ABS Steel Plate
ABS EQ70 Steel Plate – Properties, Chemistry & Equivalents

ABS EQ70 (also written AB/EQ70, ABS Grade EQ70, EQ70 steel plate) is an extra-high-strength steel plate to ABS Rules Part 2, Chapter 1, Section 8 (2018). The number 70 is the yield category (690 MPa minimum, tensile 770-940 MPa) and the prefix EQ sets the Charpy test temperature of -40°C. Grades of this family are supplied quenched and tempered (QT) or thermo-mechanically rolled (TM). It corresponds to grade E690 in IACS UR W16; ASTM A131 does not cover this strength level.
Related grades: ABS AQ70 steel plate ABS DQ70 steel plate ABS FQ70 steel plate ABS EQ63 steel plate.
Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade EQ70. For more information of Grade EQ70 steel plate, please check them in following:
AB/EQ70 Extra high Strength Chemical Composition in Tempering and Quenching
| Element | Heat analysis (max/min) | Product analysis |
|---|---|---|
| C | ≤ 0.18 | ≤ 0.22 |
| Mn | ≤ 1.70 | ≤ 1.84 |
| Si | ≤ 0.80 | ≤ 0.86 |
| P | ≤ 0.020 | ≤ 0.030 |
| S | ≤ 0.010 | ≤ 0.020 |
| Al (total) | ≥ 0.018 | — (no tolerance in ASTM A6 Table A; product value not given) |
| Nb | ≤ 0.06 | ≤ 0.07 |
| V | ≤ 0.12 | ≤ 0.14 |
| Ti | ≤ 0.05 | ≤ 0.06 |
| Ni | ≤ 3.50 | ≤ 3.57 |
| Cu | ≤ 0.50 | ≤ 0.53 |
| Cr | ≤ 2.00 | ≤ 2.06 |
| Mo | ≤ 0.70 | ≤ 0.74 |
| N | ≤ 0.015 | ≤ 0.020 |
| Ca | ≤ 0.005 | — (no tolerance in ASTM A6 Table A; product value not given) |
| B | ≤ 0.005 | product analysis not applicable (A6 Table A) |
ABS 2022: limits shown are for the quenched and tempered (QT) condition; N/NR/CR and TM supply have different limits in Table 4A. Al/N ≥ 2:1 (not required when other N-binding elements are used); higher C or N may be agreed with ABS; Ni content agreed at qualification; final chemistry must also meet the mill's ABS-approved specification. Product analysis = heat limit ± ASTM A6/A6M Table A permitted variation (band chosen by the specified maximum/upper limit); applies only when product (check) analysis is required; for a range, results may not vary both above and below it. Per ABS Rules for Materials and Welding Part 2 (2022); product analysis tolerances per ABS 2-1-2/5.3 (“chemical tolerances of ASTM A6”) and ASTM A6/A6M 7.2, Table A (also invoked by ASTM A131). Heat limits: ABS 2-1-8/4 Table 4A (2022), QT column.
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/EQ70 Extra high strength property in tempering and quenching
| Grade | Yield ReH min (MPa) | Tensile Rm (MPa) | Elongation A5 min (%) | Charpy test temp (°C) | Impact energy avg min, longitudinal (J) | Impact energy avg min, transverse (J) |
|---|---|---|---|---|---|---|
| AB/EQ70 | 690 | 770-940 | 14 | -40 | 69 | 46 |
Source: ABS Rules Pt 2, 2-1-8, Table 5A. Either longitudinal or transverse specimens per the order.
Boiler steel plates| Alloy steel plates| High strength plate| Carbon steel plate
|
Equivalent steel grade of AB/EQ70 |
|||||||
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.
Related steel grades: AB/EQ63, AB/EQ56, AB/EQ51, AB/EQ47
|
General Strength |
||||
|
High Strength |
||||
|
Extra Strength |
||||
ABS EQ70 thickness and impact requirements
For ABS EQ70 the Charpy V-notch test is run at -40°C with a minimum average of 69 J longitudinal or 46 J transverse. The requirement does not change with thickness the way it does for hull grades; the maximum thickness depends on the supply condition and the mill approval (ABS 2-1-8, Table 3). Confirm the thickness limit with the mill approval before ordering.
| Standard / society | Equivalent grade |
|---|---|
| ABS | AB/EQ70 |
| IACS UR W16 | E690 |
| DNV | VL E690 |
| Other IACS societies (LR, BV, CCS, NK, KR, RINA) | E690 with the society's own prefix |
| ASTM A131 | no equivalent (A131 stops at 390 MPa) |
Grades are equivalent in chemistry and properties because the IACS societies use the same unified requirements. A plate still needs a certificate from the vessel's own classification society, so one plate can carry dual or multiple class certification only when each society's surveyor tests it.
FAQ
What does EQ70 mean?
EQ sets the Charpy test temperature (-40°C), and 70 is the strength level: minimum yield 690 MPa.
What are the mechanical properties of ABS EQ70?
Minimum yield 690 MPa, tensile strength 770-940 MPa and minimum elongation 14%. Charpy average at -40°C is at least 69 J longitudinal or 46 J transverse.
What is the impact test temperature of ABS EQ70?
-40°C.
What is ABS EQ70 equivalent to?
Grade E690 in IACS UR W16 (DNV VL E690). ASTM A131 has no equivalent at this strength. The plate must be certified by the vessel's classification society.
How is ABS EQ70 supplied?
Quenched and tempered (QT) or thermo-mechanically rolled (TM). The chemistry limits and maximum thickness depend on the supply condition (ABS 2-1-8, Tables 3 and 4A).
-
ABS Grade A Plate – Propertie
ABS Grade A ordinary-strength hull plate: chemical composition, 235 MPa yield, 400-520 MPa tensile, Charpy test
-
ABS EH36 Steel Plate – Proper
ABS EH36 higher-strength ship plate: 355 MPa min yield, 490-620 MPa tensile, Charpy at -40°C, chemistry table
-
ABS DH36 Steel Plate – Proper
ABS DH36 higher-strength ship plate: 355 MPa min yield, 490-620 MPa tensile, Charpy at -20°C, chemistry table
-
ABS AH36 Steel Plate – Proper
ABS AH36 higher-strength ship plate: 355 MPa min yield, 490-620 MPa tensile, Charpy at 0°C, chemistry table an