.05 | 0.04-0.10 | 0.02 max | 0.005 max | Ni/Cu/Cr/Mo per delivery condition (N/TM/QT) in UR W16 |
Per IACS UR W16 / Bureau Veritas extra-high-strength rules. Exact maxima for Ni, Cu, Cr and Mo depend on delivery condition (N/NR, TM or QT). Carbon equivalent / CET / Pcm limits apply by thickness and condition; confirm on the mill certificate and current rule edition.
Product Analysis (Check Analysis)
When product analysis is required, apply ASTM A6/A6M Table A permitted variations to the heat limits unless the element is min-only or not listed in Table A.
| Element | Heat analysis limit | Product analysis (heat ± A6) |
|---|---|---|
| C | 0.21 max | 0.25 max |
| Mn | 1.70 max | see A6 Table A vs heat upper limit |
| Si | 0.10-0.55 | 0.05–0.61 (approx. A6) |
| P | 0.035 max | 0.045 max |
| S | 0.035 max | 0.045 max |
| Al (acid sol.) | 0.015 min | no A6 Table A tolerance; product value not tabulated |
| N | 0.020 max | 0.025 max (typical A6 +0.005) |
| Nb | 0.02-0.05 | 0.010–0.060 |
| V | 0.04-0.10 | 0.030–0.110 |
| Ti | 0.02 max | 0.03 max |
| B | 0.005 max | product analysis often not applicable |
Product analysis applies only when specified; for a range, results may not vary both above and below it.
BV A420 Mechanical Properties
| Grade | Yield strength, min | Tensile strength | Elongation, min |
|---|---|---|---|
| BV A420 | 420 MPa [61 ksi] | 530-680 MPa [77-99 ksi] | 18% |
Per IACS UR W16 / Bureau Veritas rules (common t≤50 mm values). Yield may step down for thicker plates per UR W16; confirm thickness-dependent values on the order.
Charpy V-Notch Impact Requirements (0°C [32°F])
| Thickness | Test temperature | Longitudinal, avg min | Transverse, avg min |
|---|---|---|---|
| t≤50 mm | 0°C [32°F] | 42 J | 28 J |
| 50<t≤70 mm | 0°C [32°F] | 42 J | 28 J |
| 70<t≤100 mm | 0°C [32°F] | 42 J | 28 J |
Per IACS UR W16 / Bureau Veritas extra-high-strength practice. Average of three full-size specimens; transverse values apply when required. Thicker plates by agreement.
Delivery Condition and Deoxidation
Deoxidation: Killed, fine-grain practice. Delivery condition: typically TMCP or QT for extra-high-strength plates; N/NR may apply at lower extra-high levels per rules. A-class (A420) grades may be as-rolled, controlled rolled, normalized or TMCP depending on thickness; thicker plates usually N or TMCP. Optional extras: UT, Z15/Z25/Z35, BV survey.
Thickness Coverage
Extra-high-strength BV A/D/E/F 420-690 plates are commonly supplied from about 6 mm to 100 mm thick (thicker by agreement under UR W16). Width 1500-4000 mm and length 6000-18000 mm are typical.
Equivalent Steel Grades of BV A420
| Society / Standard | Equivalent grade |
|---|---|
| BV (Bureau Veritas) | BV A420 steel plate (LR AH42 / ABS AQ43) |
| LR (Lloyd's Register) | LR AH42 steel plate |
| ABS | ABS AQ43 steel plate |
| CCS | CCS A420 steel plate |
| GL | GL A420 steel plate |
| DNV | DNV A420 steel plate |
| NK | NK A43 steel plate |
| KR | KR A43 steel plate |
| RINA | RINA A420 steel plate |
IACS societies align extra-high-strength hull grades under UR W16; naming differs (BV A420, LR AH42, ABS AQ43). Dual certification is common when ordered that way.
FAQ about BV A420 Steel Plate
What is BV A420 steel plate?
It is an extra-high-strength hull structural steel under Bureau Veritas Rules (IACS UR W16 extra-high-strength family), with 420 MPa minimum yield, 530-680 MPa tensile strength and Charpy toughness at 0°C [32°F].
What does BV A420 stand for?
BV is Bureau Veritas. The letter A is the toughness class (Charpy at 0°C [32°F]), and 420 is the yield-strength level in MPa. Market/LR naming often uses AH42; ABS often uses AQ43. Note: BV does not use AH420 — the grade is A420, not AH420.
What is the yield strength of BV A420?
Minimum 420 MPa (61 ksi), tensile 530-680 MPa (77-99 ksi), elongation about 18% min (for the common thickness range).
What is the impact test temperature for BV A420?
Charpy V-notch at 0°C [32°F]. Typical longitudinal average minimum is 42 J (transverse 28 J) for the tabulated thickness range on this grade page.
What is the difference between BV A420, D420, E420 and F420?
Same 420 MPa strength class. Toughness class differs: A at 0°C, D at -20°C, E at -40°C, F at -60°C. Chemistry (C, P, S, Mn) is tightened for colder classes.
How does BV A420 differ from higher-strength BV AH40?
BV AH40 is UR W11 higher-strength (390 MPa). BV A420 is UR W16 extra-high-strength (420 MPa) with different chemistry and delivery practice (often TM/QT).
Is BV A420 the same as LR AH42 or ABS AQ43?
They are IACS counterparts in the extra-high-strength family; exact chemistry/delivery options differ by society edition. Dual certification is available when surveys are arranged.
Is BV A420 weldable?
Weldable with approved procedures for extra-high-strength ship steel. Preheat, heat input and consumable matching are critical; follow the mill WPS and BV welding requirements.
What heat treatment is required for BV A420?
Extra-high-strength grades are typically delivered TMCP or quenched and tempered (QT), sometimes normalized/normalized-rolled depending on strength level and thickness. A-class (A420) grades may be as-rolled, controlled rolled, normalized or TMCP depending on thickness; thicker plates usually N or TMCP. Optional extras: UT, Z15/Z25/Z35, BV survey.
What thickness is available for BV A420?
Common supply is about 6-100 mm (thicker by agreement under UR W16 / BV rules), 1500-4000 mm wide and 6000-18000 mm long.
Other BV Steel Plate Grades
BV Grade A steel plate | BV Grade B steel plate | BV Grade D steel plate | BV Grade E steel plate | BV AH32 steel plate | BV AH36 steel plate | BV AH40 steel plate | BV DH32 steel plate | BV DH36 steel plate | BV DH40 steel plate | BV EH32 steel plate | BV EH36 steel plate | BV EH40 steel plate | BV FH32 steel plate | BV FH36 steel plate | BV FH40 steel plate | BV A460 steel plate | BV A500 steel plate | BV A550 steel plate | BV A620 steel plate | BV A690 steel plate | BV D420 steel plate | BV D460 steel plate | BV D500 steel plate | BV D550 steel plate | BV D620 steel plate | BV D690 steel plate | BV E420 steel plate | BV E460 steel plate | BV E500 steel plate | BV E550 steel plate | BV E620 steel plate | BV E690 steel plate | BV F420 steel plate | BV F460 steel plate | BV F500 steel plate | BV F550 steel plate | BV F620 steel plate | BV F690 steel plate
Equivalent Class Society Grades
BV A420 corresponds to extra-high-strength counterparts under other IACS societies (LR AH42, ABS AQ43, etc.): LR AH42 steel plate, ABS AQ43 steel plate, CCS A420 steel plate, GL A420 steel plate, DNV A420 steel plate, NK A43 steel plate, KR A43 steel plate, RINA A420 steel plate.
-
BV/E690|BV Grade E690 STEEL PLA
BV E690 shipbuilding steel plate: 690 MPa yield, 770-940 MPa tensile, Charpy at -40C, chemistry and equivalents
-
DH40,BV DH40|BV/DH40,BV DH40 ST
BV DH40 (BV Grade DH40) shipbuilding steel plate: 390 MPa yield, 510-650 MPa tensile, Charpy at -20C, chemistry
-
BV/DH36|BV Grade DH36 STEEL PLA
BV DH36 (BV Grade DH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at -20C, chemistry
-
BV/AH36|BV Grade AH36 STEEL PLA
BV AH36 (BV Grade AH36) shipbuilding steel plate: 355 MPa yield, 490-620 MPa tensile, Charpy at 0C, chemistry a