ABS DH32 shipbuilding steel plate

ABS DH32 (also written AB/DH32, ABS Grade DH32, DH32 steel plate) is a higher-strength hull structural steel plate to ABS Rules Part 2, Chapter 1, Section 3. The figure 32 is the strength class (minimum yield 315 MPa, tensile 440-590 MPa) and the letter D sets the Charpy V-notch test temperature of -20°C. It is killed and fine-grain treated, with Nb, V, Ti or Al used as grain refiners, and corresponds to grade D32 in IACS UR W11 and DH32 in ASTM A131.

Related grades: ABS AH32 steel plate ABS EH32 steel plate ABS FH32 steel plate ABS DH36 steel plate.

Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade DH32. For more information of GradeDH32 steel plate, please check them in following:

 

 

 

AB/DH32 high Strength Chemical Composition

AB/DH32

ABS DH32 chemical composition, % – heat (ladle) analysis and product (check) analysis
Element Heat analysis (max/min) Product analysis
C ≤ 0.18 ≤ 0.22
Mn 0.90–1.60 0.81–1.72
Si 0.10–0.50 0.04–0.56
P ≤ 0.035 ≤ 0.045
S ≤ 0.035 ≤ 0.045
Al (acid-soluble) ≥ 0.015 — (no tolerance in ASTM A6 Table A; product value not given)
Nb 0.02–0.05 0.010–0.060
V 0.05–0.10 0.040–0.110
Ti ≤ 0.02 ≤ 0.03
Cu ≤ 0.35 ≤ 0.38
Cr ≤ 0.20 ≤ 0.24
Ni ≤ 0.40 ≤ 0.43
Mo ≤ 0.08 ≤ 0.09

Al, Nb and V minima apply when used singly (combined minima per ABS 2-1-3/5); Si min does not apply where acid-soluble Al ≥ 0.015%; AH ≤ 12.5 mm may have Mn min 0.70%. Product analysis = heat limit ± ASTM A6/A6M Table A permitted variation (band chosen by the specified maximum/upper limit); applies only when product (check) analysis is required; for a range, results may not vary both above and below it. Per ABS Rules for Materials and Welding Part 2 (2022); product analysis tolerances per ABS 2-1-2/5.3 (“chemical tolerances of ASTM A6”) and ASTM A6/A6M 7.2, Table A (also invoked by ASTM A131). Heat limits: ABS 2-1-3/7.3 Table 1 (t ≤ 150 mm).

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

 

 

 

 

AB/DH32 high strength property

AB/DH32

ABS DH32 mechanical properties by thickness
Thickness (mm) Yield min (MPa) Tensile (MPa) Elongation A5 min (%) Charpy test temp (°C) Impact avg min, longitudinal (J) Impact avg min, transverse (J)
t≤50 315 440-590 22 -20 31 22
50<t≤70 315 440-590 22 -20 38 26
70<t≤100 315 440-590 22 -20 46 31

Source: ABS Rules Pt 2, 2-1-3 Tables 2 & 4. Either direction acceptable.

Boiler steel plates| Alloy steel plates| High strength plate| Carbon steel plate

 

 

 

 

 

Equivalent steel grade of AB/DH32

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV D32

GL-D32

LR/DH32

BV/DH32

CCS/D32

K D32

R D32

RI/D32

 

 

 

 

If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 Related steel grades: AB/B, AB/D, AB/EH32, AB/FH32

 

ABS Steel Plate Grade Supplier

General Strength

AB/A

AB/B

AB/D

AB/E

High Strength

AB/AH32

AB/DH32

AB/EH32

AB/FH32

AB/AH36

AB/DH36

AB/EH36

AB/FH36

AB/AH40

AB/DH40

AB/EH40

AB/FH40

Extra Strength

AB/AQ43

AB/DQ43

AB/EQ43

AB/FQ43

AB/AQ47

AB/DQ47

AB/EQ47

AB/FQ47

AB/AQ51

AB/DQ51

AB/EQ51

AB/FQ51

AB/AQ56

AB/DQ56

AB/EQ56

AB/FQ56

AB/AQ63

AB/DQ63

AB/EQ63

AB/FQ63

AB/AQ70

AB/DQ70

AB/EQ70

AB/FQ70

 

ABS DH32 thickness and impact requirements

ABS impact energy rises with plate thickness. ABS DH32 is tested at -20°C. Minimum average energies (full-size specimens):

  • t≤50 mm: 31 J longitudinal / 22 J transverse
  • 50<t≤70 mm: 38 J longitudinal / 26 J transverse
  • 70<t≤100 mm: 46 J longitudinal / 31 J transverse

The ABS tables cover plates up to 150 mm. Plates thicker than 100 mm, or produced from coil, have extra rules in ABS Part 2, Chapter 1, Section 1.

ABS DH32 equivalent grades
Standard / society Equivalent grade
ABS AB/DH32
IACS UR W11 D32 (also written DH32)
ASTM A131 DH32
DNV VL D32
LR / BV / CCS / RINA DH32
NK KD32
KR RD32

Grades are equivalent in chemistry and properties because the IACS societies use the same unified requirements. A plate still needs a certificate from the vessel's own classification society, so one plate can carry dual or multiple class certification only when each society's surveyor tests it.

FAQ

What does DH32 mean?

The letter D sets the Charpy test temperature (-20°C), and 32 is the strength level: minimum yield 315 MPa.

What are the mechanical properties of ABS DH32?

Minimum yield 315 MPa, tensile strength 440-590 MPa and minimum elongation 22%. Charpy average at -20°C is at least 31 J longitudinal / 22 J transverse for t ≤ 50 mm.

What is the impact test temperature of ABS DH32?

-20°C.

What is ABS DH32 equivalent to?

ASTM A131 DH32, IACS UR W11 grade D32, DNV VL D32, and DH32 under LR, BV, CCS and RINA (NK KD32, KR RD32). The plate still needs a certificate from the vessel's classification society.

What is the chemical composition of ABS DH32?

C ≤ 0.18%, Mn 0.90-1.60%, Si 0.10-0.50%, P and S ≤ 0.035%, and at least one grain refiner (Al ≥ 0.015%, Nb 0.02-0.05% or V 0.05-0.10%). Ni ≤ 0.40%.

How is ABS DH32 supplied?

Depending on thickness and grain refiner: as rolled (thin plates of A and D grades only), normalized, controlled rolled or thermo-mechanically rolled; E and F grades are normalized or TM (QT also allowed for 40 grades). See ABS 2-1-3 Table 5.

ASTM equivalent: ASTM A131 DH32 steel plate

LR equivalent: LR DH32 steel plate

Other Products